Relationship between oxide density and charge trapping in SiO2 films

Spectroscopic ellipsometry was used to determine the density of oxides thermally grown on Si substrates as a function of the oxidation temperature, and the time and temperature of postoxidation anneals. All the oxides were found to be denser than fused silica. The density of the as-grown oxides was...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of applied physics 1999-05, Vol.85 (9), p.6577-6588
Hauptverfasser: Mrstik, B. J., Afanas’ev, V. V., Stesmans, A., McMarr, P. J., Lawrence, R. K.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 6588
container_issue 9
container_start_page 6577
container_title Journal of applied physics
container_volume 85
creator Mrstik, B. J.
Afanas’ev, V. V.
Stesmans, A.
McMarr, P. J.
Lawrence, R. K.
description Spectroscopic ellipsometry was used to determine the density of oxides thermally grown on Si substrates as a function of the oxidation temperature, and the time and temperature of postoxidation anneals. All the oxides were found to be denser than fused silica. The density of the as-grown oxides was found to decrease as the growth temperature was increased. Postoxidation anneals were found to reduce the oxide density; high temperature or long-time anneals caused the greatest reduction in density. Holes alone, or holes and electrons, were injected into the oxides by irradiating with vacuum ultraviolet light or x rays under electric field bias. Using capacitance–voltage measurements, it was found that low-density oxides trap charge more efficiently than high-density oxides. Electron spin resonance measurements indicated that, for most of these oxides, the number of paramagnetic defects was substantially smaller than the number of trapped charges. It is hypothesized that the additional, nonparamagnetic, charge is in the form of protons trapped near network oxygen atoms that have large Si–O–Si bond angles. The number of these large-angle bonds in the near-interfacial oxide increases as the oxide density decreases, explaining the observed correlation between the charge trapping and the oxide density.
doi_str_mv 10.1063/1.370164
format Article
fullrecord <record><control><sourceid>crossref</sourceid><recordid>TN_cdi_crossref_primary_10_1063_1_370164</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_1063_1_370164</sourcerecordid><originalsourceid>FETCH-LOGICAL-c225t-1f3732b1297cfc7d9e3da7a209411e31f5f150d2d3694fb0696a79c8f94a96f53</originalsourceid><addsrcrecordid>eNotz01LwzAYwPEgCtYp-BFy9NL5PEmTNEeZOoXBwJdzSfOyRbq0JAXdtxeZp__tDz9CbhGWCJLf45IrQNmckQqh1bUSAs5JBcCwbrXSl-SqlC8AxJbrijy--cHMcUxlHyfa-_nb-0THn-g8dT6VOB-pSY7avck7T-dspimmHY2JvsctoyEOh3JNLoIZir_574J8Pj99rF7qzXb9unrY1JYxMdcYuOKsR6aVDVY57bkzyjDQDaLnGERAAY45LnUTepBaGqVtG3RjtAyCL8jd6WvzWEr2oZtyPJh87BC6P32H3UnPfwHBtUt1</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Relationship between oxide density and charge trapping in SiO2 films</title><source>AIP Journals Complete</source><source>AIP Digital Archive</source><creator>Mrstik, B. J. ; Afanas’ev, V. V. ; Stesmans, A. ; McMarr, P. J. ; Lawrence, R. K.</creator><creatorcontrib>Mrstik, B. J. ; Afanas’ev, V. V. ; Stesmans, A. ; McMarr, P. J. ; Lawrence, R. K.</creatorcontrib><description>Spectroscopic ellipsometry was used to determine the density of oxides thermally grown on Si substrates as a function of the oxidation temperature, and the time and temperature of postoxidation anneals. All the oxides were found to be denser than fused silica. The density of the as-grown oxides was found to decrease as the growth temperature was increased. Postoxidation anneals were found to reduce the oxide density; high temperature or long-time anneals caused the greatest reduction in density. Holes alone, or holes and electrons, were injected into the oxides by irradiating with vacuum ultraviolet light or x rays under electric field bias. Using capacitance–voltage measurements, it was found that low-density oxides trap charge more efficiently than high-density oxides. Electron spin resonance measurements indicated that, for most of these oxides, the number of paramagnetic defects was substantially smaller than the number of trapped charges. It is hypothesized that the additional, nonparamagnetic, charge is in the form of protons trapped near network oxygen atoms that have large Si–O–Si bond angles. The number of these large-angle bonds in the near-interfacial oxide increases as the oxide density decreases, explaining the observed correlation between the charge trapping and the oxide density.</description><identifier>ISSN: 0021-8979</identifier><identifier>EISSN: 1089-7550</identifier><identifier>DOI: 10.1063/1.370164</identifier><language>eng</language><ispartof>Journal of applied physics, 1999-05, Vol.85 (9), p.6577-6588</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c225t-1f3732b1297cfc7d9e3da7a209411e31f5f150d2d3694fb0696a79c8f94a96f53</citedby><cites>FETCH-LOGICAL-c225t-1f3732b1297cfc7d9e3da7a209411e31f5f150d2d3694fb0696a79c8f94a96f53</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>315,781,785,27929,27930</link.rule.ids></links><search><creatorcontrib>Mrstik, B. J.</creatorcontrib><creatorcontrib>Afanas’ev, V. V.</creatorcontrib><creatorcontrib>Stesmans, A.</creatorcontrib><creatorcontrib>McMarr, P. J.</creatorcontrib><creatorcontrib>Lawrence, R. K.</creatorcontrib><title>Relationship between oxide density and charge trapping in SiO2 films</title><title>Journal of applied physics</title><description>Spectroscopic ellipsometry was used to determine the density of oxides thermally grown on Si substrates as a function of the oxidation temperature, and the time and temperature of postoxidation anneals. All the oxides were found to be denser than fused silica. The density of the as-grown oxides was found to decrease as the growth temperature was increased. Postoxidation anneals were found to reduce the oxide density; high temperature or long-time anneals caused the greatest reduction in density. Holes alone, or holes and electrons, were injected into the oxides by irradiating with vacuum ultraviolet light or x rays under electric field bias. Using capacitance–voltage measurements, it was found that low-density oxides trap charge more efficiently than high-density oxides. Electron spin resonance measurements indicated that, for most of these oxides, the number of paramagnetic defects was substantially smaller than the number of trapped charges. It is hypothesized that the additional, nonparamagnetic, charge is in the form of protons trapped near network oxygen atoms that have large Si–O–Si bond angles. The number of these large-angle bonds in the near-interfacial oxide increases as the oxide density decreases, explaining the observed correlation between the charge trapping and the oxide density.</description><issn>0021-8979</issn><issn>1089-7550</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1999</creationdate><recordtype>article</recordtype><recordid>eNotz01LwzAYwPEgCtYp-BFy9NL5PEmTNEeZOoXBwJdzSfOyRbq0JAXdtxeZp__tDz9CbhGWCJLf45IrQNmckQqh1bUSAs5JBcCwbrXSl-SqlC8AxJbrijy--cHMcUxlHyfa-_nb-0THn-g8dT6VOB-pSY7avck7T-dspimmHY2JvsctoyEOh3JNLoIZir_574J8Pj99rF7qzXb9unrY1JYxMdcYuOKsR6aVDVY57bkzyjDQDaLnGERAAY45LnUTepBaGqVtG3RjtAyCL8jd6WvzWEr2oZtyPJh87BC6P32H3UnPfwHBtUt1</recordid><startdate>19990501</startdate><enddate>19990501</enddate><creator>Mrstik, B. J.</creator><creator>Afanas’ev, V. V.</creator><creator>Stesmans, A.</creator><creator>McMarr, P. J.</creator><creator>Lawrence, R. K.</creator><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>19990501</creationdate><title>Relationship between oxide density and charge trapping in SiO2 films</title><author>Mrstik, B. J. ; Afanas’ev, V. V. ; Stesmans, A. ; McMarr, P. J. ; Lawrence, R. K.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c225t-1f3732b1297cfc7d9e3da7a209411e31f5f150d2d3694fb0696a79c8f94a96f53</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1999</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Mrstik, B. J.</creatorcontrib><creatorcontrib>Afanas’ev, V. V.</creatorcontrib><creatorcontrib>Stesmans, A.</creatorcontrib><creatorcontrib>McMarr, P. J.</creatorcontrib><creatorcontrib>Lawrence, R. K.</creatorcontrib><collection>CrossRef</collection><jtitle>Journal of applied physics</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Mrstik, B. J.</au><au>Afanas’ev, V. V.</au><au>Stesmans, A.</au><au>McMarr, P. J.</au><au>Lawrence, R. K.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Relationship between oxide density and charge trapping in SiO2 films</atitle><jtitle>Journal of applied physics</jtitle><date>1999-05-01</date><risdate>1999</risdate><volume>85</volume><issue>9</issue><spage>6577</spage><epage>6588</epage><pages>6577-6588</pages><issn>0021-8979</issn><eissn>1089-7550</eissn><abstract>Spectroscopic ellipsometry was used to determine the density of oxides thermally grown on Si substrates as a function of the oxidation temperature, and the time and temperature of postoxidation anneals. All the oxides were found to be denser than fused silica. The density of the as-grown oxides was found to decrease as the growth temperature was increased. Postoxidation anneals were found to reduce the oxide density; high temperature or long-time anneals caused the greatest reduction in density. Holes alone, or holes and electrons, were injected into the oxides by irradiating with vacuum ultraviolet light or x rays under electric field bias. Using capacitance–voltage measurements, it was found that low-density oxides trap charge more efficiently than high-density oxides. Electron spin resonance measurements indicated that, for most of these oxides, the number of paramagnetic defects was substantially smaller than the number of trapped charges. It is hypothesized that the additional, nonparamagnetic, charge is in the form of protons trapped near network oxygen atoms that have large Si–O–Si bond angles. The number of these large-angle bonds in the near-interfacial oxide increases as the oxide density decreases, explaining the observed correlation between the charge trapping and the oxide density.</abstract><doi>10.1063/1.370164</doi><tpages>12</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0021-8979
ispartof Journal of applied physics, 1999-05, Vol.85 (9), p.6577-6588
issn 0021-8979
1089-7550
language eng
recordid cdi_crossref_primary_10_1063_1_370164
source AIP Journals Complete; AIP Digital Archive
title Relationship between oxide density and charge trapping in SiO2 films
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-16T00%3A52%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-crossref&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Relationship%20between%20oxide%20density%20and%20charge%20trapping%20in%20SiO2%20films&rft.jtitle=Journal%20of%20applied%20physics&rft.au=Mrstik,%20B.%20J.&rft.date=1999-05-01&rft.volume=85&rft.issue=9&rft.spage=6577&rft.epage=6588&rft.pages=6577-6588&rft.issn=0021-8979&rft.eissn=1089-7550&rft_id=info:doi/10.1063/1.370164&rft_dat=%3Ccrossref%3E10_1063_1_370164%3C/crossref%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true