Styrenic resin composition and articles produced therefrom

Styrenic resin composition comprising a rubber modified styrene maleic anhydride copolymer and polybutene. The resin is prepared by several methods including adding polybutene into the reactor, or adding polybutene to the syrup exiting the reactor and prior to entering the devolatilizer, or compound...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: RICHARD ALBERT COOPER, JOHN CHI HEE KWOK, STEVEN MICHAEL KRUPINSKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator RICHARD ALBERT COOPER
JOHN CHI HEE KWOK
STEVEN MICHAEL KRUPINSKI
description Styrenic resin composition comprising a rubber modified styrene maleic anhydride copolymer and polybutene. The resin is prepared by several methods including adding polybutene into the reactor, or adding polybutene to the syrup exiting the reactor and prior to entering the devolatilizer, or compounding polybutene into the polymer in an extruder after the polymer exits the devolatilizer. The polybutene ranges from 0.1 to 8% by weight and has a number average molecular weight from 900 to 2500. The rubber ranges from 4% to 20% by weight and has a particle size from 0.1 micron to 11 microns. The resin can be extruded into sheet and thermoformed into an article or can be coextruded to produce a laminated article, which may be a container for packaged foods that can be heated in microwave ovens and which container has improved toughness, elongation, and heat distortion resistance properties.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_AU2004265555A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>AU2004265555A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_AU2004265555A13</originalsourceid><addsrcrecordid>eNrjZLAKLqksSs3LTFYoSi3OzFNIzs8tyC_OLMnMz1NIzEtRSCwqyUzOSS1WKCjKTylNTk1RKMlILUpNK8rP5WFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8Y6hRgYGJkZmpkDgaGhMnCoAgQAwhw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Styrenic resin composition and articles produced therefrom</title><source>esp@cenet</source><creator>RICHARD ALBERT COOPER ; JOHN CHI HEE KWOK ; STEVEN MICHAEL KRUPINSKI</creator><creatorcontrib>RICHARD ALBERT COOPER ; JOHN CHI HEE KWOK ; STEVEN MICHAEL KRUPINSKI</creatorcontrib><description>Styrenic resin composition comprising a rubber modified styrene maleic anhydride copolymer and polybutene. The resin is prepared by several methods including adding polybutene into the reactor, or adding polybutene to the syrup exiting the reactor and prior to entering the devolatilizer, or compounding polybutene into the polymer in an extruder after the polymer exits the devolatilizer. The polybutene ranges from 0.1 to 8% by weight and has a number average molecular weight from 900 to 2500. The rubber ranges from 4% to 20% by weight and has a particle size from 0.1 micron to 11 microns. The resin can be extruded into sheet and thermoformed into an article or can be coextruded to produce a laminated article, which may be a container for packaged foods that can be heated in microwave ovens and which container has improved toughness, elongation, and heat distortion resistance properties.</description><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2005</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050224&amp;DB=EPODOC&amp;CC=AU&amp;NR=2004265555A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20050224&amp;DB=EPODOC&amp;CC=AU&amp;NR=2004265555A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>RICHARD ALBERT COOPER</creatorcontrib><creatorcontrib>JOHN CHI HEE KWOK</creatorcontrib><creatorcontrib>STEVEN MICHAEL KRUPINSKI</creatorcontrib><title>Styrenic resin composition and articles produced therefrom</title><description>Styrenic resin composition comprising a rubber modified styrene maleic anhydride copolymer and polybutene. The resin is prepared by several methods including adding polybutene into the reactor, or adding polybutene to the syrup exiting the reactor and prior to entering the devolatilizer, or compounding polybutene into the polymer in an extruder after the polymer exits the devolatilizer. The polybutene ranges from 0.1 to 8% by weight and has a number average molecular weight from 900 to 2500. The rubber ranges from 4% to 20% by weight and has a particle size from 0.1 micron to 11 microns. The resin can be extruded into sheet and thermoformed into an article or can be coextruded to produce a laminated article, which may be a container for packaged foods that can be heated in microwave ovens and which container has improved toughness, elongation, and heat distortion resistance properties.</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2005</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAKLqksSs3LTFYoSi3OzFNIzs8tyC_OLMnMz1NIzEtRSCwqyUzOSS1WKCjKTylNTk1RKMlILUpNK8rP5WFgTUvMKU7lhdLcDMpuriHOHrqpBfnxqcUFicmpeakl8Y6hRgYGJkZmpkDgaGhMnCoAgQAwhw</recordid><startdate>20050224</startdate><enddate>20050224</enddate><creator>RICHARD ALBERT COOPER</creator><creator>JOHN CHI HEE KWOK</creator><creator>STEVEN MICHAEL KRUPINSKI</creator><scope>EVB</scope></search><sort><creationdate>20050224</creationdate><title>Styrenic resin composition and articles produced therefrom</title><author>RICHARD ALBERT COOPER ; JOHN CHI HEE KWOK ; STEVEN MICHAEL KRUPINSKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_AU2004265555A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2005</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>RICHARD ALBERT COOPER</creatorcontrib><creatorcontrib>JOHN CHI HEE KWOK</creatorcontrib><creatorcontrib>STEVEN MICHAEL KRUPINSKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>RICHARD ALBERT COOPER</au><au>JOHN CHI HEE KWOK</au><au>STEVEN MICHAEL KRUPINSKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Styrenic resin composition and articles produced therefrom</title><date>2005-02-24</date><risdate>2005</risdate><abstract>Styrenic resin composition comprising a rubber modified styrene maleic anhydride copolymer and polybutene. The resin is prepared by several methods including adding polybutene into the reactor, or adding polybutene to the syrup exiting the reactor and prior to entering the devolatilizer, or compounding polybutene into the polymer in an extruder after the polymer exits the devolatilizer. The polybutene ranges from 0.1 to 8% by weight and has a number average molecular weight from 900 to 2500. The rubber ranges from 4% to 20% by weight and has a particle size from 0.1 micron to 11 microns. The resin can be extruded into sheet and thermoformed into an article or can be coextruded to produce a laminated article, which may be a container for packaged foods that can be heated in microwave ovens and which container has improved toughness, elongation, and heat distortion resistance properties.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_AU2004265555A1
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title Styrenic resin composition and articles produced therefrom
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T13%3A46%3A39IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=RICHARD%20ALBERT%20COOPER&rft.date=2005-02-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EAU2004265555A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true