Method of leaching copper sulfide ore

A method of leaching copper sulfide ore includes leaching copper from copper sulfide ore using a sulfuric acid solution comprising iodide ion and iron (III) ion surplus to the iodide ion as a leaching solution; reducing iodine in a solution obtained after the leaching step to less than 1 mg/L by an...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KUWANO, KENICHI, MANABE, MANABU, ABE, ATSUKO, MIURA, AKIRA
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KUWANO, KENICHI
MANABE, MANABU
ABE, ATSUKO
MIURA, AKIRA
description A method of leaching copper sulfide ore includes leaching copper from copper sulfide ore using a sulfuric acid solution comprising iodide ion and iron (III) ion surplus to the iodide ion as a leaching solution; reducing iodine in a solution obtained after the leaching step to less than 1 mg/L by an activated carbon treatment; and oxidizing iron (II) ion or newly added iron (II) ion in a solution obtained after the iodine reduction step by using iron oxidizing microbes to recover iron (III) ion. IODIDE REPLACEMENT AQUEOUS SOLUTION CONTAINING IODINE COPPER LEACHING STE ACIDIC ACTIVATED CARBON AQUEOUS SOLUTION' SOLUTION TREATMENT STEP --- CONTAINING CONTAINN (IODINE RECOVERING STEP) RECOVERED IODINE EXTRACTION -IELECTROWINNING STE P - CPERCTHD -- IRON (II) 1ION SOLUTION REPLACEMENT IRON OXIDIZATI ON STEP IODIDE REPLACEMENT AQUEOUS SOLUTION CONTAINING IODINE COPPER LEACHING STEP ACIDIC ANION EXCHANGE RESIN AQUEOUS SOLUTION' SOLUTION TREATMENT STEP CONTAINING CNTAINN (IODINE RECOVERING STEP) RECOVERED IODINE EXTRACTION -,ELECTROWINNING STEP HCPE AHD [ACTIVATED CARBON AQUEOUS SOLUTION TREATMENT STEP CONTAINING (IODINE RECOVERING STEP) RECOVERED lODINE. IRON (II1) ION SOLUTION REPLACEMENT] IRON OXIDIZATION STEP FIG. 2
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_AU2011201167A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>AU2011201167A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_AU2011201167A13</originalsourceid><addsrcrecordid>eNrjZFD1TS3JyE9RyE9TyElNTM7IzEtXSM4vKEgtUiguzUnLTElVyC9K5WFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8Y6hRgaGhiBsZu5oaEycKgCxuyeS</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method of leaching copper sulfide ore</title><source>esp@cenet</source><creator>KUWANO, KENICHI ; MANABE, MANABU ; ABE, ATSUKO ; MIURA, AKIRA</creator><creatorcontrib>KUWANO, KENICHI ; MANABE, MANABU ; ABE, ATSUKO ; MIURA, AKIRA</creatorcontrib><description>A method of leaching copper sulfide ore includes leaching copper from copper sulfide ore using a sulfuric acid solution comprising iodide ion and iron (III) ion surplus to the iodide ion as a leaching solution; reducing iodine in a solution obtained after the leaching step to less than 1 mg/L by an activated carbon treatment; and oxidizing iron (II) ion or newly added iron (II) ion in a solution obtained after the iodine reduction step by using iron oxidizing microbes to recover iron (III) ion. IODIDE REPLACEMENT AQUEOUS SOLUTION CONTAINING IODINE COPPER LEACHING STE ACIDIC ACTIVATED CARBON AQUEOUS SOLUTION' SOLUTION TREATMENT STEP --- CONTAINING CONTAINN (IODINE RECOVERING STEP) RECOVERED IODINE EXTRACTION -IELECTROWINNING STE P - CPERCTHD -- IRON (II) 1ION SOLUTION REPLACEMENT IRON OXIDIZATI ON STEP IODIDE REPLACEMENT AQUEOUS SOLUTION CONTAINING IODINE COPPER LEACHING STEP ACIDIC ANION EXCHANGE RESIN AQUEOUS SOLUTION' SOLUTION TREATMENT STEP CONTAINING CNTAINN (IODINE RECOVERING STEP) RECOVERED IODINE EXTRACTION -,ELECTROWINNING STEP HCPE AHD [ACTIVATED CARBON AQUEOUS SOLUTION TREATMENT STEP CONTAINING (IODINE RECOVERING STEP) RECOVERED lODINE. IRON (II1) ION SOLUTION REPLACEMENT] IRON OXIDIZATION STEP FIG. 2</description><language>eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2011</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20111006&amp;DB=EPODOC&amp;CC=AU&amp;NR=2011201167A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20111006&amp;DB=EPODOC&amp;CC=AU&amp;NR=2011201167A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KUWANO, KENICHI</creatorcontrib><creatorcontrib>MANABE, MANABU</creatorcontrib><creatorcontrib>ABE, ATSUKO</creatorcontrib><creatorcontrib>MIURA, AKIRA</creatorcontrib><title>Method of leaching copper sulfide ore</title><description>A method of leaching copper sulfide ore includes leaching copper from copper sulfide ore using a sulfuric acid solution comprising iodide ion and iron (III) ion surplus to the iodide ion as a leaching solution; reducing iodine in a solution obtained after the leaching step to less than 1 mg/L by an activated carbon treatment; and oxidizing iron (II) ion or newly added iron (II) ion in a solution obtained after the iodine reduction step by using iron oxidizing microbes to recover iron (III) ion. IODIDE REPLACEMENT AQUEOUS SOLUTION CONTAINING IODINE COPPER LEACHING STE ACIDIC ACTIVATED CARBON AQUEOUS SOLUTION' SOLUTION TREATMENT STEP --- CONTAINING CONTAINN (IODINE RECOVERING STEP) RECOVERED IODINE EXTRACTION -IELECTROWINNING STE P - CPERCTHD -- IRON (II) 1ION SOLUTION REPLACEMENT IRON OXIDIZATI ON STEP IODIDE REPLACEMENT AQUEOUS SOLUTION CONTAINING IODINE COPPER LEACHING STEP ACIDIC ANION EXCHANGE RESIN AQUEOUS SOLUTION' SOLUTION TREATMENT STEP CONTAINING CNTAINN (IODINE RECOVERING STEP) RECOVERED IODINE EXTRACTION -,ELECTROWINNING STEP HCPE AHD [ACTIVATED CARBON AQUEOUS SOLUTION TREATMENT STEP CONTAINING (IODINE RECOVERING STEP) RECOVERED lODINE. IRON (II1) ION SOLUTION REPLACEMENT] IRON OXIDIZATION STEP FIG. 2</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2011</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD1TS3JyE9RyE9TyElNTM7IzEtXSM4vKEgtUiguzUnLTElVyC9K5WFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8Y6hRgaGhiBsZu5oaEycKgCxuyeS</recordid><startdate>20111006</startdate><enddate>20111006</enddate><creator>KUWANO, KENICHI</creator><creator>MANABE, MANABU</creator><creator>ABE, ATSUKO</creator><creator>MIURA, AKIRA</creator><scope>EVB</scope></search><sort><creationdate>20111006</creationdate><title>Method of leaching copper sulfide ore</title><author>KUWANO, KENICHI ; MANABE, MANABU ; ABE, ATSUKO ; MIURA, AKIRA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_AU2011201167A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2011</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>KUWANO, KENICHI</creatorcontrib><creatorcontrib>MANABE, MANABU</creatorcontrib><creatorcontrib>ABE, ATSUKO</creatorcontrib><creatorcontrib>MIURA, AKIRA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KUWANO, KENICHI</au><au>MANABE, MANABU</au><au>ABE, ATSUKO</au><au>MIURA, AKIRA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method of leaching copper sulfide ore</title><date>2011-10-06</date><risdate>2011</risdate><abstract>A method of leaching copper sulfide ore includes leaching copper from copper sulfide ore using a sulfuric acid solution comprising iodide ion and iron (III) ion surplus to the iodide ion as a leaching solution; reducing iodine in a solution obtained after the leaching step to less than 1 mg/L by an activated carbon treatment; and oxidizing iron (II) ion or newly added iron (II) ion in a solution obtained after the iodine reduction step by using iron oxidizing microbes to recover iron (III) ion. IODIDE REPLACEMENT AQUEOUS SOLUTION CONTAINING IODINE COPPER LEACHING STE ACIDIC ACTIVATED CARBON AQUEOUS SOLUTION' SOLUTION TREATMENT STEP --- CONTAINING CONTAINN (IODINE RECOVERING STEP) RECOVERED IODINE EXTRACTION -IELECTROWINNING STE P - CPERCTHD -- IRON (II) 1ION SOLUTION REPLACEMENT IRON OXIDIZATI ON STEP IODIDE REPLACEMENT AQUEOUS SOLUTION CONTAINING IODINE COPPER LEACHING STEP ACIDIC ANION EXCHANGE RESIN AQUEOUS SOLUTION' SOLUTION TREATMENT STEP CONTAINING CNTAINN (IODINE RECOVERING STEP) RECOVERED IODINE EXTRACTION -,ELECTROWINNING STEP HCPE AHD [ACTIVATED CARBON AQUEOUS SOLUTION TREATMENT STEP CONTAINING (IODINE RECOVERING STEP) RECOVERED lODINE. IRON (II1) ION SOLUTION REPLACEMENT] IRON OXIDIZATION STEP FIG. 2</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_AU2011201167A1
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Method of leaching copper sulfide ore
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-28T13%3A47%3A21IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KUWANO,%20KENICHI&rft.date=2011-10-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EAU2011201167A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true