RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES

RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES (D#75, 797-F) The invention covers a method for making reaction injection molded polyurethanes of improved properties. The elastomeric products having superior heat distortion and tear properties comprise the reaction product of an aro...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CUSCURIDA, MICHAEL, DOMINGUEZ, RICHARD J.G, RICE, DORIS M
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CUSCURIDA, MICHAEL
DOMINGUEZ, RICHARD J.G
RICE, DORIS M
description RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES (D#75, 797-F) The invention covers a method for making reaction injection molded polyurethanes of improved properties. The elastomeric products having superior heat distortion and tear properties comprise the reaction product of an aromatic polyisocyanate, a high molecular weight polyol and a chain extending agent. Said polyol providing said improved properties is a poly(oxybutyleneoxyethylene) glycol having a molecular weight range of about 2,000-6,000. The polyurethane elastomer is prepared by injecting the above three agents through a RIM head into a mold cavity of the desired configuration. Reaction injection molded elastomers are useful as molded articles of commerce including, but not limited to, vehicle body parts. -I-
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CA1171622A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CA1171622A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CA1171622A3</originalsourceid><addsrcrecordid>eNrjZHAI8vRVcPVxDA7x93UNClYI9wzxUPD0DQjyD3N1UfBwdQxRcPEESgaFePr7KTj6uSiEuDoGKQDlA1yBYq7BPAysaYk5xam8UJqbQd7NNcTZQze1ID8-tbggMTk1L7Uk3tnR0NDc0MzIyNGYsAoAI4gp9w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES</title><source>esp@cenet</source><creator>CUSCURIDA, MICHAEL ; DOMINGUEZ, RICHARD J.G ; RICE, DORIS M</creator><creatorcontrib>CUSCURIDA, MICHAEL ; DOMINGUEZ, RICHARD J.G ; RICE, DORIS M</creatorcontrib><description>RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES (D#75, 797-F) The invention covers a method for making reaction injection molded polyurethanes of improved properties. The elastomeric products having superior heat distortion and tear properties comprise the reaction product of an aromatic polyisocyanate, a high molecular weight polyol and a chain extending agent. Said polyol providing said improved properties is a poly(oxybutyleneoxyethylene) glycol having a molecular weight range of about 2,000-6,000. The polyurethane elastomer is prepared by injecting the above three agents through a RIM head into a mold cavity of the desired configuration. Reaction injection molded elastomers are useful as molded articles of commerce including, but not limited to, vehicle body parts. -I-</description><edition>3</edition><language>eng ; fre</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>1984</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19840731&amp;DB=EPODOC&amp;CC=CA&amp;NR=1171622A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25547,76298</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19840731&amp;DB=EPODOC&amp;CC=CA&amp;NR=1171622A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CUSCURIDA, MICHAEL</creatorcontrib><creatorcontrib>DOMINGUEZ, RICHARD J.G</creatorcontrib><creatorcontrib>RICE, DORIS M</creatorcontrib><title>RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES</title><description>RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES (D#75, 797-F) The invention covers a method for making reaction injection molded polyurethanes of improved properties. The elastomeric products having superior heat distortion and tear properties comprise the reaction product of an aromatic polyisocyanate, a high molecular weight polyol and a chain extending agent. Said polyol providing said improved properties is a poly(oxybutyleneoxyethylene) glycol having a molecular weight range of about 2,000-6,000. The polyurethane elastomer is prepared by injecting the above three agents through a RIM head into a mold cavity of the desired configuration. Reaction injection molded elastomers are useful as molded articles of commerce including, but not limited to, vehicle body parts. -I-</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1984</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAI8vRVcPVxDA7x93UNClYI9wzxUPD0DQjyD3N1UfBwdQxRcPEESgaFePr7KTj6uSiEuDoGKQDlA1yBYq7BPAysaYk5xam8UJqbQd7NNcTZQze1ID8-tbggMTk1L7Uk3tnR0NDc0MzIyNGYsAoAI4gp9w</recordid><startdate>19840731</startdate><enddate>19840731</enddate><creator>CUSCURIDA, MICHAEL</creator><creator>DOMINGUEZ, RICHARD J.G</creator><creator>RICE, DORIS M</creator><scope>EVB</scope></search><sort><creationdate>19840731</creationdate><title>RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES</title><author>CUSCURIDA, MICHAEL ; DOMINGUEZ, RICHARD J.G ; RICE, DORIS M</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CA1171622A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>1984</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>CUSCURIDA, MICHAEL</creatorcontrib><creatorcontrib>DOMINGUEZ, RICHARD J.G</creatorcontrib><creatorcontrib>RICE, DORIS M</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CUSCURIDA, MICHAEL</au><au>DOMINGUEZ, RICHARD J.G</au><au>RICE, DORIS M</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES</title><date>1984-07-31</date><risdate>1984</risdate><abstract>RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES (D#75, 797-F) The invention covers a method for making reaction injection molded polyurethanes of improved properties. The elastomeric products having superior heat distortion and tear properties comprise the reaction product of an aromatic polyisocyanate, a high molecular weight polyol and a chain extending agent. Said polyol providing said improved properties is a poly(oxybutyleneoxyethylene) glycol having a molecular weight range of about 2,000-6,000. The polyurethane elastomer is prepared by injecting the above three agents through a RIM head into a mold cavity of the desired configuration. Reaction injection molded elastomers are useful as molded articles of commerce including, but not limited to, vehicle body parts. -I-</abstract><edition>3</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre
recordid cdi_epo_espacenet_CA1171622A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title RIM ELASTOMERS WITH IMPROVED HEAT DISTORTION AND TEAR PROPERTIES
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-16T20%3A47%3A33IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CUSCURIDA,%20MICHAEL&rft.date=1984-07-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECA1171622A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true