Steel-smelting revolving furnace smoke canal weld deposit process
The invention discloses a surfacing process method for a flue of a steelmaking converter. After the flue is subject to an integral pressure test, the rust removal is performed; before welding, a welding position of the flue is subject to water cooling; a selected nickel-base alloy welding wire conta...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | HUANG CONGSHI HU JIAQUAN |
description | The invention discloses a surfacing process method for a flue of a steelmaking converter. After the flue is subject to an integral pressure test, the rust removal is performed; before welding, a welding position of the flue is subject to water cooling; a selected nickel-base alloy welding wire contains 60 to 65 percent of Ni and 20 to 23 percent of Cr; the current and the voltage of a welding machine are adjusted; the welding current is selected to be between 110 and 200A, and the voltage is selected to between 22 and 26V; the MIG welding is adopted, and protective gas is Ar gas or mixed gas of Ar and He; and the gas flow is controlled to between 12 and 16L/min. The surfacing process method realizes the thin surfacing the surfacing layer thickness of which is between 1.78 and 2.50 mm. The surface of a surfacing layer is uniform and smooth, and has no phenomena of cracks, slag inclusion, air holes, and missing welding. After the successful surfacing is performed on the flue of the steelmaking converter, the se |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN101402152BB</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN101402152BB</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN101402152BB3</originalsourceid><addsrcrecordid>eNrjZHAMLklNzdEtzk3NKcnMS1coSi3LzykDsdJKi_ISk1MVinPzs1MVkhPzEnMUylNzUhRSUgvyizNLFAqK8pNTi4t5GFjTEnOKU3mhNDeDkptriLOHLlBZfGpxAdCMvNSSeGc_QwNDEwMjQ1MjJydjohQBAJtHMn4</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Steel-smelting revolving furnace smoke canal weld deposit process</title><source>esp@cenet</source><creator>HUANG CONGSHI ; HU JIAQUAN</creator><creatorcontrib>HUANG CONGSHI ; HU JIAQUAN</creatorcontrib><description>The invention discloses a surfacing process method for a flue of a steelmaking converter. After the flue is subject to an integral pressure test, the rust removal is performed; before welding, a welding position of the flue is subject to water cooling; a selected nickel-base alloy welding wire contains 60 to 65 percent of Ni and 20 to 23 percent of Cr; the current and the voltage of a welding machine are adjusted; the welding current is selected to be between 110 and 200A, and the voltage is selected to between 22 and 26V; the MIG welding is adopted, and protective gas is Ar gas or mixed gas of Ar and He; and the gas flow is controlled to between 12 and 16L/min. The surfacing process method realizes the thin surfacing the surfacing layer thickness of which is between 1.78 and 2.50 mm. The surface of a surfacing layer is uniform and smooth, and has no phenomena of cracks, slag inclusion, air holes, and missing welding. After the successful surfacing is performed on the flue of the steelmaking converter, the se</description><language>chi ; eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2010</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20101124&DB=EPODOC&CC=CN&NR=101402152B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20101124&DB=EPODOC&CC=CN&NR=101402152B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HUANG CONGSHI</creatorcontrib><creatorcontrib>HU JIAQUAN</creatorcontrib><title>Steel-smelting revolving furnace smoke canal weld deposit process</title><description>The invention discloses a surfacing process method for a flue of a steelmaking converter. After the flue is subject to an integral pressure test, the rust removal is performed; before welding, a welding position of the flue is subject to water cooling; a selected nickel-base alloy welding wire contains 60 to 65 percent of Ni and 20 to 23 percent of Cr; the current and the voltage of a welding machine are adjusted; the welding current is selected to be between 110 and 200A, and the voltage is selected to between 22 and 26V; the MIG welding is adopted, and protective gas is Ar gas or mixed gas of Ar and He; and the gas flow is controlled to between 12 and 16L/min. The surfacing process method realizes the thin surfacing the surfacing layer thickness of which is between 1.78 and 2.50 mm. The surface of a surfacing layer is uniform and smooth, and has no phenomena of cracks, slag inclusion, air holes, and missing welding. After the successful surfacing is performed on the flue of the steelmaking converter, the se</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2010</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAMLklNzdEtzk3NKcnMS1coSi3LzykDsdJKi_ISk1MVinPzs1MVkhPzEnMUylNzUhRSUgvyizNLFAqK8pNTi4t5GFjTEnOKU3mhNDeDkptriLOHLlBZfGpxAdCMvNSSeGc_QwNDEwMjQ1MjJydjohQBAJtHMn4</recordid><startdate>20101124</startdate><enddate>20101124</enddate><creator>HUANG CONGSHI</creator><creator>HU JIAQUAN</creator><scope>EVB</scope></search><sort><creationdate>20101124</creationdate><title>Steel-smelting revolving furnace smoke canal weld deposit process</title><author>HUANG CONGSHI ; HU JIAQUAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN101402152BB3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2010</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>HUANG CONGSHI</creatorcontrib><creatorcontrib>HU JIAQUAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HUANG CONGSHI</au><au>HU JIAQUAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Steel-smelting revolving furnace smoke canal weld deposit process</title><date>2010-11-24</date><risdate>2010</risdate><abstract>The invention discloses a surfacing process method for a flue of a steelmaking converter. After the flue is subject to an integral pressure test, the rust removal is performed; before welding, a welding position of the flue is subject to water cooling; a selected nickel-base alloy welding wire contains 60 to 65 percent of Ni and 20 to 23 percent of Cr; the current and the voltage of a welding machine are adjusted; the welding current is selected to be between 110 and 200A, and the voltage is selected to between 22 and 26V; the MIG welding is adopted, and protective gas is Ar gas or mixed gas of Ar and He; and the gas flow is controlled to between 12 and 16L/min. The surfacing process method realizes the thin surfacing the surfacing layer thickness of which is between 1.78 and 2.50 mm. The surface of a surfacing layer is uniform and smooth, and has no phenomena of cracks, slag inclusion, air holes, and missing welding. After the successful surfacing is performed on the flue of the steelmaking converter, the se</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN101402152BB |
source | esp@cenet |
subjects | CLADDING OR PLATING BY SOLDERING OR WELDING CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR PERFORMING OPERATIONS SOLDERING OR UNSOLDERING TRANSPORTING WELDING WORKING BY LASER BEAM |
title | Steel-smelting revolving furnace smoke canal weld deposit process |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T11%3A07%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HUANG%20CONGSHI&rft.date=2010-11-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN101402152BB%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |