Reignition method for base aluminum groove

A secondary starting method for a seat aluminum slot relates to a secondary starting method of an electrobath during an aluminum electrolyzing manufacture process which is characterized by after carrying out washing, complementing, arranging into a furnace and baking on the electrobath in turn, irri...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BIAN HANGUO, WU ZHIMING, WANG KEYUAN, YAN TAIWANG, HUANG QIAO, ZHANG HENGCHENG, LI FANGKUAI, QI HESHENG, WANG QUN, DUAN YALI, LI DENGFENG, XU WEIDONG, DAI JUN, ZHAO TIANDE, HU JINPING
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator BIAN HANGUO
WU ZHIMING
WANG KEYUAN
YAN TAIWANG
HUANG QIAO
ZHANG HENGCHENG
LI FANGKUAI
QI HESHENG
WANG QUN
DUAN YALI
LI DENGFENG
XU WEIDONG
DAI JUN
ZHAO TIANDE
HU JINPING
description A secondary starting method for a seat aluminum slot relates to a secondary starting method of an electrobath during an aluminum electrolyzing manufacture process which is characterized by after carrying out washing, complementing, arranging into a furnace and baking on the electrobath in turn, irrigating an aluminum liquid into the electrobath in 23 to 24 hours during transferring from baking to starting and the voltage rises to 6 to 6.5v in 2 to 3 hours after irrigating the aluminum liquid; uniformly decreasing the voltage 6 to 6.5v to 4.5 to 4.8v in 2 to 3 hours after irrigating the aluminum, controlling the voltage to be uniformly decreased from 4.5 to 4.8V to 4.3 to 4.5 V in 24 hours, then uniformly decreasing the voltage to 4.2 to 4.3V again in 24 to 48hours, then uniformly decreasing the voltage to 4.18 to 4.2V again in 48 to72hours again, then uniformly decreasing the voltage to 4.16 to 4.18V again in 72 to 96hours, maintaining the voltage in 4.10 to 4.16V in 96 to 120 hours, then entering into an ana
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN101270481A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN101270481A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN101270481A3</originalsourceid><addsrcrecordid>eNrjZNAKSs1Mz8ssyczPU8hNLcnIT1FIyy9SSEosTlVIzCnNzcwrzVVIL8rPL0vlYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBoZG5gYmFoaOxsSoAQA7iCkW</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Reignition method for base aluminum groove</title><source>esp@cenet</source><creator>BIAN HANGUO ; WU ZHIMING ; WANG KEYUAN ; YAN TAIWANG ; HUANG QIAO ; ZHANG HENGCHENG ; LI FANGKUAI ; QI HESHENG ; WANG QUN ; DUAN YALI ; LI DENGFENG ; XU WEIDONG ; DAI JUN ; ZHAO TIANDE ; HU JINPING</creator><creatorcontrib>BIAN HANGUO ; WU ZHIMING ; WANG KEYUAN ; YAN TAIWANG ; HUANG QIAO ; ZHANG HENGCHENG ; LI FANGKUAI ; QI HESHENG ; WANG QUN ; DUAN YALI ; LI DENGFENG ; XU WEIDONG ; DAI JUN ; ZHAO TIANDE ; HU JINPING</creatorcontrib><description>A secondary starting method for a seat aluminum slot relates to a secondary starting method of an electrobath during an aluminum electrolyzing manufacture process which is characterized by after carrying out washing, complementing, arranging into a furnace and baking on the electrobath in turn, irrigating an aluminum liquid into the electrobath in 23 to 24 hours during transferring from baking to starting and the voltage rises to 6 to 6.5v in 2 to 3 hours after irrigating the aluminum liquid; uniformly decreasing the voltage 6 to 6.5v to 4.5 to 4.8v in 2 to 3 hours after irrigating the aluminum, controlling the voltage to be uniformly decreased from 4.5 to 4.8V to 4.3 to 4.5 V in 24 hours, then uniformly decreasing the voltage to 4.2 to 4.3V again in 24 to 48hours, then uniformly decreasing the voltage to 4.18 to 4.2V again in 48 to72hours again, then uniformly decreasing the voltage to 4.16 to 4.18V again in 72 to 96hours, maintaining the voltage in 4.10 to 4.16V in 96 to 120 hours, then entering into an ana</description><language>chi ; eng</language><subject>APPARATUS THEREFOR ; CHEMISTRY ; ELECTROLYTIC OR ELECTROPHORETIC PROCESSES ; METALLURGY ; PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</subject><creationdate>2008</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20080924&amp;DB=EPODOC&amp;CC=CN&amp;NR=101270481A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20080924&amp;DB=EPODOC&amp;CC=CN&amp;NR=101270481A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>BIAN HANGUO</creatorcontrib><creatorcontrib>WU ZHIMING</creatorcontrib><creatorcontrib>WANG KEYUAN</creatorcontrib><creatorcontrib>YAN TAIWANG</creatorcontrib><creatorcontrib>HUANG QIAO</creatorcontrib><creatorcontrib>ZHANG HENGCHENG</creatorcontrib><creatorcontrib>LI FANGKUAI</creatorcontrib><creatorcontrib>QI HESHENG</creatorcontrib><creatorcontrib>WANG QUN</creatorcontrib><creatorcontrib>DUAN YALI</creatorcontrib><creatorcontrib>LI DENGFENG</creatorcontrib><creatorcontrib>XU WEIDONG</creatorcontrib><creatorcontrib>DAI JUN</creatorcontrib><creatorcontrib>ZHAO TIANDE</creatorcontrib><creatorcontrib>HU JINPING</creatorcontrib><title>Reignition method for base aluminum groove</title><description>A secondary starting method for a seat aluminum slot relates to a secondary starting method of an electrobath during an aluminum electrolyzing manufacture process which is characterized by after carrying out washing, complementing, arranging into a furnace and baking on the electrobath in turn, irrigating an aluminum liquid into the electrobath in 23 to 24 hours during transferring from baking to starting and the voltage rises to 6 to 6.5v in 2 to 3 hours after irrigating the aluminum liquid; uniformly decreasing the voltage 6 to 6.5v to 4.5 to 4.8v in 2 to 3 hours after irrigating the aluminum, controlling the voltage to be uniformly decreased from 4.5 to 4.8V to 4.3 to 4.5 V in 24 hours, then uniformly decreasing the voltage to 4.2 to 4.3V again in 24 to 48hours, then uniformly decreasing the voltage to 4.18 to 4.2V again in 48 to72hours again, then uniformly decreasing the voltage to 4.16 to 4.18V again in 72 to 96hours, maintaining the voltage in 4.10 to 4.16V in 96 to 120 hours, then entering into an ana</description><subject>APPARATUS THEREFOR</subject><subject>CHEMISTRY</subject><subject>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</subject><subject>METALLURGY</subject><subject>PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2008</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNAKSs1Mz8ssyczPU8hNLcnIT1FIyy9SSEosTlVIzCnNzcwrzVVIL8rPL0vlYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GBoZG5gYmFoaOxsSoAQA7iCkW</recordid><startdate>20080924</startdate><enddate>20080924</enddate><creator>BIAN HANGUO</creator><creator>WU ZHIMING</creator><creator>WANG KEYUAN</creator><creator>YAN TAIWANG</creator><creator>HUANG QIAO</creator><creator>ZHANG HENGCHENG</creator><creator>LI FANGKUAI</creator><creator>QI HESHENG</creator><creator>WANG QUN</creator><creator>DUAN YALI</creator><creator>LI DENGFENG</creator><creator>XU WEIDONG</creator><creator>DAI JUN</creator><creator>ZHAO TIANDE</creator><creator>HU JINPING</creator><scope>EVB</scope></search><sort><creationdate>20080924</creationdate><title>Reignition method for base aluminum groove</title><author>BIAN HANGUO ; WU ZHIMING ; WANG KEYUAN ; YAN TAIWANG ; HUANG QIAO ; ZHANG HENGCHENG ; LI FANGKUAI ; QI HESHENG ; WANG QUN ; DUAN YALI ; LI DENGFENG ; XU WEIDONG ; DAI JUN ; ZHAO TIANDE ; HU JINPING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN101270481A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2008</creationdate><topic>APPARATUS THEREFOR</topic><topic>CHEMISTRY</topic><topic>ELECTROLYTIC OR ELECTROPHORETIC PROCESSES</topic><topic>METALLURGY</topic><topic>PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>BIAN HANGUO</creatorcontrib><creatorcontrib>WU ZHIMING</creatorcontrib><creatorcontrib>WANG KEYUAN</creatorcontrib><creatorcontrib>YAN TAIWANG</creatorcontrib><creatorcontrib>HUANG QIAO</creatorcontrib><creatorcontrib>ZHANG HENGCHENG</creatorcontrib><creatorcontrib>LI FANGKUAI</creatorcontrib><creatorcontrib>QI HESHENG</creatorcontrib><creatorcontrib>WANG QUN</creatorcontrib><creatorcontrib>DUAN YALI</creatorcontrib><creatorcontrib>LI DENGFENG</creatorcontrib><creatorcontrib>XU WEIDONG</creatorcontrib><creatorcontrib>DAI JUN</creatorcontrib><creatorcontrib>ZHAO TIANDE</creatorcontrib><creatorcontrib>HU JINPING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>BIAN HANGUO</au><au>WU ZHIMING</au><au>WANG KEYUAN</au><au>YAN TAIWANG</au><au>HUANG QIAO</au><au>ZHANG HENGCHENG</au><au>LI FANGKUAI</au><au>QI HESHENG</au><au>WANG QUN</au><au>DUAN YALI</au><au>LI DENGFENG</au><au>XU WEIDONG</au><au>DAI JUN</au><au>ZHAO TIANDE</au><au>HU JINPING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Reignition method for base aluminum groove</title><date>2008-09-24</date><risdate>2008</risdate><abstract>A secondary starting method for a seat aluminum slot relates to a secondary starting method of an electrobath during an aluminum electrolyzing manufacture process which is characterized by after carrying out washing, complementing, arranging into a furnace and baking on the electrobath in turn, irrigating an aluminum liquid into the electrobath in 23 to 24 hours during transferring from baking to starting and the voltage rises to 6 to 6.5v in 2 to 3 hours after irrigating the aluminum liquid; uniformly decreasing the voltage 6 to 6.5v to 4.5 to 4.8v in 2 to 3 hours after irrigating the aluminum, controlling the voltage to be uniformly decreased from 4.5 to 4.8V to 4.3 to 4.5 V in 24 hours, then uniformly decreasing the voltage to 4.2 to 4.3V again in 24 to 48hours, then uniformly decreasing the voltage to 4.18 to 4.2V again in 48 to72hours again, then uniformly decreasing the voltage to 4.16 to 4.18V again in 72 to 96hours, maintaining the voltage in 4.10 to 4.16V in 96 to 120 hours, then entering into an ana</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN101270481A
source esp@cenet
subjects APPARATUS THEREFOR
CHEMISTRY
ELECTROLYTIC OR ELECTROPHORETIC PROCESSES
METALLURGY
PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY ORREFINING OF METALS
title Reignition method for base aluminum groove
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-02T10%3A36%3A51IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=BIAN%20HANGUO&rft.date=2008-09-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN101270481A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true