Gallium doped zinc oxide (ZnO:Ga) thin films were deposited on glass substrates by means of r.f. magnetron sputtering at room temperature, non-reactively. Both the wet chemical etching behavior and the influence of etching time variations on ZnO:Ga films were investigated. 0.1 % HCl was used as an e...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materialprüfung 2018-11, Vol.60 (11), p.1097-1103
Hauptverfasser: Duygulu, Nilufer Evcimen, Mustafaoglu, Ummu, Kodolbas, Alp Osman, Karaaslan, Ahmet
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 1103
container_issue 11
container_start_page 1097
container_title Materialprüfung
container_volume 60
creator Duygulu, Nilufer Evcimen
Mustafaoglu, Ummu
Kodolbas, Alp Osman
Karaaslan, Ahmet
description Gallium doped zinc oxide (ZnO:Ga) thin films were deposited on glass substrates by means of r.f. magnetron sputtering at room temperature, non-reactively. Both the wet chemical etching behavior and the influence of etching time variations on ZnO:Ga films were investigated. 0.1 % HCl was used as an etchant and the etching time varied in small increments. The thickness of the etched films was determined using scanning electron microscopy (SEM). The etching depth of the ZnO:Ga thin films increased from 13 to 58 % and the resistivity was 10 Ω × cm at different etching times. X-ray diffraction (XRD) results revealed that etching did not influence the crystal structure in a clear way. The (002) peak intensity to thickness ratio reached its maximum at 15 s while full width at half maximum (FWHM) was determined as the minimum. Morphological investigations were conducted using both high resolution scanning electron microscopy (HRSEM) and atomic force microscopy (AFM). The surface of the etched films became rougher and the root mean square (RMS) values increased according to etching time; at 15 s etching the RMS value was calculated to be 8.48 nm. The optical transmittance was measured using an ultraviolet–visible (UV–VIS) spectrophotometer and decreased from 86.60 to 82.50 % while haze increased from 0.85 to 16.68 %.
doi_str_mv 10.3139/120.111254
format Article
fullrecord <record><control><sourceid>walterdegruyter_cross</sourceid><recordid>TN_cdi_crossref_primary_10_3139_120_111254</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_3139_120_11125460111097</sourcerecordid><originalsourceid>FETCH-LOGICAL-c241t-bfe7cb7bf94d17945d5e11fa57fbea12173ceb602150897327e68027e68d813c3</originalsourceid><addsrcrecordid>eNptjzFPwzAQhS0EEqGw8AuysCCl3NlxnHRDVSmVKnWBhcWyHbtNlSbITkH99xjC2OXeSffu3n2E3CNMGbLqCSlMEZHy_IIkFCuelVzQS5IAUJ5xBnBNbkLYAxSc0iIhD4vB7Jpum2q7U19N79PepR_dZrZU6RAHqWvaQ7glV061wd7964S8vyze5q_ZerNczZ_XmaE5Dpl2VhgttKvyGkWV85pbRKe4cNoqpCiYsboAihzKSjAqbFHCX61LZIZNyON41_g-BG-d_PTNQfmTRJC_gDICyhEwmmej-Vu1g_W13frjKTZy3x99F988s1RAVIjRP8OuUoU</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Etching behavior of ZnO:Ga thin films</title><source>De Gruyter journals</source><creator>Duygulu, Nilufer Evcimen ; Mustafaoglu, Ummu ; Kodolbas, Alp Osman ; Karaaslan, Ahmet</creator><creatorcontrib>Duygulu, Nilufer Evcimen ; Mustafaoglu, Ummu ; Kodolbas, Alp Osman ; Karaaslan, Ahmet</creatorcontrib><description>Gallium doped zinc oxide (ZnO:Ga) thin films were deposited on glass substrates by means of r.f. magnetron sputtering at room temperature, non-reactively. Both the wet chemical etching behavior and the influence of etching time variations on ZnO:Ga films were investigated. 0.1 % HCl was used as an etchant and the etching time varied in small increments. The thickness of the etched films was determined using scanning electron microscopy (SEM). The etching depth of the ZnO:Ga thin films increased from 13 to 58 % and the resistivity was 10 Ω × cm at different etching times. X-ray diffraction (XRD) results revealed that etching did not influence the crystal structure in a clear way. The (002) peak intensity to thickness ratio reached its maximum at 15 s while full width at half maximum (FWHM) was determined as the minimum. Morphological investigations were conducted using both high resolution scanning electron microscopy (HRSEM) and atomic force microscopy (AFM). The surface of the etched films became rougher and the root mean square (RMS) values increased according to etching time; at 15 s etching the RMS value was calculated to be 8.48 nm. The optical transmittance was measured using an ultraviolet–visible (UV–VIS) spectrophotometer and decreased from 86.60 to 82.50 % while haze increased from 0.85 to 16.68 %.</description><identifier>ISSN: 0025-5300</identifier><identifier>EISSN: 2195-8572</identifier><identifier>DOI: 10.3139/120.111254</identifier><language>eng</language><publisher>De Gruyter</publisher><ispartof>Materialprüfung, 2018-11, Vol.60 (11), p.1097-1103</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-c241t-bfe7cb7bf94d17945d5e11fa57fbea12173ceb602150897327e68027e68d813c3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://www.degruyter.com/document/doi/10.3139/120.111254/pdf$$EPDF$$P50$$Gwalterdegruyter$$H</linktopdf><linktohtml>$$Uhttps://www.degruyter.com/document/doi/10.3139/120.111254/html$$EHTML$$P50$$Gwalterdegruyter$$H</linktohtml><link.rule.ids>314,776,780,27901,27902,66497,68281</link.rule.ids></links><search><creatorcontrib>Duygulu, Nilufer Evcimen</creatorcontrib><creatorcontrib>Mustafaoglu, Ummu</creatorcontrib><creatorcontrib>Kodolbas, Alp Osman</creatorcontrib><creatorcontrib>Karaaslan, Ahmet</creatorcontrib><title>Etching behavior of ZnO:Ga thin films</title><title>Materialprüfung</title><description>Gallium doped zinc oxide (ZnO:Ga) thin films were deposited on glass substrates by means of r.f. magnetron sputtering at room temperature, non-reactively. Both the wet chemical etching behavior and the influence of etching time variations on ZnO:Ga films were investigated. 0.1 % HCl was used as an etchant and the etching time varied in small increments. The thickness of the etched films was determined using scanning electron microscopy (SEM). The etching depth of the ZnO:Ga thin films increased from 13 to 58 % and the resistivity was 10 Ω × cm at different etching times. X-ray diffraction (XRD) results revealed that etching did not influence the crystal structure in a clear way. The (002) peak intensity to thickness ratio reached its maximum at 15 s while full width at half maximum (FWHM) was determined as the minimum. Morphological investigations were conducted using both high resolution scanning electron microscopy (HRSEM) and atomic force microscopy (AFM). The surface of the etched films became rougher and the root mean square (RMS) values increased according to etching time; at 15 s etching the RMS value was calculated to be 8.48 nm. The optical transmittance was measured using an ultraviolet–visible (UV–VIS) spectrophotometer and decreased from 86.60 to 82.50 % while haze increased from 0.85 to 16.68 %.</description><issn>0025-5300</issn><issn>2195-8572</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2018</creationdate><recordtype>article</recordtype><recordid>eNptjzFPwzAQhS0EEqGw8AuysCCl3NlxnHRDVSmVKnWBhcWyHbtNlSbITkH99xjC2OXeSffu3n2E3CNMGbLqCSlMEZHy_IIkFCuelVzQS5IAUJ5xBnBNbkLYAxSc0iIhD4vB7Jpum2q7U19N79PepR_dZrZU6RAHqWvaQ7glV061wd7964S8vyze5q_ZerNczZ_XmaE5Dpl2VhgttKvyGkWV85pbRKe4cNoqpCiYsboAihzKSjAqbFHCX61LZIZNyON41_g-BG-d_PTNQfmTRJC_gDICyhEwmmej-Vu1g_W13frjKTZy3x99F988s1RAVIjRP8OuUoU</recordid><startdate>20181115</startdate><enddate>20181115</enddate><creator>Duygulu, Nilufer Evcimen</creator><creator>Mustafaoglu, Ummu</creator><creator>Kodolbas, Alp Osman</creator><creator>Karaaslan, Ahmet</creator><general>De Gruyter</general><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20181115</creationdate><title>Etching behavior of ZnO:Ga thin films</title><author>Duygulu, Nilufer Evcimen ; Mustafaoglu, Ummu ; Kodolbas, Alp Osman ; Karaaslan, Ahmet</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c241t-bfe7cb7bf94d17945d5e11fa57fbea12173ceb602150897327e68027e68d813c3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2018</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Duygulu, Nilufer Evcimen</creatorcontrib><creatorcontrib>Mustafaoglu, Ummu</creatorcontrib><creatorcontrib>Kodolbas, Alp Osman</creatorcontrib><creatorcontrib>Karaaslan, Ahmet</creatorcontrib><collection>CrossRef</collection><jtitle>Materialprüfung</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Duygulu, Nilufer Evcimen</au><au>Mustafaoglu, Ummu</au><au>Kodolbas, Alp Osman</au><au>Karaaslan, Ahmet</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Etching behavior of ZnO:Ga thin films</atitle><jtitle>Materialprüfung</jtitle><date>2018-11-15</date><risdate>2018</risdate><volume>60</volume><issue>11</issue><spage>1097</spage><epage>1103</epage><pages>1097-1103</pages><issn>0025-5300</issn><eissn>2195-8572</eissn><abstract>Gallium doped zinc oxide (ZnO:Ga) thin films were deposited on glass substrates by means of r.f. magnetron sputtering at room temperature, non-reactively. Both the wet chemical etching behavior and the influence of etching time variations on ZnO:Ga films were investigated. 0.1 % HCl was used as an etchant and the etching time varied in small increments. The thickness of the etched films was determined using scanning electron microscopy (SEM). The etching depth of the ZnO:Ga thin films increased from 13 to 58 % and the resistivity was 10 Ω × cm at different etching times. X-ray diffraction (XRD) results revealed that etching did not influence the crystal structure in a clear way. The (002) peak intensity to thickness ratio reached its maximum at 15 s while full width at half maximum (FWHM) was determined as the minimum. Morphological investigations were conducted using both high resolution scanning electron microscopy (HRSEM) and atomic force microscopy (AFM). The surface of the etched films became rougher and the root mean square (RMS) values increased according to etching time; at 15 s etching the RMS value was calculated to be 8.48 nm. The optical transmittance was measured using an ultraviolet–visible (UV–VIS) spectrophotometer and decreased from 86.60 to 82.50 % while haze increased from 0.85 to 16.68 %.</abstract><pub>De Gruyter</pub><doi>10.3139/120.111254</doi><tpages>7</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0025-5300
ispartof Materialprüfung, 2018-11, Vol.60 (11), p.1097-1103
issn 0025-5300
2195-8572
language eng
recordid cdi_crossref_primary_10_3139_120_111254
source De Gruyter journals
title Etching behavior of ZnO:Ga thin films
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T21%3A05%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-walterdegruyter_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Etching%20behavior%20of%20ZnO:Ga%20thin%20films&rft.jtitle=Materialpr%C3%BCfung&rft.au=Duygulu,%20Nilufer%20Evcimen&rft.date=2018-11-15&rft.volume=60&rft.issue=11&rft.spage=1097&rft.epage=1103&rft.pages=1097-1103&rft.issn=0025-5300&rft.eissn=2195-8572&rft_id=info:doi/10.3139/120.111254&rft_dat=%3Cwalterdegruyter_cross%3E10_3139_120_11125460111097%3C/walterdegruyter_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true