In this study, we presented the synthesis of LaNi0.3Co0.7O3- delta (LNCO) and SrCo0.8Fe0.2O3- delta (SFCO) perovskites and their catalytic reactivity under CO gas flow. The synthesis method is based on the complexation method combining ethylenediaminetetraacetic acid (EDTA)-citrate. The as-prepared...
Gespeichert in:
Veröffentlicht in: | Catalysts 2014-06, Vol.4 (2), p.77-88 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | In this study, we presented the synthesis of LaNi0.3Co0.7O3- delta (LNCO) and SrCo0.8Fe0.2O3- delta (SFCO) perovskites and their catalytic reactivity under CO gas flow. The synthesis method is based on the complexation method combining ethylenediaminetetraacetic acid (EDTA)-citrate. The as-prepared materials were characterized using X-ray diffraction/Rietveld refinement and electron microscopy. The diffractograms and Rietveld refinement showed that the EDTA-citrate method allows us to obtain monophasic powders with submicronic size. The structural analyses revealed different morphologies linked to the crystallinity of LNCO and SFCO, and to the mean crystallite size. The catalytic performances of LNCO and SFCO were studied in situ by Fourier Transform InfraRed spectrometer as a function of time and temperature. The catalytic process gave rise to total oxidation with carbon dioxide and water production. LNCO and SFCO exhibit the same profile for catalytic activity with a conversion rate of twice as high for LNCO. Below 150 degree C, the kinetic conversion is slow, but beyond this temperature they reach rapidly the complete transformation at 250 degree C and 275 degree C for LNCO and SFCO, respectively. |
---|---|
ISSN: | 2073-4344 2073-4344 |
DOI: | 10.3390/catal4020077 |