The Viscoelastic Properties of Crosslinked Poly(Ethylene Tetrasulfide) III

THE VISCOELASTIC PROPERTIES OF POLY(ETHYLENE TETRASULFIDE) CONTAINING 5% OF THE CROSSLINKING AGENT 1,2,3 TRICHLOROPROPANE, HAVE BEEN EXAMINED OVER A WIDE TEMPERATURE RANGE, ESPECIALLY IN THE TRANSITION REGION. THIS EXTENDS THE WORK PREVIOUSLY REPORTED ON THE PREPARATION OF CROSSLINKED POLY(ETHYLENE...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Tobolsky,A. V, Beevers,R. B, Owen,G. D. T
Format: Report
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Tobolsky,A. V
Beevers,R. B
Owen,G. D. T
description THE VISCOELASTIC PROPERTIES OF POLY(ETHYLENE TETRASULFIDE) CONTAINING 5% OF THE CROSSLINKING AGENT 1,2,3 TRICHLOROPROPANE, HAVE BEEN EXAMINED OVER A WIDE TEMPERATURE RANGE, ESPECIALLY IN THE TRANSITION REGION. THIS EXTENDS THE WORK PREVIOUSLY REPORTED ON THE PREPARATION OF CROSSLINKED POLY(ETHYLENE TETRASULFIDES) AND THEIR PROPERTIES IN THE REGION OF CHEMICAL STRESS RELAXATION. FROM THE RELAXATION CURVES THE MASTER CURVE HAS BEEN CONSTRUCTED AND THE FIRST AND SECOND APPROXIMATION TO THE DISTRIBUTION OF RELAXATION TIMES EVALUATED. THE DATA HAS BEEN FOUND TO FIT QUITE SATISFACTORILY TO A MODIFIED WILLIAMS-LANDEL-FERRY TYPE EQUATION. APPARENT ACTIVATION ENERGIES HAVE BEEN EVALUATED AND SHOW A MARKED TEMPERATURE DEPENDENCE WITH PEAK VALUE OF 207 K CALS MOLE TO THE NEGATIVE FIRST POWER AT -17 DEGREES C. (AUTHOR-PL).
format Report
fullrecord <record><control><sourceid>dtic_1RU</sourceid><recordid>TN_cdi_dtic_stinet_ADA952731</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>ADA952731</sourcerecordid><originalsourceid>FETCH-dtic_stinet_ADA9527313</originalsourceid><addsrcrecordid>eNrjZPAKyUhVCMssTs5PzUksLslMVggoyi9ILSrJTC1WyE9TcC7KLy7OyczLTk1RCMjPqdRwLcmozEnNS1UISS0pSiwuzUnLTEnVVPD09ORhYE1LzClO5YXS3Awybq4hzh66KUBj44Fm56WWxDu6OFqaGpkbGxoTkAYA8Xcxyg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>report</recordtype></control><display><type>report</type><title>The Viscoelastic Properties of Crosslinked Poly(Ethylene Tetrasulfide) III</title><source>DTIC Technical Reports</source><creator>Tobolsky,A. V ; Beevers,R. B ; Owen,G. D. T</creator><creatorcontrib>Tobolsky,A. V ; Beevers,R. B ; Owen,G. D. T ; PRINCETON UNIV N J FRICK CHEMICAL LAB</creatorcontrib><description>THE VISCOELASTIC PROPERTIES OF POLY(ETHYLENE TETRASULFIDE) CONTAINING 5% OF THE CROSSLINKING AGENT 1,2,3 TRICHLOROPROPANE, HAVE BEEN EXAMINED OVER A WIDE TEMPERATURE RANGE, ESPECIALLY IN THE TRANSITION REGION. THIS EXTENDS THE WORK PREVIOUSLY REPORTED ON THE PREPARATION OF CROSSLINKED POLY(ETHYLENE TETRASULFIDES) AND THEIR PROPERTIES IN THE REGION OF CHEMICAL STRESS RELAXATION. FROM THE RELAXATION CURVES THE MASTER CURVE HAS BEEN CONSTRUCTED AND THE FIRST AND SECOND APPROXIMATION TO THE DISTRIBUTION OF RELAXATION TIMES EVALUATED. THE DATA HAS BEEN FOUND TO FIT QUITE SATISFACTORILY TO A MODIFIED WILLIAMS-LANDEL-FERRY TYPE EQUATION. APPARENT ACTIVATION ENERGIES HAVE BEEN EVALUATED AND SHOW A MARKED TEMPERATURE DEPENDENCE WITH PEAK VALUE OF 207 K CALS MOLE TO THE NEGATIVE FIRST POWER AT -17 DEGREES C. (AUTHOR-PL).</description><language>eng</language><subject>Activation energy ; Approximation(Mathematics) ; Chlorides ; Crosslinking(Chemistry) ; Distribution ; Mechanics ; Plastics ; Polyethylene ; Polysulfides ; Propane ; Relaxation time ; Transition temperature ; Viscoelasticity</subject><creationdate>1962</creationdate><rights>APPROVED FOR PUBLIC RELEASE</rights><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>230,776,881,27544,27545</link.rule.ids><linktorsrc>$$Uhttps://apps.dtic.mil/sti/citations/ADA952731$$EView_record_in_DTIC$$FView_record_in_$$GDTIC$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Tobolsky,A. V</creatorcontrib><creatorcontrib>Beevers,R. B</creatorcontrib><creatorcontrib>Owen,G. D. T</creatorcontrib><creatorcontrib>PRINCETON UNIV N J FRICK CHEMICAL LAB</creatorcontrib><title>The Viscoelastic Properties of Crosslinked Poly(Ethylene Tetrasulfide) III</title><description>THE VISCOELASTIC PROPERTIES OF POLY(ETHYLENE TETRASULFIDE) CONTAINING 5% OF THE CROSSLINKING AGENT 1,2,3 TRICHLOROPROPANE, HAVE BEEN EXAMINED OVER A WIDE TEMPERATURE RANGE, ESPECIALLY IN THE TRANSITION REGION. THIS EXTENDS THE WORK PREVIOUSLY REPORTED ON THE PREPARATION OF CROSSLINKED POLY(ETHYLENE TETRASULFIDES) AND THEIR PROPERTIES IN THE REGION OF CHEMICAL STRESS RELAXATION. FROM THE RELAXATION CURVES THE MASTER CURVE HAS BEEN CONSTRUCTED AND THE FIRST AND SECOND APPROXIMATION TO THE DISTRIBUTION OF RELAXATION TIMES EVALUATED. THE DATA HAS BEEN FOUND TO FIT QUITE SATISFACTORILY TO A MODIFIED WILLIAMS-LANDEL-FERRY TYPE EQUATION. APPARENT ACTIVATION ENERGIES HAVE BEEN EVALUATED AND SHOW A MARKED TEMPERATURE DEPENDENCE WITH PEAK VALUE OF 207 K CALS MOLE TO THE NEGATIVE FIRST POWER AT -17 DEGREES C. (AUTHOR-PL).</description><subject>Activation energy</subject><subject>Approximation(Mathematics)</subject><subject>Chlorides</subject><subject>Crosslinking(Chemistry)</subject><subject>Distribution</subject><subject>Mechanics</subject><subject>Plastics</subject><subject>Polyethylene</subject><subject>Polysulfides</subject><subject>Propane</subject><subject>Relaxation time</subject><subject>Transition temperature</subject><subject>Viscoelasticity</subject><fulltext>true</fulltext><rsrctype>report</rsrctype><creationdate>1962</creationdate><recordtype>report</recordtype><sourceid>1RU</sourceid><recordid>eNrjZPAKyUhVCMssTs5PzUksLslMVggoyi9ILSrJTC1WyE9TcC7KLy7OyczLTk1RCMjPqdRwLcmozEnNS1UISS0pSiwuzUnLTEnVVPD09ORhYE1LzClO5YXS3Awybq4hzh66KUBj44Fm56WWxDu6OFqaGpkbGxoTkAYA8Xcxyg</recordid><startdate>196208</startdate><enddate>196208</enddate><creator>Tobolsky,A. V</creator><creator>Beevers,R. B</creator><creator>Owen,G. D. T</creator><scope>1RU</scope><scope>BHM</scope></search><sort><creationdate>196208</creationdate><title>The Viscoelastic Properties of Crosslinked Poly(Ethylene Tetrasulfide) III</title><author>Tobolsky,A. V ; Beevers,R. B ; Owen,G. D. T</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-dtic_stinet_ADA9527313</frbrgroupid><rsrctype>reports</rsrctype><prefilter>reports</prefilter><language>eng</language><creationdate>1962</creationdate><topic>Activation energy</topic><topic>Approximation(Mathematics)</topic><topic>Chlorides</topic><topic>Crosslinking(Chemistry)</topic><topic>Distribution</topic><topic>Mechanics</topic><topic>Plastics</topic><topic>Polyethylene</topic><topic>Polysulfides</topic><topic>Propane</topic><topic>Relaxation time</topic><topic>Transition temperature</topic><topic>Viscoelasticity</topic><toplevel>online_resources</toplevel><creatorcontrib>Tobolsky,A. V</creatorcontrib><creatorcontrib>Beevers,R. B</creatorcontrib><creatorcontrib>Owen,G. D. T</creatorcontrib><creatorcontrib>PRINCETON UNIV N J FRICK CHEMICAL LAB</creatorcontrib><collection>DTIC Technical Reports</collection><collection>DTIC STINET</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Tobolsky,A. V</au><au>Beevers,R. B</au><au>Owen,G. D. T</au><aucorp>PRINCETON UNIV N J FRICK CHEMICAL LAB</aucorp><format>book</format><genre>unknown</genre><ristype>RPRT</ristype><btitle>The Viscoelastic Properties of Crosslinked Poly(Ethylene Tetrasulfide) III</btitle><date>1962-08</date><risdate>1962</risdate><abstract>THE VISCOELASTIC PROPERTIES OF POLY(ETHYLENE TETRASULFIDE) CONTAINING 5% OF THE CROSSLINKING AGENT 1,2,3 TRICHLOROPROPANE, HAVE BEEN EXAMINED OVER A WIDE TEMPERATURE RANGE, ESPECIALLY IN THE TRANSITION REGION. THIS EXTENDS THE WORK PREVIOUSLY REPORTED ON THE PREPARATION OF CROSSLINKED POLY(ETHYLENE TETRASULFIDES) AND THEIR PROPERTIES IN THE REGION OF CHEMICAL STRESS RELAXATION. FROM THE RELAXATION CURVES THE MASTER CURVE HAS BEEN CONSTRUCTED AND THE FIRST AND SECOND APPROXIMATION TO THE DISTRIBUTION OF RELAXATION TIMES EVALUATED. THE DATA HAS BEEN FOUND TO FIT QUITE SATISFACTORILY TO A MODIFIED WILLIAMS-LANDEL-FERRY TYPE EQUATION. APPARENT ACTIVATION ENERGIES HAVE BEEN EVALUATED AND SHOW A MARKED TEMPERATURE DEPENDENCE WITH PEAK VALUE OF 207 K CALS MOLE TO THE NEGATIVE FIRST POWER AT -17 DEGREES C. (AUTHOR-PL).</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_dtic_stinet_ADA952731
source DTIC Technical Reports
subjects Activation energy
Approximation(Mathematics)
Chlorides
Crosslinking(Chemistry)
Distribution
Mechanics
Plastics
Polyethylene
Polysulfides
Propane
Relaxation time
Transition temperature
Viscoelasticity
title The Viscoelastic Properties of Crosslinked Poly(Ethylene Tetrasulfide) III
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T16%3A56%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-dtic_1RU&rft_val_fmt=info:ofi/fmt:kev:mtx:book&rft.genre=unknown&rft.btitle=The%20Viscoelastic%20Properties%20of%20Crosslinked%20Poly(Ethylene%20Tetrasulfide)%20III&rft.au=Tobolsky,A.%20V&rft.aucorp=PRINCETON%20UNIV%20N%20J%20FRICK%20CHEMICAL%20LAB&rft.date=1962-08&rft_id=info:doi/&rft_dat=%3Cdtic_1RU%3EADA952731%3C/dtic_1RU%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true