METHOD FOR PRODUCING A PRECURSOR PITCH FOR CARBON FIBER
KAWASAKI STEEL 58-38,182 Precursor pitch to be used for formation of carbon fiber is produced by heating a coal tar soft or middle pitch at a temperature of 350-500.degree.C at a first stage to form mesophase, extracting the thus treated pitch with a solvent, separating and removing the solvent inso...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; fre |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | YUDATE, KOZO NAGASAWA, KEN |
description | KAWASAKI STEEL 58-38,182 Precursor pitch to be used for formation of carbon fiber is produced by heating a coal tar soft or middle pitch at a temperature of 350-500.degree.C at a first stage to form mesophase, extracting the thus treated pitch with a solvent, separating and removing the solvent insoluble portion including mesophase to obtain a pitch containing no free carbon and further at the second stage heat-treating the pitch containing no free carbon in an inert gas atmosphere under atmospheric pressure or a reduced pressure under the following condition 600-1.2 T ? 0 ? 1,800-3.6 T (provided that 350 ? T ? 500) wherein T(.degree.C) is the temperature of the heat treatment and .theta. (min) is the time for which said temperature is held, to form bulk mesophase pitch containing 20-60% by weight of quinoline insoluble portion. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CA1234548A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CA1234548A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CA1234548A3</originalsourceid><addsrcrecordid>eNrjZDD3dQ3x8HdRcPMPUggI8ncJdfb0c1dwBLJdnUODgkGiniHOHmB5Z8cgJ38_BTdPJ9cgHgbWtMSc4lReKM3NIO_mClSom1qQH59aXJCYnJqXWhLv7GhoZGxiamLhaExYBQCIECcL</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING A PRECURSOR PITCH FOR CARBON FIBER</title><source>esp@cenet</source><creator>YUDATE, KOZO ; NAGASAWA, KEN</creator><creatorcontrib>YUDATE, KOZO ; NAGASAWA, KEN</creatorcontrib><description>KAWASAKI STEEL 58-38,182 Precursor pitch to be used for formation of carbon fiber is produced by heating a coal tar soft or middle pitch at a temperature of 350-500.degree.C at a first stage to form mesophase, extracting the thus treated pitch with a solvent, separating and removing the solvent insoluble portion including mesophase to obtain a pitch containing no free carbon and further at the second stage heat-treating the pitch containing no free carbon in an inert gas atmosphere under atmospheric pressure or a reduced pressure under the following condition 600-1.2 T ? 0 ? 1,800-3.6 T (provided that 350 ? T ? 500) wherein T(.degree.C) is the temperature of the heat treatment and .theta. (min) is the time for which said temperature is held, to form bulk mesophase pitch containing 20-60% by weight of quinoline insoluble portion.</description><edition>4</edition><language>eng ; fre</language><subject>CHEMISTRY ; FUELS ; LUBRICANTS ; METALLURGY ; PEAT ; PETROLEUM, GAS OR COKE INDUSTRIES ; PYROLIGNEOUS ACID ; TECHNICAL GASES CONTAINING CARBON MONOXIDE ; WORKING-UP PITCH, ASPHALT, BITUMEN, TAR</subject><creationdate>1988</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19880329&DB=EPODOC&CC=CA&NR=1234548A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=19880329&DB=EPODOC&CC=CA&NR=1234548A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YUDATE, KOZO</creatorcontrib><creatorcontrib>NAGASAWA, KEN</creatorcontrib><title>METHOD FOR PRODUCING A PRECURSOR PITCH FOR CARBON FIBER</title><description>KAWASAKI STEEL 58-38,182 Precursor pitch to be used for formation of carbon fiber is produced by heating a coal tar soft or middle pitch at a temperature of 350-500.degree.C at a first stage to form mesophase, extracting the thus treated pitch with a solvent, separating and removing the solvent insoluble portion including mesophase to obtain a pitch containing no free carbon and further at the second stage heat-treating the pitch containing no free carbon in an inert gas atmosphere under atmospheric pressure or a reduced pressure under the following condition 600-1.2 T ? 0 ? 1,800-3.6 T (provided that 350 ? T ? 500) wherein T(.degree.C) is the temperature of the heat treatment and .theta. (min) is the time for which said temperature is held, to form bulk mesophase pitch containing 20-60% by weight of quinoline insoluble portion.</description><subject>CHEMISTRY</subject><subject>FUELS</subject><subject>LUBRICANTS</subject><subject>METALLURGY</subject><subject>PEAT</subject><subject>PETROLEUM, GAS OR COKE INDUSTRIES</subject><subject>PYROLIGNEOUS ACID</subject><subject>TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><subject>WORKING-UP PITCH, ASPHALT, BITUMEN, TAR</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1988</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD3dQ3x8HdRcPMPUggI8ncJdfb0c1dwBLJdnUODgkGiniHOHmB5Z8cgJ38_BTdPJ9cgHgbWtMSc4lReKM3NIO_mClSom1qQH59aXJCYnJqXWhLv7GhoZGxiamLhaExYBQCIECcL</recordid><startdate>19880329</startdate><enddate>19880329</enddate><creator>YUDATE, KOZO</creator><creator>NAGASAWA, KEN</creator><scope>EVB</scope></search><sort><creationdate>19880329</creationdate><title>METHOD FOR PRODUCING A PRECURSOR PITCH FOR CARBON FIBER</title><author>YUDATE, KOZO ; NAGASAWA, KEN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CA1234548A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>1988</creationdate><topic>CHEMISTRY</topic><topic>FUELS</topic><topic>LUBRICANTS</topic><topic>METALLURGY</topic><topic>PEAT</topic><topic>PETROLEUM, GAS OR COKE INDUSTRIES</topic><topic>PYROLIGNEOUS ACID</topic><topic>TECHNICAL GASES CONTAINING CARBON MONOXIDE</topic><topic>WORKING-UP PITCH, ASPHALT, BITUMEN, TAR</topic><toplevel>online_resources</toplevel><creatorcontrib>YUDATE, KOZO</creatorcontrib><creatorcontrib>NAGASAWA, KEN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YUDATE, KOZO</au><au>NAGASAWA, KEN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING A PRECURSOR PITCH FOR CARBON FIBER</title><date>1988-03-29</date><risdate>1988</risdate><abstract>KAWASAKI STEEL 58-38,182 Precursor pitch to be used for formation of carbon fiber is produced by heating a coal tar soft or middle pitch at a temperature of 350-500.degree.C at a first stage to form mesophase, extracting the thus treated pitch with a solvent, separating and removing the solvent insoluble portion including mesophase to obtain a pitch containing no free carbon and further at the second stage heat-treating the pitch containing no free carbon in an inert gas atmosphere under atmospheric pressure or a reduced pressure under the following condition 600-1.2 T ? 0 ? 1,800-3.6 T (provided that 350 ? T ? 500) wherein T(.degree.C) is the temperature of the heat treatment and .theta. (min) is the time for which said temperature is held, to form bulk mesophase pitch containing 20-60% by weight of quinoline insoluble portion.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; fre |
recordid | cdi_epo_espacenet_CA1234548A |
source | esp@cenet |
subjects | CHEMISTRY FUELS LUBRICANTS METALLURGY PEAT PETROLEUM, GAS OR COKE INDUSTRIES PYROLIGNEOUS ACID TECHNICAL GASES CONTAINING CARBON MONOXIDE WORKING-UP PITCH, ASPHALT, BITUMEN, TAR |
title | METHOD FOR PRODUCING A PRECURSOR PITCH FOR CARBON FIBER |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T22%3A21%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YUDATE,%20KOZO&rft.date=1988-03-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECA1234548A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |