Advanced epoxy resins are prepared from a liquid diglycidyl ether of bisphenol A and bisphenol A which advanced epoxy resins have an equivalent weight in the range of 3,000 to 3,900 and a weight average molecular weight of 13,000 to 17,000.These resins are prepared by heating a heating a mixture of...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PONG SU SHEIH, MANUEL C. TYLER JR
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator PONG SU SHEIH
MANUEL C. TYLER JR
description Advanced epoxy resins are prepared from a liquid diglycidyl ether of bisphenol A and bisphenol A which advanced epoxy resins have an equivalent weight in the range of 3,000 to 3,900 and a weight average molecular weight of 13,000 to 17,000.These resins are prepared by heating a heating a mixture of (A) a liquid diglycidyl ether of bisphenol A having an average epoxide equivalent weight of from 170 to 195, (B).bisphenol A, (C) a catalytic quantity of one or more catalysts for effecting the reaction between components A and B and (D) a solvent or mixture of solvents such that the exotherm temperature is between 190°C and 210°C; cooling the resuitant reaction mixture to a temperature between 150°C and 185°C and maintaining the tem- ; perature thereat until the desired epoxide equivalent weignt and weight average molecular weight are obtainec: and thereafter quenching the resulting reaction product to a temperature between 90°C and 130°C with (E) one or more solvents.In the process of this invention, component A is employed in an amount which comprises from 54 to 62 percent by weight of the combined weight of components A, B, C and D; component B is employed in an amount which comprises from 30 to 35 percent by weight of the combined weight of components A, B, C and D; component C is employed in an amount which comprises from 0.01 to 0.2 percent by weight of the combined weight of components A, B, C and D; component D is employed in an amount which comprises from 5 to 30 percent by weight of the combined weight of components A, B, C and D;and component E is employed in an amount which comprises from 30 to 80 percent by weight of components A, B, C, D and E.When these advanced epoxy resins are formulated into can coating compositions they result in coatings having good wet and dry adhesion.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_AU587803BB2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>AU587803BB2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_AU587803BB23</originalsourceid><addsrcrecordid>eNrjZBBxdAlz9HN2dVFwDfCPiFQIcg329ONhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfGOoaYW5hYGxk5ORsZEKAEAPSAeVw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>ADVANCED EPOXY RESIN</title><source>esp@cenet</source><creator>PONG SU SHEIH ; MANUEL C. TYLER JR</creator><creatorcontrib>PONG SU SHEIH ; MANUEL C. TYLER JR</creatorcontrib><description>Advanced epoxy resins are prepared from a liquid diglycidyl ether of bisphenol A and bisphenol A which advanced epoxy resins have an equivalent weight in the range of 3,000 to 3,900 and a weight average molecular weight of 13,000 to 17,000.These resins are prepared by heating a heating a mixture of (A) a liquid diglycidyl ether of bisphenol A having an average epoxide equivalent weight of from 170 to 195, (B).bisphenol A, (C) a catalytic quantity of one or more catalysts for effecting the reaction between components A and B and (D) a solvent or mixture of solvents such that the exotherm temperature is between 190°C and 210°C; cooling the resuitant reaction mixture to a temperature between 150°C and 185°C and maintaining the tem- ; perature thereat until the desired epoxide equivalent weignt and weight average molecular weight are obtainec: and thereafter quenching the resulting reaction product to a temperature between 90°C and 130°C with (E) one or more solvents.In the process of this invention, component A is employed in an amount which comprises from 54 to 62 percent by weight of the combined weight of components A, B, C and D; component B is employed in an amount which comprises from 30 to 35 percent by weight of the combined weight of components A, B, C and D; component C is employed in an amount which comprises from 0.01 to 0.2 percent by weight of the combined weight of components A, B, C and D; component D is employed in an amount which comprises from 5 to 30 percent by weight of the combined weight of components A, B, C and D;and component E is employed in an amount which comprises from 30 to 80 percent by weight of components A, B, C, D and E.When these advanced epoxy resins are formulated into can coating compositions they result in coatings having good wet and dry adhesion.</description><edition>4</edition><language>eng</language><subject>ADHESIVES ; CHEMICAL PAINT OR INK REMOVERS ; CHEMISTRY ; COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS ; COMPOSITIONS BASED THEREON ; CORRECTING FLUIDS ; DYES ; FILLING PASTES ; INKS ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; PASTES OR SOLIDS FOR COLOURING OR PRINTING ; POLISHES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF MATERIALS THEREFOR ; WOODSTAINS</subject><creationdate>1989</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19890831&amp;DB=EPODOC&amp;CC=AU&amp;NR=587803B2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19890831&amp;DB=EPODOC&amp;CC=AU&amp;NR=587803B2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>PONG SU SHEIH</creatorcontrib><creatorcontrib>MANUEL C. TYLER JR</creatorcontrib><title>ADVANCED EPOXY RESIN</title><description>Advanced epoxy resins are prepared from a liquid diglycidyl ether of bisphenol A and bisphenol A which advanced epoxy resins have an equivalent weight in the range of 3,000 to 3,900 and a weight average molecular weight of 13,000 to 17,000.These resins are prepared by heating a heating a mixture of (A) a liquid diglycidyl ether of bisphenol A having an average epoxide equivalent weight of from 170 to 195, (B).bisphenol A, (C) a catalytic quantity of one or more catalysts for effecting the reaction between components A and B and (D) a solvent or mixture of solvents such that the exotherm temperature is between 190°C and 210°C; cooling the resuitant reaction mixture to a temperature between 150°C and 185°C and maintaining the tem- ; perature thereat until the desired epoxide equivalent weignt and weight average molecular weight are obtainec: and thereafter quenching the resulting reaction product to a temperature between 90°C and 130°C with (E) one or more solvents.In the process of this invention, component A is employed in an amount which comprises from 54 to 62 percent by weight of the combined weight of components A, B, C and D; component B is employed in an amount which comprises from 30 to 35 percent by weight of the combined weight of components A, B, C and D; component C is employed in an amount which comprises from 0.01 to 0.2 percent by weight of the combined weight of components A, B, C and D; component D is employed in an amount which comprises from 5 to 30 percent by weight of the combined weight of components A, B, C and D;and component E is employed in an amount which comprises from 30 to 80 percent by weight of components A, B, C, D and E.When these advanced epoxy resins are formulated into can coating compositions they result in coatings having good wet and dry adhesion.</description><subject>ADHESIVES</subject><subject>CHEMICAL PAINT OR INK REMOVERS</subject><subject>CHEMISTRY</subject><subject>COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>CORRECTING FLUIDS</subject><subject>DYES</subject><subject>FILLING PASTES</subject><subject>INKS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>PASTES OR SOLIDS FOR COLOURING OR PRINTING</subject><subject>POLISHES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF MATERIALS THEREFOR</subject><subject>WOODSTAINS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1989</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZBBxdAlz9HN2dVFwDfCPiFQIcg329ONhYE1LzClO5YXS3AwKbq4hzh66qQX58anFBYnJqXmpJfGOoaYW5hYGxk5ORsZEKAEAPSAeVw</recordid><startdate>19890831</startdate><enddate>19890831</enddate><creator>PONG SU SHEIH</creator><creator>MANUEL C. TYLER JR</creator><scope>EVB</scope></search><sort><creationdate>19890831</creationdate><title>ADVANCED EPOXY RESIN</title><author>PONG SU SHEIH ; MANUEL C. TYLER JR</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_AU587803BB23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1989</creationdate><topic>ADHESIVES</topic><topic>CHEMICAL PAINT OR INK REMOVERS</topic><topic>CHEMISTRY</topic><topic>COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>CORRECTING FLUIDS</topic><topic>DYES</topic><topic>FILLING PASTES</topic><topic>INKS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>PASTES OR SOLIDS FOR COLOURING OR PRINTING</topic><topic>POLISHES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF MATERIALS THEREFOR</topic><topic>WOODSTAINS</topic><toplevel>online_resources</toplevel><creatorcontrib>PONG SU SHEIH</creatorcontrib><creatorcontrib>MANUEL C. TYLER JR</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>PONG SU SHEIH</au><au>MANUEL C. TYLER JR</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>ADVANCED EPOXY RESIN</title><date>1989-08-31</date><risdate>1989</risdate><abstract>Advanced epoxy resins are prepared from a liquid diglycidyl ether of bisphenol A and bisphenol A which advanced epoxy resins have an equivalent weight in the range of 3,000 to 3,900 and a weight average molecular weight of 13,000 to 17,000.These resins are prepared by heating a heating a mixture of (A) a liquid diglycidyl ether of bisphenol A having an average epoxide equivalent weight of from 170 to 195, (B).bisphenol A, (C) a catalytic quantity of one or more catalysts for effecting the reaction between components A and B and (D) a solvent or mixture of solvents such that the exotherm temperature is between 190°C and 210°C; cooling the resuitant reaction mixture to a temperature between 150°C and 185°C and maintaining the tem- ; perature thereat until the desired epoxide equivalent weignt and weight average molecular weight are obtainec: and thereafter quenching the resulting reaction product to a temperature between 90°C and 130°C with (E) one or more solvents.In the process of this invention, component A is employed in an amount which comprises from 54 to 62 percent by weight of the combined weight of components A, B, C and D; component B is employed in an amount which comprises from 30 to 35 percent by weight of the combined weight of components A, B, C and D; component C is employed in an amount which comprises from 0.01 to 0.2 percent by weight of the combined weight of components A, B, C and D; component D is employed in an amount which comprises from 5 to 30 percent by weight of the combined weight of components A, B, C and D;and component E is employed in an amount which comprises from 30 to 80 percent by weight of components A, B, C, D and E.When these advanced epoxy resins are formulated into can coating compositions they result in coatings having good wet and dry adhesion.</abstract><edition>4</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_AU587803BB2
source esp@cenet
subjects ADHESIVES
CHEMICAL PAINT OR INK REMOVERS
CHEMISTRY
COATING COMPOSITIONS, e.g. PAINTS, VARNISHES ORLACQUERS
COMPOSITIONS BASED THEREON
CORRECTING FLUIDS
DYES
FILLING PASTES
INKS
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
ORGANIC MACROMOLECULAR COMPOUNDS
PAINTS
PASTES OR SOLIDS FOR COLOURING OR PRINTING
POLISHES
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF MATERIALS THEREFOR
WOODSTAINS
title ADVANCED EPOXY RESIN
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T23%3A17%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=PONG%20SU%20SHEIH&rft.date=1989-08-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EAU587803BB2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true