Deslagging and dephosphorizing method of electric stove

The invention relates to a deslagging and dephosphorizing method of an electric stove, which adopts the following public technical scheme: slagging; deslagging for the first time; smelting by blowing oxygen, starting to deslag when the temperature of molten steel increases to 1500-1510 DEG C, and co...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHOU XINLONG, WANG GUOQIU, WEI ZEHONG, ZHANG XIANZHONG, LI XIANZHONG, MIAO KAI, GUI JIANGBING, XIONG YUZHANG, CHEN QINGFENG, GUO YUANKUI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHOU XINLONG
WANG GUOQIU
WEI ZEHONG
ZHANG XIANZHONG
LI XIANZHONG
MIAO KAI
GUI JIANGBING
XIONG YUZHANG
CHEN QINGFENG
GUO YUANKUI
description The invention relates to a deslagging and dephosphorizing method of an electric stove, which adopts the following public technical scheme: slagging; deslagging for the first time; smelting by blowing oxygen, starting to deslag when the temperature of molten steel increases to 1500-1510 DEG C, and controlling the weight percentage of phosphorus to decrease to be not more than 0.015 percent; slagging for the second time; deslagging for the second time, i.e. starting to deslag for the second time when the temperature of molten steel increases to 1520-1550 DEG C, and controlling the weight percentage of the phosphorus to decrease to be not more than 0.010 percent; slagging for the third time; deslagging for the third time, and controlling the weight percentage of the phosphorus to decrease to be not more than 0.005 percent; slagging for the fourth time; and preserving heat by blowing oxygen, adopting steel and slag residual operation with a tapping amount accounting for 85-90 percent of the total capacity of the
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN101619377A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN101619377A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN101619377A3</originalsourceid><addsrcrecordid>eNrjZDB3SS3OSUxPz8xLV0jMS1FISS3IyC8G4qLMKpBYbmpJRn6KQn6aQmpOanJJUWayQnFJflkqDwNrWmJOcSovlOZmUHRzDXH20E0tyI9PLS5ITE7NSy2Jd_YzNDA0M7Q0Njd3NCZGDQD0bS47</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Deslagging and dephosphorizing method of electric stove</title><source>esp@cenet</source><creator>ZHOU XINLONG ; WANG GUOQIU ; WEI ZEHONG ; ZHANG XIANZHONG ; LI XIANZHONG ; MIAO KAI ; GUI JIANGBING ; XIONG YUZHANG ; CHEN QINGFENG ; GUO YUANKUI</creator><creatorcontrib>ZHOU XINLONG ; WANG GUOQIU ; WEI ZEHONG ; ZHANG XIANZHONG ; LI XIANZHONG ; MIAO KAI ; GUI JIANGBING ; XIONG YUZHANG ; CHEN QINGFENG ; GUO YUANKUI</creatorcontrib><description>The invention relates to a deslagging and dephosphorizing method of an electric stove, which adopts the following public technical scheme: slagging; deslagging for the first time; smelting by blowing oxygen, starting to deslag when the temperature of molten steel increases to 1500-1510 DEG C, and controlling the weight percentage of phosphorus to decrease to be not more than 0.015 percent; slagging for the second time; deslagging for the second time, i.e. starting to deslag for the second time when the temperature of molten steel increases to 1520-1550 DEG C, and controlling the weight percentage of the phosphorus to decrease to be not more than 0.010 percent; slagging for the third time; deslagging for the third time, and controlling the weight percentage of the phosphorus to decrease to be not more than 0.005 percent; slagging for the fourth time; and preserving heat by blowing oxygen, adopting steel and slag residual operation with a tapping amount accounting for 85-90 percent of the total capacity of the</description><language>chi ; eng</language><subject>CHEMISTRY ; METALLURGY ; METALLURGY OF IRON ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><creationdate>2010</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20100106&amp;DB=EPODOC&amp;CC=CN&amp;NR=101619377A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20100106&amp;DB=EPODOC&amp;CC=CN&amp;NR=101619377A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHOU XINLONG</creatorcontrib><creatorcontrib>WANG GUOQIU</creatorcontrib><creatorcontrib>WEI ZEHONG</creatorcontrib><creatorcontrib>ZHANG XIANZHONG</creatorcontrib><creatorcontrib>LI XIANZHONG</creatorcontrib><creatorcontrib>MIAO KAI</creatorcontrib><creatorcontrib>GUI JIANGBING</creatorcontrib><creatorcontrib>XIONG YUZHANG</creatorcontrib><creatorcontrib>CHEN QINGFENG</creatorcontrib><creatorcontrib>GUO YUANKUI</creatorcontrib><title>Deslagging and dephosphorizing method of electric stove</title><description>The invention relates to a deslagging and dephosphorizing method of an electric stove, which adopts the following public technical scheme: slagging; deslagging for the first time; smelting by blowing oxygen, starting to deslag when the temperature of molten steel increases to 1500-1510 DEG C, and controlling the weight percentage of phosphorus to decrease to be not more than 0.015 percent; slagging for the second time; deslagging for the second time, i.e. starting to deslag for the second time when the temperature of molten steel increases to 1520-1550 DEG C, and controlling the weight percentage of the phosphorus to decrease to be not more than 0.010 percent; slagging for the third time; deslagging for the third time, and controlling the weight percentage of the phosphorus to decrease to be not more than 0.005 percent; slagging for the fourth time; and preserving heat by blowing oxygen, adopting steel and slag residual operation with a tapping amount accounting for 85-90 percent of the total capacity of the</description><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2010</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDB3SS3OSUxPz8xLV0jMS1FISS3IyC8G4qLMKpBYbmpJRn6KQn6aQmpOanJJUWayQnFJflkqDwNrWmJOcSovlOZmUHRzDXH20E0tyI9PLS5ITE7NSy2Jd_YzNDA0M7Q0Njd3NCZGDQD0bS47</recordid><startdate>20100106</startdate><enddate>20100106</enddate><creator>ZHOU XINLONG</creator><creator>WANG GUOQIU</creator><creator>WEI ZEHONG</creator><creator>ZHANG XIANZHONG</creator><creator>LI XIANZHONG</creator><creator>MIAO KAI</creator><creator>GUI JIANGBING</creator><creator>XIONG YUZHANG</creator><creator>CHEN QINGFENG</creator><creator>GUO YUANKUI</creator><scope>EVB</scope></search><sort><creationdate>20100106</creationdate><title>Deslagging and dephosphorizing method of electric stove</title><author>ZHOU XINLONG ; WANG GUOQIU ; WEI ZEHONG ; ZHANG XIANZHONG ; LI XIANZHONG ; MIAO KAI ; GUI JIANGBING ; XIONG YUZHANG ; CHEN QINGFENG ; GUO YUANKUI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN101619377A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2010</creationdate><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHOU XINLONG</creatorcontrib><creatorcontrib>WANG GUOQIU</creatorcontrib><creatorcontrib>WEI ZEHONG</creatorcontrib><creatorcontrib>ZHANG XIANZHONG</creatorcontrib><creatorcontrib>LI XIANZHONG</creatorcontrib><creatorcontrib>MIAO KAI</creatorcontrib><creatorcontrib>GUI JIANGBING</creatorcontrib><creatorcontrib>XIONG YUZHANG</creatorcontrib><creatorcontrib>CHEN QINGFENG</creatorcontrib><creatorcontrib>GUO YUANKUI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHOU XINLONG</au><au>WANG GUOQIU</au><au>WEI ZEHONG</au><au>ZHANG XIANZHONG</au><au>LI XIANZHONG</au><au>MIAO KAI</au><au>GUI JIANGBING</au><au>XIONG YUZHANG</au><au>CHEN QINGFENG</au><au>GUO YUANKUI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Deslagging and dephosphorizing method of electric stove</title><date>2010-01-06</date><risdate>2010</risdate><abstract>The invention relates to a deslagging and dephosphorizing method of an electric stove, which adopts the following public technical scheme: slagging; deslagging for the first time; smelting by blowing oxygen, starting to deslag when the temperature of molten steel increases to 1500-1510 DEG C, and controlling the weight percentage of phosphorus to decrease to be not more than 0.015 percent; slagging for the second time; deslagging for the second time, i.e. starting to deslag for the second time when the temperature of molten steel increases to 1520-1550 DEG C, and controlling the weight percentage of the phosphorus to decrease to be not more than 0.010 percent; slagging for the third time; deslagging for the third time, and controlling the weight percentage of the phosphorus to decrease to be not more than 0.005 percent; slagging for the fourth time; and preserving heat by blowing oxygen, adopting steel and slag residual operation with a tapping amount accounting for 85-90 percent of the total capacity of the</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN101619377A
source esp@cenet
subjects CHEMISTRY
METALLURGY
METALLURGY OF IRON
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
title Deslagging and dephosphorizing method of electric stove
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-28T20%3A22%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHOU%20XINLONG&rft.date=2010-01-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN101619377A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true