The Influence of the Deposition and Annealing Temperatures on the Structure and Properties of Zirconium Oxide

ZrO2 thin films were deposited by atomic vapor deposition (AVD) using Zr[OC(CH3)3]4 as precursor. The maximum growth rate (~7 nm/min) and the strongest crystalline phase with preferential tetragonal/cubic orientation were obtained at 400{degree sign} C. Growth rate and crystallinity dropped down wit...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Lisker, Marco, Silinskas, Mindaugas, Matichyn, Serhiy, Burte, Edmund
Format: Tagungsbericht
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 88
container_issue 7
container_start_page 79
container_title
container_volume 2
creator Lisker, Marco
Silinskas, Mindaugas
Matichyn, Serhiy
Burte, Edmund
description ZrO2 thin films were deposited by atomic vapor deposition (AVD) using Zr[OC(CH3)3]4 as precursor. The maximum growth rate (~7 nm/min) and the strongest crystalline phase with preferential tetragonal/cubic orientation were obtained at 400{degree sign} C. Growth rate and crystallinity dropped down with increasing or decreasing deposition temperature. Additionally, the increase of the deposition temperature changed the crystalline ZrO2 phase from cubic/tetragonal to monoclinic. Annealing reduced the cubic/tetragonal phase and enhanced the monoclinic one. The values of the dielectric constant (up to 32) varied depending on the deposition temperature, film thickness, and annealing temperature. Leakage current density measurements showed typical values of about 2×10-7 Acm-2 at 1×106 Vcm-1. The midgap density of interface states was Dit = 5×1011 eV-1cm- 2. Due to annealing the leakage current density and the density of interface states were lowered to 10-7 A/cm-2 and to 1010 eV-1cm-2, respectively. However, the dielectric constant also decreased.
doi_str_mv 10.1149/1.2408905
format Conference Proceeding
fullrecord <record><control><sourceid>crossref</sourceid><recordid>TN_cdi_crossref_primary_10_1149_1_2408905</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_1149_1_2408905</sourcerecordid><originalsourceid>FETCH-LOGICAL-c144t-a3ef587e7e88746f31f2c189713f8d117e20dc64803c2304933994cfccff6dc23</originalsourceid><addsrcrecordid>eNotkMFKxDAURYMoOI4u_INsXXTMa9ImWQ6jjgMDI1g3bkpJXzTSpiVpQf_eVrt6l3MPb3EJuQW2ARD6HjapYEqz7IysQHOV5JLL8yVnKk8vyVWMX4zlky5XpC0-kR68bUb0Bmln6TCBB-y76AbXeVr5mm69x6px_oMW2PYYqmEMGOnUzvLrEEYzkz_3JXSTMbi5t_TdBdN5N7b09O1qvCYXtmoi3ix3Td6eHovdc3I87Q-77TExIMSQVBxtpiRKVEqK3HKwqQGlJXCragCJKatNLhTjJuVMaM61FsYaY21eT2hN7v7_mtDFGNCWfXBtFX5KYOW8UwnlshP_BQFUW1I</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>conference_proceeding</recordtype></control><display><type>conference_proceeding</type><title>The Influence of the Deposition and Annealing Temperatures on the Structure and Properties of Zirconium Oxide</title><source>IOP Publishing Journals</source><source>Institute of Physics (IOP) Journals - HEAL-Link</source><creator>Lisker, Marco ; Silinskas, Mindaugas ; Matichyn, Serhiy ; Burte, Edmund</creator><creatorcontrib>Lisker, Marco ; Silinskas, Mindaugas ; Matichyn, Serhiy ; Burte, Edmund</creatorcontrib><description>ZrO2 thin films were deposited by atomic vapor deposition (AVD) using Zr[OC(CH3)3]4 as precursor. The maximum growth rate (~7 nm/min) and the strongest crystalline phase with preferential tetragonal/cubic orientation were obtained at 400{degree sign} C. Growth rate and crystallinity dropped down with increasing or decreasing deposition temperature. Additionally, the increase of the deposition temperature changed the crystalline ZrO2 phase from cubic/tetragonal to monoclinic. Annealing reduced the cubic/tetragonal phase and enhanced the monoclinic one. The values of the dielectric constant (up to 32) varied depending on the deposition temperature, film thickness, and annealing temperature. Leakage current density measurements showed typical values of about 2×10-7 Acm-2 at 1×106 Vcm-1. The midgap density of interface states was Dit = 5×1011 eV-1cm- 2. Due to annealing the leakage current density and the density of interface states were lowered to 10-7 A/cm-2 and to 1010 eV-1cm-2, respectively. However, the dielectric constant also decreased.</description><identifier>ISSN: 1938-5862</identifier><identifier>EISSN: 1938-6737</identifier><identifier>DOI: 10.1149/1.2408905</identifier><language>eng</language><ispartof>ECS transactions, 2007, Vol.2 (7), p.79-88</ispartof><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c144t-a3ef587e7e88746f31f2c189713f8d117e20dc64803c2304933994cfccff6dc23</citedby></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27922,27923</link.rule.ids></links><search><creatorcontrib>Lisker, Marco</creatorcontrib><creatorcontrib>Silinskas, Mindaugas</creatorcontrib><creatorcontrib>Matichyn, Serhiy</creatorcontrib><creatorcontrib>Burte, Edmund</creatorcontrib><title>The Influence of the Deposition and Annealing Temperatures on the Structure and Properties of Zirconium Oxide</title><title>ECS transactions</title><description>ZrO2 thin films were deposited by atomic vapor deposition (AVD) using Zr[OC(CH3)3]4 as precursor. The maximum growth rate (~7 nm/min) and the strongest crystalline phase with preferential tetragonal/cubic orientation were obtained at 400{degree sign} C. Growth rate and crystallinity dropped down with increasing or decreasing deposition temperature. Additionally, the increase of the deposition temperature changed the crystalline ZrO2 phase from cubic/tetragonal to monoclinic. Annealing reduced the cubic/tetragonal phase and enhanced the monoclinic one. The values of the dielectric constant (up to 32) varied depending on the deposition temperature, film thickness, and annealing temperature. Leakage current density measurements showed typical values of about 2×10-7 Acm-2 at 1×106 Vcm-1. The midgap density of interface states was Dit = 5×1011 eV-1cm- 2. Due to annealing the leakage current density and the density of interface states were lowered to 10-7 A/cm-2 and to 1010 eV-1cm-2, respectively. However, the dielectric constant also decreased.</description><issn>1938-5862</issn><issn>1938-6737</issn><fulltext>true</fulltext><rsrctype>conference_proceeding</rsrctype><creationdate>2007</creationdate><recordtype>conference_proceeding</recordtype><recordid>eNotkMFKxDAURYMoOI4u_INsXXTMa9ImWQ6jjgMDI1g3bkpJXzTSpiVpQf_eVrt6l3MPb3EJuQW2ARD6HjapYEqz7IysQHOV5JLL8yVnKk8vyVWMX4zlky5XpC0-kR68bUb0Bmln6TCBB-y76AbXeVr5mm69x6px_oMW2PYYqmEMGOnUzvLrEEYzkz_3JXSTMbi5t_TdBdN5N7b09O1qvCYXtmoi3ix3Td6eHovdc3I87Q-77TExIMSQVBxtpiRKVEqK3HKwqQGlJXCragCJKatNLhTjJuVMaM61FsYaY21eT2hN7v7_mtDFGNCWfXBtFX5KYOW8UwnlshP_BQFUW1I</recordid><startdate>20070207</startdate><enddate>20070207</enddate><creator>Lisker, Marco</creator><creator>Silinskas, Mindaugas</creator><creator>Matichyn, Serhiy</creator><creator>Burte, Edmund</creator><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20070207</creationdate><title>The Influence of the Deposition and Annealing Temperatures on the Structure and Properties of Zirconium Oxide</title><author>Lisker, Marco ; Silinskas, Mindaugas ; Matichyn, Serhiy ; Burte, Edmund</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c144t-a3ef587e7e88746f31f2c189713f8d117e20dc64803c2304933994cfccff6dc23</frbrgroupid><rsrctype>conference_proceedings</rsrctype><prefilter>conference_proceedings</prefilter><language>eng</language><creationdate>2007</creationdate><toplevel>online_resources</toplevel><creatorcontrib>Lisker, Marco</creatorcontrib><creatorcontrib>Silinskas, Mindaugas</creatorcontrib><creatorcontrib>Matichyn, Serhiy</creatorcontrib><creatorcontrib>Burte, Edmund</creatorcontrib><collection>CrossRef</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Lisker, Marco</au><au>Silinskas, Mindaugas</au><au>Matichyn, Serhiy</au><au>Burte, Edmund</au><format>book</format><genre>proceeding</genre><ristype>CONF</ristype><atitle>The Influence of the Deposition and Annealing Temperatures on the Structure and Properties of Zirconium Oxide</atitle><btitle>ECS transactions</btitle><date>2007-02-07</date><risdate>2007</risdate><volume>2</volume><issue>7</issue><spage>79</spage><epage>88</epage><pages>79-88</pages><issn>1938-5862</issn><eissn>1938-6737</eissn><abstract>ZrO2 thin films were deposited by atomic vapor deposition (AVD) using Zr[OC(CH3)3]4 as precursor. The maximum growth rate (~7 nm/min) and the strongest crystalline phase with preferential tetragonal/cubic orientation were obtained at 400{degree sign} C. Growth rate and crystallinity dropped down with increasing or decreasing deposition temperature. Additionally, the increase of the deposition temperature changed the crystalline ZrO2 phase from cubic/tetragonal to monoclinic. Annealing reduced the cubic/tetragonal phase and enhanced the monoclinic one. The values of the dielectric constant (up to 32) varied depending on the deposition temperature, film thickness, and annealing temperature. Leakage current density measurements showed typical values of about 2×10-7 Acm-2 at 1×106 Vcm-1. The midgap density of interface states was Dit = 5×1011 eV-1cm- 2. Due to annealing the leakage current density and the density of interface states were lowered to 10-7 A/cm-2 and to 1010 eV-1cm-2, respectively. However, the dielectric constant also decreased.</abstract><doi>10.1149/1.2408905</doi><tpages>10</tpages></addata></record>
fulltext fulltext
identifier ISSN: 1938-5862
ispartof ECS transactions, 2007, Vol.2 (7), p.79-88
issn 1938-5862
1938-6737
language eng
recordid cdi_crossref_primary_10_1149_1_2408905
source IOP Publishing Journals; Institute of Physics (IOP) Journals - HEAL-Link
title The Influence of the Deposition and Annealing Temperatures on the Structure and Properties of Zirconium Oxide
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-10T07%3A35%3A06IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-crossref&rft_val_fmt=info:ofi/fmt:kev:mtx:book&rft.genre=proceeding&rft.atitle=The%20Influence%20of%20the%20Deposition%20and%20Annealing%20Temperatures%20on%20the%20Structure%20and%20Properties%20of%20Zirconium%20Oxide&rft.btitle=ECS%20transactions&rft.au=Lisker,%20Marco&rft.date=2007-02-07&rft.volume=2&rft.issue=7&rft.spage=79&rft.epage=88&rft.pages=79-88&rft.issn=1938-5862&rft.eissn=1938-6737&rft_id=info:doi/10.1149/1.2408905&rft_dat=%3Ccrossref%3E10_1149_1_2408905%3C/crossref%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true