THE TESTING OF HERMETIC SEALS AND SEPARATORS, POSITIVE PLATE STUDIES, AND INVESTIGATIONS ON THE UNIFORMITY OF SEALED NICKEL-CADMIUM CELLS
Cells were charged and then discharged with and without an 8 hour stand period. Capacity was decreased by an average of 9% when the cells were on open circuit for 8 hours after charge. The capacity dependence upon charge rate was determined after a 24 AH input. Findings were similar to those observe...