Method for preparing vinyl chloride using dichloroethane as raw material

The invention discloses a method for preparing vinyl chloride using dichloroethane as raw material, comprising the following steps: feeding gaseous dichloroethane of 245-265 DEG C and 2.9-3.5 Mpa into a cracking furnace for cracking at 470-500 DEG C, then obtaining mixture of dichloroethane, vinyl c...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG JUNJUN, CHEN JIANG, TANG QUANXING, TANG LIANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHANG JUNJUN
CHEN JIANG
TANG QUANXING
TANG LIANG
description The invention discloses a method for preparing vinyl chloride using dichloroethane as raw material, comprising the following steps: feeding gaseous dichloroethane of 245-265 DEG C and 2.9-3.5 Mpa into a cracking furnace for cracking at 470-500 DEG C, then obtaining mixture of dichloroethane, vinyl chloride and hydrogen chloride, and feeding the mixture to the subsequent separation section to obtain vinyl chloride, wherein the detention time of the materials is 20-30 seconds in a cracking tube, the linear speed of the materials at the outlet of the cracking tube is 25-35 m/s, the diameter of the inlet is less than the diameter of the inlet, and the pressure difference of the materials at the inlet and outlet is 0.9-1.5 Mpa. The invention reduces the usage of fuel gas from 110 kg/t-vcm to 68 kg/t-vcm, increases the yield of vinyl chloride by about 15%, and prolongs the decoking period of the cracking furnace from 4-5 months to 8-10 months.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN101514139A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN101514139A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN101514139A3</originalsourceid><addsrcrecordid>eNrjZPDwTS3JyE9RSMsvUigoSi1ILMrMS1coy8yrzFFIzsjJL8pMSVUoLQYJpmSCBfKBGhLzUhUSixWKEssVchNLUosyE3N4GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hgaGpoYmhsaWjMTFqAMfUNIk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing vinyl chloride using dichloroethane as raw material</title><source>esp@cenet</source><creator>ZHANG JUNJUN ; CHEN JIANG ; TANG QUANXING ; TANG LIANG</creator><creatorcontrib>ZHANG JUNJUN ; CHEN JIANG ; TANG QUANXING ; TANG LIANG</creatorcontrib><description>The invention discloses a method for preparing vinyl chloride using dichloroethane as raw material, comprising the following steps: feeding gaseous dichloroethane of 245-265 DEG C and 2.9-3.5 Mpa into a cracking furnace for cracking at 470-500 DEG C, then obtaining mixture of dichloroethane, vinyl chloride and hydrogen chloride, and feeding the mixture to the subsequent separation section to obtain vinyl chloride, wherein the detention time of the materials is 20-30 seconds in a cracking tube, the linear speed of the materials at the outlet of the cracking tube is 25-35 m/s, the diameter of the inlet is less than the diameter of the inlet, and the pressure difference of the materials at the inlet and outlet is 0.9-1.5 Mpa. The invention reduces the usage of fuel gas from 110 kg/t-vcm to 68 kg/t-vcm, increases the yield of vinyl chloride by about 15%, and prolongs the decoking period of the cracking furnace from 4-5 months to 8-10 months.</description><language>chi ; eng</language><subject>ACYCLIC OR CARBOCYCLIC COMPOUNDS ; CHEMISTRY ; METALLURGY ; ORGANIC CHEMISTRY</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090826&amp;DB=EPODOC&amp;CC=CN&amp;NR=101514139A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20090826&amp;DB=EPODOC&amp;CC=CN&amp;NR=101514139A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG JUNJUN</creatorcontrib><creatorcontrib>CHEN JIANG</creatorcontrib><creatorcontrib>TANG QUANXING</creatorcontrib><creatorcontrib>TANG LIANG</creatorcontrib><title>Method for preparing vinyl chloride using dichloroethane as raw material</title><description>The invention discloses a method for preparing vinyl chloride using dichloroethane as raw material, comprising the following steps: feeding gaseous dichloroethane of 245-265 DEG C and 2.9-3.5 Mpa into a cracking furnace for cracking at 470-500 DEG C, then obtaining mixture of dichloroethane, vinyl chloride and hydrogen chloride, and feeding the mixture to the subsequent separation section to obtain vinyl chloride, wherein the detention time of the materials is 20-30 seconds in a cracking tube, the linear speed of the materials at the outlet of the cracking tube is 25-35 m/s, the diameter of the inlet is less than the diameter of the inlet, and the pressure difference of the materials at the inlet and outlet is 0.9-1.5 Mpa. The invention reduces the usage of fuel gas from 110 kg/t-vcm to 68 kg/t-vcm, increases the yield of vinyl chloride by about 15%, and prolongs the decoking period of the cracking furnace from 4-5 months to 8-10 months.</description><subject>ACYCLIC OR CARBOCYCLIC COMPOUNDS</subject><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>ORGANIC CHEMISTRY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPDwTS3JyE9RSMsvUigoSi1ILMrMS1coy8yrzFFIzsjJL8pMSVUoLQYJpmSCBfKBGhLzUhUSixWKEssVchNLUosyE3N4GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hgaGpoYmhsaWjMTFqAMfUNIk</recordid><startdate>20090826</startdate><enddate>20090826</enddate><creator>ZHANG JUNJUN</creator><creator>CHEN JIANG</creator><creator>TANG QUANXING</creator><creator>TANG LIANG</creator><scope>EVB</scope></search><sort><creationdate>20090826</creationdate><title>Method for preparing vinyl chloride using dichloroethane as raw material</title><author>ZHANG JUNJUN ; CHEN JIANG ; TANG QUANXING ; TANG LIANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN101514139A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2009</creationdate><topic>ACYCLIC OR CARBOCYCLIC COMPOUNDS</topic><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>ORGANIC CHEMISTRY</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG JUNJUN</creatorcontrib><creatorcontrib>CHEN JIANG</creatorcontrib><creatorcontrib>TANG QUANXING</creatorcontrib><creatorcontrib>TANG LIANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG JUNJUN</au><au>CHEN JIANG</au><au>TANG QUANXING</au><au>TANG LIANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing vinyl chloride using dichloroethane as raw material</title><date>2009-08-26</date><risdate>2009</risdate><abstract>The invention discloses a method for preparing vinyl chloride using dichloroethane as raw material, comprising the following steps: feeding gaseous dichloroethane of 245-265 DEG C and 2.9-3.5 Mpa into a cracking furnace for cracking at 470-500 DEG C, then obtaining mixture of dichloroethane, vinyl chloride and hydrogen chloride, and feeding the mixture to the subsequent separation section to obtain vinyl chloride, wherein the detention time of the materials is 20-30 seconds in a cracking tube, the linear speed of the materials at the outlet of the cracking tube is 25-35 m/s, the diameter of the inlet is less than the diameter of the inlet, and the pressure difference of the materials at the inlet and outlet is 0.9-1.5 Mpa. The invention reduces the usage of fuel gas from 110 kg/t-vcm to 68 kg/t-vcm, increases the yield of vinyl chloride by about 15%, and prolongs the decoking period of the cracking furnace from 4-5 months to 8-10 months.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN101514139A
source esp@cenet
subjects ACYCLIC OR CARBOCYCLIC COMPOUNDS
CHEMISTRY
METALLURGY
ORGANIC CHEMISTRY
title Method for preparing vinyl chloride using dichloroethane as raw material
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T23%3A36%3A06IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20JUNJUN&rft.date=2009-08-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN101514139A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true