Origin of high piezoelectric activity in ferroelectric (K0.44Na0.52Li0.04)−(Nb0.84Ta0.1Sb0.06)O3 ceramics

We study the temperature dependence of dielectric constant (K) and spontaneous polarization (Ps) in the range of −95–200°C. Cubic (C)-tetragonal (T) and T-orthorhombic (O) transitions are observed at 264 and 25°C, respectively. The Curie–Weiss temperature of C-T transition is 249°C, indicating it is...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied physics letters 2008-03, Vol.92 (11)
Hauptverfasser: Akdoğan, E. K., Kerman, K., Abazari, M., Safari, A.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:We study the temperature dependence of dielectric constant (K) and spontaneous polarization (Ps) in the range of −95–200°C. Cubic (C)-tetragonal (T) and T-orthorhombic (O) transitions are observed at 264 and 25°C, respectively. The Curie–Weiss temperature of C-T transition is 249°C, indicating it is first order. X-ray data indicate T-O phase coexistence at 25°C. A singularity in Ps at 25°C and a T-O phase coexistence spanning 25–31°C was observed, wherein Ps increases from 17×10−2C∕m2 at 31°Cto23×10−2C∕m2 25°C. The transition at 25°C appears diffusionless and polymorphic with martensite start and finish temperatures of 31 and 25°C, respectively. The maximum in d33 is 345pC∕N and is attributed to the instability at 25°C, where Ps and K show singularity.