PRODUCTION OF HIGH-PERFORMANCE LOW DENSITY FIBREBOARD FROM CO-REFINED RUBBERWOOD-KENAF CORE FIBRES

A 50:50 kenaf core to rubberwood ratio were used to fabricate low-density fibreboards. Firstly, the fibres were co-refined at 180 °C for 10 min. Refined fibres were sieved on six levels of size distribution. Results on fibre size distribution concluded that the co-refined fibres were similar in size...