Waterproof resin
The invention discloses a waterproof resin. The waterproof resin comprises the following components in weight percentages: 14-19% of soya oil acid, 7-13% of glycerol, 8-15% of phthalic anhydride, 2-6% of fumaric acid, 1-4% of pentaerythritol, 4-10% of rosin, 1-5% of E-20 epoxy resin, 0.1-0.5% of hyp...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | TAN JIANSHENG |
description | The invention discloses a waterproof resin. The waterproof resin comprises the following components in weight percentages: 14-19% of soya oil acid, 7-13% of glycerol, 8-15% of phthalic anhydride, 2-6% of fumaric acid, 1-4% of pentaerythritol, 4-10% of rosin, 1-5% of E-20 epoxy resin, 0.1-0.5% of hypophosphorous acid, 2-6% of xylene and 40-50% of toluene; the preparation comprises the following steps: diluting the glycerol with water; adding the soya oil acid, the glycerol, the phthalic anhydride, the fumaric acid, the pentaerythritol, the rosin, the E-20 epoxy resin and the hypophosphorous acid; adding 20%-50% of the xylene to react for 0.5-1.5 hours at 170 DEG C, adding the rest xylene to react for 0.5-1.5 hours at 180 DEG C; heating to 204-208 DEG C, cooling after refluxing to an acid value not more than 4mgKOH/g and viscosity not less than 3sec/grille with water; and using toluene to dilute reaction product after cooling to below 150 DEG C. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN101503509A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN101503509A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN101503509A3</originalsourceid><addsrcrecordid>eNrjZBAITyxJLSooys9PUyhKLc7M42FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hgaGpgbGpgaWjsbEqAEAtyYfUQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Waterproof resin</title><source>esp@cenet</source><creator>TAN JIANSHENG</creator><creatorcontrib>TAN JIANSHENG</creatorcontrib><description>The invention discloses a waterproof resin. The waterproof resin comprises the following components in weight percentages: 14-19% of soya oil acid, 7-13% of glycerol, 8-15% of phthalic anhydride, 2-6% of fumaric acid, 1-4% of pentaerythritol, 4-10% of rosin, 1-5% of E-20 epoxy resin, 0.1-0.5% of hypophosphorous acid, 2-6% of xylene and 40-50% of toluene; the preparation comprises the following steps: diluting the glycerol with water; adding the soya oil acid, the glycerol, the phthalic anhydride, the fumaric acid, the pentaerythritol, the rosin, the E-20 epoxy resin and the hypophosphorous acid; adding 20%-50% of the xylene to react for 0.5-1.5 hours at 170 DEG C, adding the rest xylene to react for 0.5-1.5 hours at 180 DEG C; heating to 204-208 DEG C, cooling after refluxing to an acid value not more than 4mgKOH/g and viscosity not less than 3sec/grille with water; and using toluene to dilute reaction product after cooling to below 150 DEG C.</description><language>chi ; eng</language><subject>ADHESIVES ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; DYES ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; POLISHES ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090812&DB=EPODOC&CC=CN&NR=101503509A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090812&DB=EPODOC&CC=CN&NR=101503509A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAN JIANSHENG</creatorcontrib><title>Waterproof resin</title><description>The invention discloses a waterproof resin. The waterproof resin comprises the following components in weight percentages: 14-19% of soya oil acid, 7-13% of glycerol, 8-15% of phthalic anhydride, 2-6% of fumaric acid, 1-4% of pentaerythritol, 4-10% of rosin, 1-5% of E-20 epoxy resin, 0.1-0.5% of hypophosphorous acid, 2-6% of xylene and 40-50% of toluene; the preparation comprises the following steps: diluting the glycerol with water; adding the soya oil acid, the glycerol, the phthalic anhydride, the fumaric acid, the pentaerythritol, the rosin, the E-20 epoxy resin and the hypophosphorous acid; adding 20%-50% of the xylene to react for 0.5-1.5 hours at 170 DEG C, adding the rest xylene to react for 0.5-1.5 hours at 180 DEG C; heating to 204-208 DEG C, cooling after refluxing to an acid value not more than 4mgKOH/g and viscosity not less than 3sec/grille with water; and using toluene to dilute reaction product after cooling to below 150 DEG C.</description><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>DYES</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBAITyxJLSooys9PUyhKLc7M42FgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hgaGpgbGpgaWjsbEqAEAtyYfUQ</recordid><startdate>20090812</startdate><enddate>20090812</enddate><creator>TAN JIANSHENG</creator><scope>EVB</scope></search><sort><creationdate>20090812</creationdate><title>Waterproof resin</title><author>TAN JIANSHENG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN101503509A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2009</creationdate><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>DYES</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>TAN JIANSHENG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAN JIANSHENG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Waterproof resin</title><date>2009-08-12</date><risdate>2009</risdate><abstract>The invention discloses a waterproof resin. The waterproof resin comprises the following components in weight percentages: 14-19% of soya oil acid, 7-13% of glycerol, 8-15% of phthalic anhydride, 2-6% of fumaric acid, 1-4% of pentaerythritol, 4-10% of rosin, 1-5% of E-20 epoxy resin, 0.1-0.5% of hypophosphorous acid, 2-6% of xylene and 40-50% of toluene; the preparation comprises the following steps: diluting the glycerol with water; adding the soya oil acid, the glycerol, the phthalic anhydride, the fumaric acid, the pentaerythritol, the rosin, the E-20 epoxy resin and the hypophosphorous acid; adding 20%-50% of the xylene to react for 0.5-1.5 hours at 170 DEG C, adding the rest xylene to react for 0.5-1.5 hours at 180 DEG C; heating to 204-208 DEG C, cooling after refluxing to an acid value not more than 4mgKOH/g and viscosity not less than 3sec/grille with water; and using toluene to dilute reaction product after cooling to below 150 DEG C.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN101503509A |
source | esp@cenet |
subjects | ADHESIVES CHEMISTRY COMPOSITIONS BASED THEREON DYES MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS ORGANIC MACROMOLECULAR COMPOUNDS PAINTS POLISHES THEIR PREPARATION OR CHEMICAL WORKING-UP |
title | Waterproof resin |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-03T03%3A09%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAN%20JIANSHENG&rft.date=2009-08-12&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN101503509A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |