Methods of fabricating flat glass with low levels of warp

A method of fabricating glass sheets (13) is provided in which the sheets are cut from a glass ribbon (15) composed of a glass having a glass transition temperature range (GTTR). The ribbon (15) is formed by a drawing process in which edge rollers (27a,27b) contact the glass ribbon (15) at a locatio...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NOVAK ROBERT A, SHAY CLINTON G, BLEVINS JOHN DAVID
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator NOVAK ROBERT A
SHAY CLINTON G
BLEVINS JOHN DAVID
description A method of fabricating glass sheets (13) is provided in which the sheets are cut from a glass ribbon (15) composed of a glass having a glass transition temperature range (GTTR). The ribbon (15) is formed by a drawing process in which edge rollers (27a,27b) contact the glass ribbon (15) at a location along the length of the ribbon where the temperature along the center line (17) of the ribbon (15) is above the GTTR. The edge rollers (27a, 27b) locally cool the ribbon (15), and the cooling produces a sine wave type buckling (S warp) along the edges of the glass sheets (13). The S warp is reduced or eliminated by heating the bead portions (21a, 21b) of the ribbon (15) and/or portions of the ribbon (the S warp portions 25a and 25b) which are located next to the bead portions (21a, 21b) and/or by cooling the center portion of the ribbon (15) at least one location along the length of the ribbon (15) where the temperature at the ribbon's center line (17) is within the GTTR.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN101312918BB</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN101312918BB</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN101312918BB3</originalsourceid><addsrcrecordid>eNrjZLD0TS3JyE8pVshPU0hLTCrKTE4sycxLV0jLSSxRSM9JLC5WKM8syVDIyS9XyEktS80BqyxPLCrgYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxzn6GBobGhkaWhhZOTsZEKQIAcpwuyA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Methods of fabricating flat glass with low levels of warp</title><source>esp@cenet</source><creator>NOVAK ROBERT A ; SHAY CLINTON G ; BLEVINS JOHN DAVID</creator><creatorcontrib>NOVAK ROBERT A ; SHAY CLINTON G ; BLEVINS JOHN DAVID</creatorcontrib><description>A method of fabricating glass sheets (13) is provided in which the sheets are cut from a glass ribbon (15) composed of a glass having a glass transition temperature range (GTTR). The ribbon (15) is formed by a drawing process in which edge rollers (27a,27b) contact the glass ribbon (15) at a location along the length of the ribbon where the temperature along the center line (17) of the ribbon (15) is above the GTTR. The edge rollers (27a, 27b) locally cool the ribbon (15), and the cooling produces a sine wave type buckling (S warp) along the edges of the glass sheets (13). The S warp is reduced or eliminated by heating the bead portions (21a, 21b) of the ribbon (15) and/or portions of the ribbon (the S warp portions 25a and 25b) which are located next to the bead portions (21a, 21b) and/or by cooling the center portion of the ribbon (15) at least one location along the length of the ribbon (15) where the temperature at the ribbon's center line (17) is within the GTTR.</description><language>chi ; eng</language><subject>CHEMISTRY ; GLASS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120404&amp;DB=EPODOC&amp;CC=CN&amp;NR=101312918B$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120404&amp;DB=EPODOC&amp;CC=CN&amp;NR=101312918B$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>NOVAK ROBERT A</creatorcontrib><creatorcontrib>SHAY CLINTON G</creatorcontrib><creatorcontrib>BLEVINS JOHN DAVID</creatorcontrib><title>Methods of fabricating flat glass with low levels of warp</title><description>A method of fabricating glass sheets (13) is provided in which the sheets are cut from a glass ribbon (15) composed of a glass having a glass transition temperature range (GTTR). The ribbon (15) is formed by a drawing process in which edge rollers (27a,27b) contact the glass ribbon (15) at a location along the length of the ribbon where the temperature along the center line (17) of the ribbon (15) is above the GTTR. The edge rollers (27a, 27b) locally cool the ribbon (15), and the cooling produces a sine wave type buckling (S warp) along the edges of the glass sheets (13). The S warp is reduced or eliminated by heating the bead portions (21a, 21b) of the ribbon (15) and/or portions of the ribbon (the S warp portions 25a and 25b) which are located next to the bead portions (21a, 21b) and/or by cooling the center portion of the ribbon (15) at least one location along the length of the ribbon (15) where the temperature at the ribbon's center line (17) is within the GTTR.</description><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLD0TS3JyE8pVshPU0hLTCrKTE4sycxLV0jLSSxRSM9JLC5WKM8syVDIyS9XyEktS80BqyxPLCrgYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxzn6GBobGhkaWhhZOTsZEKQIAcpwuyA</recordid><startdate>20120404</startdate><enddate>20120404</enddate><creator>NOVAK ROBERT A</creator><creator>SHAY CLINTON G</creator><creator>BLEVINS JOHN DAVID</creator><scope>EVB</scope></search><sort><creationdate>20120404</creationdate><title>Methods of fabricating flat glass with low levels of warp</title><author>NOVAK ROBERT A ; SHAY CLINTON G ; BLEVINS JOHN DAVID</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN101312918BB3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2012</creationdate><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><toplevel>online_resources</toplevel><creatorcontrib>NOVAK ROBERT A</creatorcontrib><creatorcontrib>SHAY CLINTON G</creatorcontrib><creatorcontrib>BLEVINS JOHN DAVID</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>NOVAK ROBERT A</au><au>SHAY CLINTON G</au><au>BLEVINS JOHN DAVID</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Methods of fabricating flat glass with low levels of warp</title><date>2012-04-04</date><risdate>2012</risdate><abstract>A method of fabricating glass sheets (13) is provided in which the sheets are cut from a glass ribbon (15) composed of a glass having a glass transition temperature range (GTTR). The ribbon (15) is formed by a drawing process in which edge rollers (27a,27b) contact the glass ribbon (15) at a location along the length of the ribbon where the temperature along the center line (17) of the ribbon (15) is above the GTTR. The edge rollers (27a, 27b) locally cool the ribbon (15), and the cooling produces a sine wave type buckling (S warp) along the edges of the glass sheets (13). The S warp is reduced or eliminated by heating the bead portions (21a, 21b) of the ribbon (15) and/or portions of the ribbon (the S warp portions 25a and 25b) which are located next to the bead portions (21a, 21b) and/or by cooling the center portion of the ribbon (15) at least one location along the length of the ribbon (15) where the temperature at the ribbon's center line (17) is within the GTTR.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN101312918BB
source esp@cenet
subjects CHEMISTRY
GLASS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
title Methods of fabricating flat glass with low levels of warp
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T12%3A49%3A43IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=NOVAK%20ROBERT%20A&rft.date=2012-04-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN101312918BB%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true