Method for producing a nitrided packaging steel

The invention relates to a method for producing a nitrided packaging steel from a hot-rolled steel product with a carbon content of 400 to 1200 ppm, characterized by a cold-rolling of the steel product to a flat steel product, subsequent recrystallization annealing of the cold-rolled flat steel prod...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Sauer, Reiner, Massicot, Blaise, Kaup, Burkhard, Kohl, Manuel, Klemmer, Ricarda, Kiewitz, Chrysanthus
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Sauer, Reiner
Massicot, Blaise
Kaup, Burkhard
Kohl, Manuel
Klemmer, Ricarda
Kiewitz, Chrysanthus
description The invention relates to a method for producing a nitrided packaging steel from a hot-rolled steel product with a carbon content of 400 to 1200 ppm, characterized by a cold-rolling of the steel product to a flat steel product, subsequent recrystallization annealing of the cold-rolled flat steel product in an annealing furnace, in particular a continuous annealing furnace, wherein a nitrogen-containing gas is supplied into the annealing furnace and is directed at the flat steel product in order to introduce unbonded nitrogen into the flat steel product in an amount corresponding to a concentration of more than 100 ppm, or to increase the amount of unbonded nitrogen in the flat steel product to a concentration of more than 100 ppm, and subsequent cooling of the recrystallized annealed flat steel product at a cooling rate of at least 100 K/s directly after the recrystallization annealing. Using this method, cold-rolled flat steel products may be produced for packaging purposes with a tensile strength of more than 650 MPa and in particular between 700 and 850 MPa.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_AU2015349052A2</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>AU2015349052A2</sourcerecordid><originalsourceid>FETCH-epo_espacenet_AU2015349052A23</originalsourceid><addsrcrecordid>eNrjZND3TS3JyE9RSMsvUigoyk8pTc7MS1dIVMjLLCnKTElNUShITM5OTAcJFpekpubwMLCmJeYUp_JCaW4GZTfXEGcP3dSC_PjUYqDq1LzUknjHUCMDQ1NjE0sDUyNHI2PiVAEAwGErjw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for producing a nitrided packaging steel</title><source>esp@cenet</source><creator>Sauer, Reiner ; Massicot, Blaise ; Kaup, Burkhard ; Kohl, Manuel ; Klemmer, Ricarda ; Kiewitz, Chrysanthus</creator><creatorcontrib>Sauer, Reiner ; Massicot, Blaise ; Kaup, Burkhard ; Kohl, Manuel ; Klemmer, Ricarda ; Kiewitz, Chrysanthus</creatorcontrib><description>The invention relates to a method for producing a nitrided packaging steel from a hot-rolled steel product with a carbon content of 400 to 1200 ppm, characterized by a cold-rolling of the steel product to a flat steel product, subsequent recrystallization annealing of the cold-rolled flat steel product in an annealing furnace, in particular a continuous annealing furnace, wherein a nitrogen-containing gas is supplied into the annealing furnace and is directed at the flat steel product in order to introduce unbonded nitrogen into the flat steel product in an amount corresponding to a concentration of more than 100 ppm, or to increase the amount of unbonded nitrogen in the flat steel product to a concentration of more than 100 ppm, and subsequent cooling of the recrystallized annealed flat steel product at a cooling rate of at least 100 K/s directly after the recrystallization annealing. Using this method, cold-rolled flat steel products may be produced for packaging purposes with a tensile strength of more than 650 MPa and in particular between 700 and 850 MPa.</description><language>eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2017</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170928&amp;DB=EPODOC&amp;CC=AU&amp;NR=2015349052A2$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20170928&amp;DB=EPODOC&amp;CC=AU&amp;NR=2015349052A2$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Sauer, Reiner</creatorcontrib><creatorcontrib>Massicot, Blaise</creatorcontrib><creatorcontrib>Kaup, Burkhard</creatorcontrib><creatorcontrib>Kohl, Manuel</creatorcontrib><creatorcontrib>Klemmer, Ricarda</creatorcontrib><creatorcontrib>Kiewitz, Chrysanthus</creatorcontrib><title>Method for producing a nitrided packaging steel</title><description>The invention relates to a method for producing a nitrided packaging steel from a hot-rolled steel product with a carbon content of 400 to 1200 ppm, characterized by a cold-rolling of the steel product to a flat steel product, subsequent recrystallization annealing of the cold-rolled flat steel product in an annealing furnace, in particular a continuous annealing furnace, wherein a nitrogen-containing gas is supplied into the annealing furnace and is directed at the flat steel product in order to introduce unbonded nitrogen into the flat steel product in an amount corresponding to a concentration of more than 100 ppm, or to increase the amount of unbonded nitrogen in the flat steel product to a concentration of more than 100 ppm, and subsequent cooling of the recrystallized annealed flat steel product at a cooling rate of at least 100 K/s directly after the recrystallization annealing. Using this method, cold-rolled flat steel products may be produced for packaging purposes with a tensile strength of more than 650 MPa and in particular between 700 and 850 MPa.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2017</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND3TS3JyE9RSMsvUigoyk8pTc7MS1dIVMjLLCnKTElNUShITM5OTAcJFpekpubwMLCmJeYUp_JCaW4GZTfXEGcP3dSC_PjUYqDq1LzUknjHUCMDQ1NjE0sDUyNHI2PiVAEAwGErjw</recordid><startdate>20170928</startdate><enddate>20170928</enddate><creator>Sauer, Reiner</creator><creator>Massicot, Blaise</creator><creator>Kaup, Burkhard</creator><creator>Kohl, Manuel</creator><creator>Klemmer, Ricarda</creator><creator>Kiewitz, Chrysanthus</creator><scope>EVB</scope></search><sort><creationdate>20170928</creationdate><title>Method for producing a nitrided packaging steel</title><author>Sauer, Reiner ; Massicot, Blaise ; Kaup, Burkhard ; Kohl, Manuel ; Klemmer, Ricarda ; Kiewitz, Chrysanthus</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_AU2015349052A23</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2017</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>Sauer, Reiner</creatorcontrib><creatorcontrib>Massicot, Blaise</creatorcontrib><creatorcontrib>Kaup, Burkhard</creatorcontrib><creatorcontrib>Kohl, Manuel</creatorcontrib><creatorcontrib>Klemmer, Ricarda</creatorcontrib><creatorcontrib>Kiewitz, Chrysanthus</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Sauer, Reiner</au><au>Massicot, Blaise</au><au>Kaup, Burkhard</au><au>Kohl, Manuel</au><au>Klemmer, Ricarda</au><au>Kiewitz, Chrysanthus</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for producing a nitrided packaging steel</title><date>2017-09-28</date><risdate>2017</risdate><abstract>The invention relates to a method for producing a nitrided packaging steel from a hot-rolled steel product with a carbon content of 400 to 1200 ppm, characterized by a cold-rolling of the steel product to a flat steel product, subsequent recrystallization annealing of the cold-rolled flat steel product in an annealing furnace, in particular a continuous annealing furnace, wherein a nitrogen-containing gas is supplied into the annealing furnace and is directed at the flat steel product in order to introduce unbonded nitrogen into the flat steel product in an amount corresponding to a concentration of more than 100 ppm, or to increase the amount of unbonded nitrogen in the flat steel product to a concentration of more than 100 ppm, and subsequent cooling of the recrystallized annealed flat steel product at a cooling rate of at least 100 K/s directly after the recrystallization annealing. Using this method, cold-rolled flat steel products may be produced for packaging purposes with a tensile strength of more than 650 MPa and in particular between 700 and 850 MPa.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_AU2015349052A2
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Method for producing a nitrided packaging steel
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T07%3A13%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Sauer,%20Reiner&rft.date=2017-09-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EAU2015349052A2%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true