FLUORESCENT LAMP CONSTRUCTION UTILIZING A MIXTURE OF TWO PHOSPHOR MATERIALS

A fluorescent lamp construction uses a particular blended phosphor mixture to provide an efficient light source having good color rendition. The phosphor mixture uses a blend of a strontium-haloapatite phosphor with europium-activated yttrium oxide phosphor. The phosphor mixture produces light emiss...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OFFERLE, THOMAS E, SOULES, THOMAS F
Format: Patent
Sprache:eng ; fre
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator OFFERLE, THOMAS E
SOULES, THOMAS F
description A fluorescent lamp construction uses a particular blended phosphor mixture to provide an efficient light source having good color rendition. The phosphor mixture uses a blend of a strontium-haloapatite phosphor with europium-activated yttrium oxide phosphor. The phosphor mixture produces light emission in a color temperature range from about 2,700.degree.K to about 6,500.degree.K with both a satisfactory color rendition and higher luminous efficiency than can be obtained with conventional phosphor mixtures. The useful strontium-haloapatite phosphors include strontium blue halophosphate phosphor activated with antimony, strontium green halophosphate phosphor coactivated with antimony and manganese, and strontium yellow halophosphate phosphor which contains a still greater manganese activator level. The useful strontium-haloapatite phosphor have the general formula: Sr10-x-ySbxMny(PO4)6.A2 wherein A is a halide selected from F and C1 including combinations thereof, x is in the approximate range 0.04 to 0.15, and y is in the approximate range 0.01 to 0.42. The phosphor mixture contains approximately 75 to 85 weight percent of the strontium-haloapatite phosphor.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CA1065949A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CA1065949A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CA1065949A3</originalsourceid><addsrcrecordid>eNrjZPB28wn1D3INdnb1C1HwcfQNUHD29wsOCQp1DvH091MIDfH08Yzy9HNXcFTw9YwICQ1yVfB3UwgJ91cI8PAPBuIgBV_HENcgT0efYB4G1rTEnOJUXijNzSDv5hri7KGbWpAfn1pckJicmpdaEu_saGhgZmppYuloTFgFACjbLWk</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FLUORESCENT LAMP CONSTRUCTION UTILIZING A MIXTURE OF TWO PHOSPHOR MATERIALS</title><source>esp@cenet</source><creator>OFFERLE, THOMAS E ; SOULES, THOMAS F</creator><creatorcontrib>OFFERLE, THOMAS E ; SOULES, THOMAS F</creatorcontrib><description>A fluorescent lamp construction uses a particular blended phosphor mixture to provide an efficient light source having good color rendition. The phosphor mixture uses a blend of a strontium-haloapatite phosphor with europium-activated yttrium oxide phosphor. The phosphor mixture produces light emission in a color temperature range from about 2,700.degree.K to about 6,500.degree.K with both a satisfactory color rendition and higher luminous efficiency than can be obtained with conventional phosphor mixtures. The useful strontium-haloapatite phosphors include strontium blue halophosphate phosphor activated with antimony, strontium green halophosphate phosphor coactivated with antimony and manganese, and strontium yellow halophosphate phosphor which contains a still greater manganese activator level. The useful strontium-haloapatite phosphor have the general formula: Sr10-x-ySbxMny(PO4)6.A2 wherein A is a halide selected from F and C1 including combinations thereof, x is in the approximate range 0.04 to 0.15, and y is in the approximate range 0.01 to 0.42. The phosphor mixture contains approximately 75 to 85 weight percent of the strontium-haloapatite phosphor.</description><language>eng ; fre</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS ; ELECTRICITY</subject><creationdate>1979</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19791106&amp;DB=EPODOC&amp;CC=CA&amp;NR=1065949A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25553,76306</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19791106&amp;DB=EPODOC&amp;CC=CA&amp;NR=1065949A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OFFERLE, THOMAS E</creatorcontrib><creatorcontrib>SOULES, THOMAS F</creatorcontrib><title>FLUORESCENT LAMP CONSTRUCTION UTILIZING A MIXTURE OF TWO PHOSPHOR MATERIALS</title><description>A fluorescent lamp construction uses a particular blended phosphor mixture to provide an efficient light source having good color rendition. The phosphor mixture uses a blend of a strontium-haloapatite phosphor with europium-activated yttrium oxide phosphor. The phosphor mixture produces light emission in a color temperature range from about 2,700.degree.K to about 6,500.degree.K with both a satisfactory color rendition and higher luminous efficiency than can be obtained with conventional phosphor mixtures. The useful strontium-haloapatite phosphors include strontium blue halophosphate phosphor activated with antimony, strontium green halophosphate phosphor coactivated with antimony and manganese, and strontium yellow halophosphate phosphor which contains a still greater manganese activator level. The useful strontium-haloapatite phosphor have the general formula: Sr10-x-ySbxMny(PO4)6.A2 wherein A is a halide selected from F and C1 including combinations thereof, x is in the approximate range 0.04 to 0.15, and y is in the approximate range 0.01 to 0.42. The phosphor mixture contains approximately 75 to 85 weight percent of the strontium-haloapatite phosphor.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS</subject><subject>ELECTRICITY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1979</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPB28wn1D3INdnb1C1HwcfQNUHD29wsOCQp1DvH091MIDfH08Yzy9HNXcFTw9YwICQ1yVfB3UwgJ91cI8PAPBuIgBV_HENcgT0efYB4G1rTEnOJUXijNzSDv5hri7KGbWpAfn1pckJicmpdaEu_saGhgZmppYuloTFgFACjbLWk</recordid><startdate>19791106</startdate><enddate>19791106</enddate><creator>OFFERLE, THOMAS E</creator><creator>SOULES, THOMAS F</creator><scope>EVB</scope></search><sort><creationdate>19791106</creationdate><title>FLUORESCENT LAMP CONSTRUCTION UTILIZING A MIXTURE OF TWO PHOSPHOR MATERIALS</title><author>OFFERLE, THOMAS E ; SOULES, THOMAS F</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CA1065949A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; fre</language><creationdate>1979</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS</topic><topic>ELECTRICITY</topic><toplevel>online_resources</toplevel><creatorcontrib>OFFERLE, THOMAS E</creatorcontrib><creatorcontrib>SOULES, THOMAS F</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OFFERLE, THOMAS E</au><au>SOULES, THOMAS F</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FLUORESCENT LAMP CONSTRUCTION UTILIZING A MIXTURE OF TWO PHOSPHOR MATERIALS</title><date>1979-11-06</date><risdate>1979</risdate><abstract>A fluorescent lamp construction uses a particular blended phosphor mixture to provide an efficient light source having good color rendition. The phosphor mixture uses a blend of a strontium-haloapatite phosphor with europium-activated yttrium oxide phosphor. The phosphor mixture produces light emission in a color temperature range from about 2,700.degree.K to about 6,500.degree.K with both a satisfactory color rendition and higher luminous efficiency than can be obtained with conventional phosphor mixtures. The useful strontium-haloapatite phosphors include strontium blue halophosphate phosphor activated with antimony, strontium green halophosphate phosphor coactivated with antimony and manganese, and strontium yellow halophosphate phosphor which contains a still greater manganese activator level. The useful strontium-haloapatite phosphor have the general formula: Sr10-x-ySbxMny(PO4)6.A2 wherein A is a halide selected from F and C1 including combinations thereof, x is in the approximate range 0.04 to 0.15, and y is in the approximate range 0.01 to 0.42. The phosphor mixture contains approximately 75 to 85 weight percent of the strontium-haloapatite phosphor.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; fre
recordid cdi_epo_espacenet_CA1065949A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS
ELECTRICITY
title FLUORESCENT LAMP CONSTRUCTION UTILIZING A MIXTURE OF TWO PHOSPHOR MATERIALS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T08%3A46%3A05IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OFFERLE,%20THOMAS%20E&rft.date=1979-11-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECA1065949A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true