METHOD FOR CONVERTING

This method is an application for non-ferrous metallurgy. By this method the consumption of fluxes is reduced, the slag-formation processes are intensified and the quantity of the cold turnover materials being processed is increased. During the first period of converting fluxes, the cold turnover ma...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: STEFANOV, BORIS S, GENEVSKA, TATJANA N, PETROV, DIMITAR A, KOTOV, TODOR I, NIKOLOV, TSVJATKO N, STEFANOVA, VLADISLAVA P, GENEVSKI, KONSTANTIN V, PETKOV, BORIS A
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator STEFANOV, BORIS S
GENEVSKA, TATJANA N
PETROV, DIMITAR A
KOTOV, TODOR I
NIKOLOV, TSVJATKO N
STEFANOVA, VLADISLAVA P
GENEVSKI, KONSTANTIN V
PETKOV, BORIS A
description This method is an application for non-ferrous metallurgy. By this method the consumption of fluxes is reduced, the slag-formation processes are intensified and the quantity of the cold turnover materials being processed is increased. During the first period of converting fluxes, the cold turnover materials are fed. In the converter, preceding the pouring of each portion of matter, floatation wastes from coal dressings are supplied which feature the following composition in wt.%: carbon 30 - 50, silica 20 - 30, calcium oxide 2 - 5, alumina 5 - 10 and ferrous oxides 2 - 5. The ignition temperature of the floatation waste is 250-450 degrees C and its quantity is 5 - 15% of the mass of the fed matter.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_BG48402A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>BG48402A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_BG48402A13</originalsourceid><addsrcrecordid>eNrjZBD1dQ3x8HdRcPMPUnD29wtzDQrx9HPnYWBNS8wpTuWF0twMcm6uIc4euqkF-fGpxQWJyal5qSXxTu4mFiYGRo6GxgQVAADoUR2T</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR CONVERTING</title><source>esp@cenet</source><creator>STEFANOV, BORIS S ; GENEVSKA, TATJANA N ; PETROV, DIMITAR A ; KOTOV, TODOR I ; NIKOLOV, TSVJATKO N ; STEFANOVA, VLADISLAVA P ; GENEVSKI, KONSTANTIN V ; PETKOV, BORIS A</creator><creatorcontrib>STEFANOV, BORIS S ; GENEVSKA, TATJANA N ; PETROV, DIMITAR A ; KOTOV, TODOR I ; NIKOLOV, TSVJATKO N ; STEFANOVA, VLADISLAVA P ; GENEVSKI, KONSTANTIN V ; PETKOV, BORIS A</creatorcontrib><description>This method is an application for non-ferrous metallurgy. By this method the consumption of fluxes is reduced, the slag-formation processes are intensified and the quantity of the cold turnover materials being processed is increased. During the first period of converting fluxes, the cold turnover materials are fed. In the converter, preceding the pouring of each portion of matter, floatation wastes from coal dressings are supplied which feature the following composition in wt.%: carbon 30 - 50, silica 20 - 30, calcium oxide 2 - 5, alumina 5 - 10 and ferrous oxides 2 - 5. The ignition temperature of the floatation waste is 250-450 degrees C and its quantity is 5 - 15% of the mass of the fed matter.</description><edition>5</edition><language>eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1991</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19910215&amp;DB=EPODOC&amp;CC=BG&amp;NR=48402A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19910215&amp;DB=EPODOC&amp;CC=BG&amp;NR=48402A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>STEFANOV, BORIS S</creatorcontrib><creatorcontrib>GENEVSKA, TATJANA N</creatorcontrib><creatorcontrib>PETROV, DIMITAR A</creatorcontrib><creatorcontrib>KOTOV, TODOR I</creatorcontrib><creatorcontrib>NIKOLOV, TSVJATKO N</creatorcontrib><creatorcontrib>STEFANOVA, VLADISLAVA P</creatorcontrib><creatorcontrib>GENEVSKI, KONSTANTIN V</creatorcontrib><creatorcontrib>PETKOV, BORIS A</creatorcontrib><title>METHOD FOR CONVERTING</title><description>This method is an application for non-ferrous metallurgy. By this method the consumption of fluxes is reduced, the slag-formation processes are intensified and the quantity of the cold turnover materials being processed is increased. During the first period of converting fluxes, the cold turnover materials are fed. In the converter, preceding the pouring of each portion of matter, floatation wastes from coal dressings are supplied which feature the following composition in wt.%: carbon 30 - 50, silica 20 - 30, calcium oxide 2 - 5, alumina 5 - 10 and ferrous oxides 2 - 5. The ignition temperature of the floatation waste is 250-450 degrees C and its quantity is 5 - 15% of the mass of the fed matter.</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1991</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBD1dQ3x8HdRcPMPUnD29wtzDQrx9HPnYWBNS8wpTuWF0twMcm6uIc4euqkF-fGpxQWJyal5qSXxTu4mFiYGRo6GxgQVAADoUR2T</recordid><startdate>19910215</startdate><enddate>19910215</enddate><creator>STEFANOV, BORIS S</creator><creator>GENEVSKA, TATJANA N</creator><creator>PETROV, DIMITAR A</creator><creator>KOTOV, TODOR I</creator><creator>NIKOLOV, TSVJATKO N</creator><creator>STEFANOVA, VLADISLAVA P</creator><creator>GENEVSKI, KONSTANTIN V</creator><creator>PETKOV, BORIS A</creator><scope>EVB</scope></search><sort><creationdate>19910215</creationdate><title>METHOD FOR CONVERTING</title><author>STEFANOV, BORIS S ; GENEVSKA, TATJANA N ; PETROV, DIMITAR A ; KOTOV, TODOR I ; NIKOLOV, TSVJATKO N ; STEFANOVA, VLADISLAVA P ; GENEVSKI, KONSTANTIN V ; PETKOV, BORIS A</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_BG48402A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1991</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>STEFANOV, BORIS S</creatorcontrib><creatorcontrib>GENEVSKA, TATJANA N</creatorcontrib><creatorcontrib>PETROV, DIMITAR A</creatorcontrib><creatorcontrib>KOTOV, TODOR I</creatorcontrib><creatorcontrib>NIKOLOV, TSVJATKO N</creatorcontrib><creatorcontrib>STEFANOVA, VLADISLAVA P</creatorcontrib><creatorcontrib>GENEVSKI, KONSTANTIN V</creatorcontrib><creatorcontrib>PETKOV, BORIS A</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>STEFANOV, BORIS S</au><au>GENEVSKA, TATJANA N</au><au>PETROV, DIMITAR A</au><au>KOTOV, TODOR I</au><au>NIKOLOV, TSVJATKO N</au><au>STEFANOVA, VLADISLAVA P</au><au>GENEVSKI, KONSTANTIN V</au><au>PETKOV, BORIS A</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR CONVERTING</title><date>1991-02-15</date><risdate>1991</risdate><abstract>This method is an application for non-ferrous metallurgy. By this method the consumption of fluxes is reduced, the slag-formation processes are intensified and the quantity of the cold turnover materials being processed is increased. During the first period of converting fluxes, the cold turnover materials are fed. In the converter, preceding the pouring of each portion of matter, floatation wastes from coal dressings are supplied which feature the following composition in wt.%: carbon 30 - 50, silica 20 - 30, calcium oxide 2 - 5, alumina 5 - 10 and ferrous oxides 2 - 5. The ignition temperature of the floatation waste is 250-450 degrees C and its quantity is 5 - 15% of the mass of the fed matter.</abstract><edition>5</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_BG48402A1
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title METHOD FOR CONVERTING
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T02%3A37%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=STEFANOV,%20BORIS%20S&rft.date=1991-02-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EBG48402A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true