HIGH TENACITY, HIGH MODULUS POLYAMIDE YARN AND PROCESS FOR MAKING SAME

A yarn comprised of a polyamide which is at least about 85% poly(hexamethylene adipamide) or poly( epsilon -caproamide) is disclosed which has a relative viscosity of greater than about 50, a tenacity of greater than about 11.0 g/d, a dry heat shrinkage at 160 DEG C of not more than about 6.5 percen...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: THOMAS RUSSELL CLARK III, JOSEPH ARNOLD COFER JR
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator THOMAS RUSSELL CLARK III
JOSEPH ARNOLD COFER JR
description A yarn comprised of a polyamide which is at least about 85% poly(hexamethylene adipamide) or poly( epsilon -caproamide) is disclosed which has a relative viscosity of greater than about 50, a tenacity of greater than about 11.0 g/d, a dry heat shrinkage at 160 DEG C of not more than about 6.5 percent, a boil-off shrinkage of less than about 7%, a modulus of greater than about 35 g/d, a birefringence of greater than about 0.060, a differential birefringence D: DELTA .90-.00, of greater than 0, and a sonic modulus of greater than about 90 g/d. The process for making the yarn includes drawing of a feed yarn while heating to at least about 185 DEG C in at least a final draw stage to a draw tension of at least 3.8 g/d, subsequently decreasing the tension while heating to at least about 185 DEG C to produce a length decrease of between about 2 and about 13.5, and cooling and packaging the yarn.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_AU6482690A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>AU6482690A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_AU6482690A3</originalsourceid><addsrcrecordid>eNrjZHDz8HT3UAhx9XN09gyJ1FEAc339XUJ9QoMVAvx9Ih19PV1cFSIdg_wUHP1cFAKC_J1dg4MV3PyDFHwdvT393BWCHX1deRhY0xJzilN5oTQ3g7yba4izh25qQX58anFBYnJqXmpJvGOomYmFkZmlgaMxYRUA4RgrQw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>HIGH TENACITY, HIGH MODULUS POLYAMIDE YARN AND PROCESS FOR MAKING SAME</title><source>esp@cenet</source><creator>THOMAS RUSSELL CLARK III ; JOSEPH ARNOLD COFER JR</creator><creatorcontrib>THOMAS RUSSELL CLARK III ; JOSEPH ARNOLD COFER JR</creatorcontrib><description>A yarn comprised of a polyamide which is at least about 85% poly(hexamethylene adipamide) or poly( epsilon -caproamide) is disclosed which has a relative viscosity of greater than about 50, a tenacity of greater than about 11.0 g/d, a dry heat shrinkage at 160 DEG C of not more than about 6.5 percent, a boil-off shrinkage of less than about 7%, a modulus of greater than about 35 g/d, a birefringence of greater than about 0.060, a differential birefringence D: DELTA .90-.00, of greater than 0, and a sonic modulus of greater than about 90 g/d. The process for making the yarn includes drawing of a feed yarn while heating to at least about 185 DEG C in at least a final draw stage to a draw tension of at least 3.8 g/d, subsequently decreasing the tension while heating to at least about 185 DEG C to produce a length decrease of between about 2 and about 13.5, and cooling and packaging the yarn.</description><edition>5</edition><language>eng</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; FINISHING OR DRESSING OF FILAMENTS, YARNS, THREADS, CORDS,ROPES OR THE LIKE ; MECHANICAL FINISHING OF YARNS OR ROPES ; MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; SPINNING ; TEXTILES ; WARPING OR BEAMING ; YARNS</subject><creationdate>1991</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19910426&amp;DB=EPODOC&amp;CC=AU&amp;NR=6482690A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19910426&amp;DB=EPODOC&amp;CC=AU&amp;NR=6482690A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>THOMAS RUSSELL CLARK III</creatorcontrib><creatorcontrib>JOSEPH ARNOLD COFER JR</creatorcontrib><title>HIGH TENACITY, HIGH MODULUS POLYAMIDE YARN AND PROCESS FOR MAKING SAME</title><description>A yarn comprised of a polyamide which is at least about 85% poly(hexamethylene adipamide) or poly( epsilon -caproamide) is disclosed which has a relative viscosity of greater than about 50, a tenacity of greater than about 11.0 g/d, a dry heat shrinkage at 160 DEG C of not more than about 6.5 percent, a boil-off shrinkage of less than about 7%, a modulus of greater than about 35 g/d, a birefringence of greater than about 0.060, a differential birefringence D: DELTA .90-.00, of greater than 0, and a sonic modulus of greater than about 90 g/d. The process for making the yarn includes drawing of a feed yarn while heating to at least about 185 DEG C in at least a final draw stage to a draw tension of at least 3.8 g/d, subsequently decreasing the tension while heating to at least about 185 DEG C to produce a length decrease of between about 2 and about 13.5, and cooling and packaging the yarn.</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>FINISHING OR DRESSING OF FILAMENTS, YARNS, THREADS, CORDS,ROPES OR THE LIKE</subject><subject>MECHANICAL FINISHING OF YARNS OR ROPES</subject><subject>MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>SPINNING</subject><subject>TEXTILES</subject><subject>WARPING OR BEAMING</subject><subject>YARNS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1991</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDz8HT3UAhx9XN09gyJ1FEAc339XUJ9QoMVAvx9Ih19PV1cFSIdg_wUHP1cFAKC_J1dg4MV3PyDFHwdvT393BWCHX1deRhY0xJzilN5oTQ3g7yba4izh25qQX58anFBYnJqXmpJvGOomYmFkZmlgaMxYRUA4RgrQw</recordid><startdate>19910426</startdate><enddate>19910426</enddate><creator>THOMAS RUSSELL CLARK III</creator><creator>JOSEPH ARNOLD COFER JR</creator><scope>EVB</scope></search><sort><creationdate>19910426</creationdate><title>HIGH TENACITY, HIGH MODULUS POLYAMIDE YARN AND PROCESS FOR MAKING SAME</title><author>THOMAS RUSSELL CLARK III ; JOSEPH ARNOLD COFER JR</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_AU6482690A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1991</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>FINISHING OR DRESSING OF FILAMENTS, YARNS, THREADS, CORDS,ROPES OR THE LIKE</topic><topic>MECHANICAL FINISHING OF YARNS OR ROPES</topic><topic>MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>SPINNING</topic><topic>TEXTILES</topic><topic>WARPING OR BEAMING</topic><topic>YARNS</topic><toplevel>online_resources</toplevel><creatorcontrib>THOMAS RUSSELL CLARK III</creatorcontrib><creatorcontrib>JOSEPH ARNOLD COFER JR</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>THOMAS RUSSELL CLARK III</au><au>JOSEPH ARNOLD COFER JR</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>HIGH TENACITY, HIGH MODULUS POLYAMIDE YARN AND PROCESS FOR MAKING SAME</title><date>1991-04-26</date><risdate>1991</risdate><abstract>A yarn comprised of a polyamide which is at least about 85% poly(hexamethylene adipamide) or poly( epsilon -caproamide) is disclosed which has a relative viscosity of greater than about 50, a tenacity of greater than about 11.0 g/d, a dry heat shrinkage at 160 DEG C of not more than about 6.5 percent, a boil-off shrinkage of less than about 7%, a modulus of greater than about 35 g/d, a birefringence of greater than about 0.060, a differential birefringence D: DELTA .90-.00, of greater than 0, and a sonic modulus of greater than about 90 g/d. The process for making the yarn includes drawing of a feed yarn while heating to at least about 185 DEG C in at least a final draw stage to a draw tension of at least 3.8 g/d, subsequently decreasing the tension while heating to at least about 185 DEG C to produce a length decrease of between about 2 and about 13.5, and cooling and packaging the yarn.</abstract><edition>5</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_AU6482690A
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
FINISHING OR DRESSING OF FILAMENTS, YARNS, THREADS, CORDS,ROPES OR THE LIKE
MECHANICAL FINISHING OF YARNS OR ROPES
MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS
NATURAL OR ARTIFICIAL THREADS OR FIBRES
SPINNING
TEXTILES
WARPING OR BEAMING
YARNS
title HIGH TENACITY, HIGH MODULUS POLYAMIDE YARN AND PROCESS FOR MAKING SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T02%3A03%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=THOMAS%20RUSSELL%20CLARK%20III&rft.date=1991-04-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EAU6482690A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true