Technique for directly smelting stainless steel from dephosphorization blast furnace molten iron in furnace
The invention provides a technique for dephosphorizing blast furnace iron melt in a furnace and directly smelting stainless steel, and the technique comprises following steps: firstly, dephosphorizing raw material iron melt which contains nickel and chrome in a blast furnace, enabling the content of...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | LIU SHENJIE LIU GUANGHUO |
description | The invention provides a technique for dephosphorizing blast furnace iron melt in a furnace and directly smelting stainless steel, and the technique comprises following steps: firstly, dephosphorizing raw material iron melt which contains nickel and chrome in a blast furnace, enabling the content of phosphor to be lower than 0.035%, adding quick lime slag 3-18% into molten steel each ton, secondly, adding nitrogen gas or argon gas and oxygen to use together, wherein the blowing oxygen quantity of the molten steel each ton is 0.8-2 cubic meters, the argon gas is 0.4-1.2 cubic meters, the nitrogen gas is 0.5-1.5 cubic meters, obtaining finished products, adding stainless steel pregnant antimony solution, and outputting the molten steel after the content of main components of the molten steel in an electric furnace reaches the following standards through slightly mixing. The standards are that chrome is 8-18%, nickel is 0.8-8.5%, manganese is 5.5-14%, copper is 1.5-3.2%, carbon is less than 0.15%, silicon is les |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN100577840CC</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN100577840CC</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN100577840CC3</originalsourceid><addsrcrecordid>eNqNirEOwjAMRLswIOAfLHakIkBlj0BMTN2r0DrUwnVK7A7w9WSAneF0p3dvXjxqbHuh54QQYoKOErbGL9AB2UjuoOZJGFXzQmQIKQ7Q4dhHzUn09kZR4MZeDcKUxLcIQ2RDAUr5IfnhZTELnhVX314U6_OpdpcNjrFBHbMiaI27bsvyUFXHfenc7i_pAwNTQws</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Technique for directly smelting stainless steel from dephosphorization blast furnace molten iron in furnace</title><source>esp@cenet</source><creator>LIU SHENJIE ; LIU GUANGHUO</creator><creatorcontrib>LIU SHENJIE ; LIU GUANGHUO</creatorcontrib><description>The invention provides a technique for dephosphorizing blast furnace iron melt in a furnace and directly smelting stainless steel, and the technique comprises following steps: firstly, dephosphorizing raw material iron melt which contains nickel and chrome in a blast furnace, enabling the content of phosphor to be lower than 0.035%, adding quick lime slag 3-18% into molten steel each ton, secondly, adding nitrogen gas or argon gas and oxygen to use together, wherein the blowing oxygen quantity of the molten steel each ton is 0.8-2 cubic meters, the argon gas is 0.4-1.2 cubic meters, the nitrogen gas is 0.5-1.5 cubic meters, obtaining finished products, adding stainless steel pregnant antimony solution, and outputting the molten steel after the content of main components of the molten steel in an electric furnace reaches the following standards through slightly mixing. The standards are that chrome is 8-18%, nickel is 0.8-8.5%, manganese is 5.5-14%, copper is 1.5-3.2%, carbon is less than 0.15%, silicon is les</description><language>chi ; eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; METALLURGY OF IRON ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2010</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20100106&DB=EPODOC&CC=CN&NR=100577840C$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20100106&DB=EPODOC&CC=CN&NR=100577840C$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU SHENJIE</creatorcontrib><creatorcontrib>LIU GUANGHUO</creatorcontrib><title>Technique for directly smelting stainless steel from dephosphorization blast furnace molten iron in furnace</title><description>The invention provides a technique for dephosphorizing blast furnace iron melt in a furnace and directly smelting stainless steel, and the technique comprises following steps: firstly, dephosphorizing raw material iron melt which contains nickel and chrome in a blast furnace, enabling the content of phosphor to be lower than 0.035%, adding quick lime slag 3-18% into molten steel each ton, secondly, adding nitrogen gas or argon gas and oxygen to use together, wherein the blowing oxygen quantity of the molten steel each ton is 0.8-2 cubic meters, the argon gas is 0.4-1.2 cubic meters, the nitrogen gas is 0.5-1.5 cubic meters, obtaining finished products, adding stainless steel pregnant antimony solution, and outputting the molten steel after the content of main components of the molten steel in an electric furnace reaches the following standards through slightly mixing. The standards are that chrome is 8-18%, nickel is 0.8-8.5%, manganese is 5.5-14%, copper is 1.5-3.2%, carbon is less than 0.15%, silicon is les</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2010</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNirEOwjAMRLswIOAfLHakIkBlj0BMTN2r0DrUwnVK7A7w9WSAneF0p3dvXjxqbHuh54QQYoKOErbGL9AB2UjuoOZJGFXzQmQIKQ7Q4dhHzUn09kZR4MZeDcKUxLcIQ2RDAUr5IfnhZTELnhVX314U6_OpdpcNjrFBHbMiaI27bsvyUFXHfenc7i_pAwNTQws</recordid><startdate>20100106</startdate><enddate>20100106</enddate><creator>LIU SHENJIE</creator><creator>LIU GUANGHUO</creator><scope>EVB</scope></search><sort><creationdate>20100106</creationdate><title>Technique for directly smelting stainless steel from dephosphorization blast furnace molten iron in furnace</title><author>LIU SHENJIE ; LIU GUANGHUO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN100577840CC3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2010</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU SHENJIE</creatorcontrib><creatorcontrib>LIU GUANGHUO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU SHENJIE</au><au>LIU GUANGHUO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Technique for directly smelting stainless steel from dephosphorization blast furnace molten iron in furnace</title><date>2010-01-06</date><risdate>2010</risdate><abstract>The invention provides a technique for dephosphorizing blast furnace iron melt in a furnace and directly smelting stainless steel, and the technique comprises following steps: firstly, dephosphorizing raw material iron melt which contains nickel and chrome in a blast furnace, enabling the content of phosphor to be lower than 0.035%, adding quick lime slag 3-18% into molten steel each ton, secondly, adding nitrogen gas or argon gas and oxygen to use together, wherein the blowing oxygen quantity of the molten steel each ton is 0.8-2 cubic meters, the argon gas is 0.4-1.2 cubic meters, the nitrogen gas is 0.5-1.5 cubic meters, obtaining finished products, adding stainless steel pregnant antimony solution, and outputting the molten steel after the content of main components of the molten steel in an electric furnace reaches the following standards through slightly mixing. The standards are that chrome is 8-18%, nickel is 0.8-8.5%, manganese is 5.5-14%, copper is 1.5-3.2%, carbon is less than 0.15%, silicon is les</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN100577840CC |
source | esp@cenet |
subjects | ALLOYS CHEMISTRY FERROUS OR NON-FERROUS ALLOYS METALLURGY METALLURGY OF IRON PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Technique for directly smelting stainless steel from dephosphorization blast furnace molten iron in furnace |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T17%3A06%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20SHENJIE&rft.date=2010-01-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN100577840CC%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |