Effect of texture on dielectric properties and thermal depoling of Bi4Ti3O12 ferroelectric ceramics

Ordinary fired Bi4Ti3O12 ceramics show a gradual reduction in their room temperature d33 after annealing at temperatures from room temperature to 450°C. Textured ceramics show a greater resistance to thermal depoling. At about 450°C there is a rapid drop of d33 for the textured materials, which may...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of applied physics 2006-10, Vol.100 (7)
Hauptverfasser: Yan, Haixue, Reece, Michael J., Liu, Jing, Shen, Zhijian, Kan, Yanmei, Wang, Peiling
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue 7
container_start_page
container_title Journal of applied physics
container_volume 100
creator Yan, Haixue
Reece, Michael J.
Liu, Jing
Shen, Zhijian
Kan, Yanmei
Wang, Peiling
description Ordinary fired Bi4Ti3O12 ceramics show a gradual reduction in their room temperature d33 after annealing at temperatures from room temperature to 450°C. Textured ceramics show a greater resistance to thermal depoling. At about 450°C there is a rapid drop of d33 for the textured materials, which may be a consequence of a phase transition. Between 500 and 650°C the d33 is stable. The depolarization is assisted by internal mechanical stresses. These stresses are smaller in textured materials, which explains the increasing resistance to thermal depoling with increasing texture.
doi_str_mv 10.1063/1.2356092
format Article
fullrecord <record><control><sourceid>crossref</sourceid><recordid>TN_cdi_crossref_primary_10_1063_1_2356092</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_1063_1_2356092</sourcerecordid><originalsourceid>FETCH-LOGICAL-c225t-ce0d2502eb4636bad60e63561ef0911b71fcdb2959361a3fa9f4709deec95b753</originalsourceid><addsrcrecordid>eNo9kE1LxDAURYMoWEcX_oNsXXR8L2nSZqnD-AEDsxnXJU1eNNJpS1JB_70zOLi6cOFcuIexW4Qlgpb3uBRSaTDijBUIjSlrpeCcFQACy8bU5pJd5fwJgNhIUzC3DoHczMfAZ_qevxLxceA-Un9oU3R8SuNEaY6UuR08nz8o7W3PPU1jH4f3I_gYq12UWxQ8UErjP-oo2X10-ZpdBNtnujnlgr09rXerl3KzfX5dPWxKJ4SaS0fghQJBXaWl7qzXQPpwBimAQexqDM53wigjNVoZrAlVDcYTOaO6WskFu_vbdWnMOVFopxT3Nv20CO3RTovtyY78Bd-4V6Q</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Effect of texture on dielectric properties and thermal depoling of Bi4Ti3O12 ferroelectric ceramics</title><source>AIP Journals Complete</source><source>AIP Digital Archive</source><creator>Yan, Haixue ; Reece, Michael J. ; Liu, Jing ; Shen, Zhijian ; Kan, Yanmei ; Wang, Peiling</creator><creatorcontrib>Yan, Haixue ; Reece, Michael J. ; Liu, Jing ; Shen, Zhijian ; Kan, Yanmei ; Wang, Peiling</creatorcontrib><description>Ordinary fired Bi4Ti3O12 ceramics show a gradual reduction in their room temperature d33 after annealing at temperatures from room temperature to 450°C. Textured ceramics show a greater resistance to thermal depoling. At about 450°C there is a rapid drop of d33 for the textured materials, which may be a consequence of a phase transition. Between 500 and 650°C the d33 is stable. The depolarization is assisted by internal mechanical stresses. These stresses are smaller in textured materials, which explains the increasing resistance to thermal depoling with increasing texture.</description><identifier>ISSN: 0021-8979</identifier><identifier>EISSN: 1089-7550</identifier><identifier>DOI: 10.1063/1.2356092</identifier><language>eng</language><ispartof>Journal of applied physics, 2006-10, Vol.100 (7)</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c225t-ce0d2502eb4636bad60e63561ef0911b71fcdb2959361a3fa9f4709deec95b753</citedby><cites>FETCH-LOGICAL-c225t-ce0d2502eb4636bad60e63561ef0911b71fcdb2959361a3fa9f4709deec95b753</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27923,27924</link.rule.ids></links><search><creatorcontrib>Yan, Haixue</creatorcontrib><creatorcontrib>Reece, Michael J.</creatorcontrib><creatorcontrib>Liu, Jing</creatorcontrib><creatorcontrib>Shen, Zhijian</creatorcontrib><creatorcontrib>Kan, Yanmei</creatorcontrib><creatorcontrib>Wang, Peiling</creatorcontrib><title>Effect of texture on dielectric properties and thermal depoling of Bi4Ti3O12 ferroelectric ceramics</title><title>Journal of applied physics</title><description>Ordinary fired Bi4Ti3O12 ceramics show a gradual reduction in their room temperature d33 after annealing at temperatures from room temperature to 450°C. Textured ceramics show a greater resistance to thermal depoling. At about 450°C there is a rapid drop of d33 for the textured materials, which may be a consequence of a phase transition. Between 500 and 650°C the d33 is stable. The depolarization is assisted by internal mechanical stresses. These stresses are smaller in textured materials, which explains the increasing resistance to thermal depoling with increasing texture.</description><issn>0021-8979</issn><issn>1089-7550</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2006</creationdate><recordtype>article</recordtype><recordid>eNo9kE1LxDAURYMoWEcX_oNsXXR8L2nSZqnD-AEDsxnXJU1eNNJpS1JB_70zOLi6cOFcuIexW4Qlgpb3uBRSaTDijBUIjSlrpeCcFQACy8bU5pJd5fwJgNhIUzC3DoHczMfAZ_qevxLxceA-Un9oU3R8SuNEaY6UuR08nz8o7W3PPU1jH4f3I_gYq12UWxQ8UErjP-oo2X10-ZpdBNtnujnlgr09rXerl3KzfX5dPWxKJ4SaS0fghQJBXaWl7qzXQPpwBimAQexqDM53wigjNVoZrAlVDcYTOaO6WskFu_vbdWnMOVFopxT3Nv20CO3RTovtyY78Bd-4V6Q</recordid><startdate>20061001</startdate><enddate>20061001</enddate><creator>Yan, Haixue</creator><creator>Reece, Michael J.</creator><creator>Liu, Jing</creator><creator>Shen, Zhijian</creator><creator>Kan, Yanmei</creator><creator>Wang, Peiling</creator><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20061001</creationdate><title>Effect of texture on dielectric properties and thermal depoling of Bi4Ti3O12 ferroelectric ceramics</title><author>Yan, Haixue ; Reece, Michael J. ; Liu, Jing ; Shen, Zhijian ; Kan, Yanmei ; Wang, Peiling</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c225t-ce0d2502eb4636bad60e63561ef0911b71fcdb2959361a3fa9f4709deec95b753</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2006</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Yan, Haixue</creatorcontrib><creatorcontrib>Reece, Michael J.</creatorcontrib><creatorcontrib>Liu, Jing</creatorcontrib><creatorcontrib>Shen, Zhijian</creatorcontrib><creatorcontrib>Kan, Yanmei</creatorcontrib><creatorcontrib>Wang, Peiling</creatorcontrib><collection>CrossRef</collection><jtitle>Journal of applied physics</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Yan, Haixue</au><au>Reece, Michael J.</au><au>Liu, Jing</au><au>Shen, Zhijian</au><au>Kan, Yanmei</au><au>Wang, Peiling</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effect of texture on dielectric properties and thermal depoling of Bi4Ti3O12 ferroelectric ceramics</atitle><jtitle>Journal of applied physics</jtitle><date>2006-10-01</date><risdate>2006</risdate><volume>100</volume><issue>7</issue><issn>0021-8979</issn><eissn>1089-7550</eissn><abstract>Ordinary fired Bi4Ti3O12 ceramics show a gradual reduction in their room temperature d33 after annealing at temperatures from room temperature to 450°C. Textured ceramics show a greater resistance to thermal depoling. At about 450°C there is a rapid drop of d33 for the textured materials, which may be a consequence of a phase transition. Between 500 and 650°C the d33 is stable. The depolarization is assisted by internal mechanical stresses. These stresses are smaller in textured materials, which explains the increasing resistance to thermal depoling with increasing texture.</abstract><doi>10.1063/1.2356092</doi></addata></record>
fulltext fulltext
identifier ISSN: 0021-8979
ispartof Journal of applied physics, 2006-10, Vol.100 (7)
issn 0021-8979
1089-7550
language eng
recordid cdi_crossref_primary_10_1063_1_2356092
source AIP Journals Complete; AIP Digital Archive
title Effect of texture on dielectric properties and thermal depoling of Bi4Ti3O12 ferroelectric ceramics
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-09T07%3A59%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-crossref&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effect%20of%20texture%20on%20dielectric%20properties%20and%20thermal%20depoling%20of%20Bi4Ti3O12%20ferroelectric%20ceramics&rft.jtitle=Journal%20of%20applied%20physics&rft.au=Yan,%20Haixue&rft.date=2006-10-01&rft.volume=100&rft.issue=7&rft.issn=0021-8979&rft.eissn=1089-7550&rft_id=info:doi/10.1063/1.2356092&rft_dat=%3Ccrossref%3E10_1063_1_2356092%3C/crossref%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true