Glass-forming ability and soft magnetic properties of FeCoSiAlGaPCB amorphous alloys
The glass-forming ability of (FexCoyBzCu)80Si3Al5Ga2P10 with x=5–70, y=0–63, z=5–12, and u=0–5 amorphous alloys has been analyzed in terms of the width of the supercooled liquid region, the reduced glass transition temperature, and the Vogel–Fulcher–Tammann parameters. Substitution of Fe by Co sligh...
Gespeichert in:
Veröffentlicht in: | Journal of applied physics 2002-08, Vol.92 (4), p.2073-2078 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 2078 |
---|---|
container_issue | 4 |
container_start_page | 2073 |
container_title | Journal of applied physics |
container_volume | 92 |
creator | Borrego, J. M. Conde, A. Roth, S. Eckert, J. |
description | The glass-forming ability of (FexCoyBzCu)80Si3Al5Ga2P10 with x=5–70, y=0–63, z=5–12, and u=0–5 amorphous alloys has been analyzed in terms of the width of the supercooled liquid region, the reduced glass transition temperature, and the Vogel–Fulcher–Tammann parameters. Substitution of Fe by Co slightly decreases the glass-forming ability of the studied alloys. The value of the fragility parameter m is discussed in the frame of the general classification scheme of glass-forming liquids. The crystalline phases formed during the first crystallization step are identified. Magnetic moment at low and room temperature, Curie temperature, room temperature magnetostriction, and coercivity decrease with increasing Co content. |
doi_str_mv | 10.1063/1.1494848 |
format | Article |
fullrecord | <record><control><sourceid>crossref</sourceid><recordid>TN_cdi_crossref_primary_10_1063_1_1494848</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_1063_1_1494848</sourcerecordid><originalsourceid>FETCH-LOGICAL-c328t-c37b77f668abb528cd169f8fa4660d91cea8049c4603818632a614e56809b3ae3</originalsourceid><addsrcrecordid>eNotkLFOwzAUAC0EEqEw8AdeGVL8Ysd5HktEA1IlkChz9JLaxSipIzsM_XtA7XK33XCM3YNYgtDyEZagjEKFFywDgSavylJcskyIAnI0lblmNyl9CwGA0mRs2wyUUu5CHP1hz6nzg5-PnA47noKb-Uj7g519z6cYJhtnbxMPjq9tHT78amjovX7iNIY4fYWfxGkYwjHdsitHQ7J3Zy_Y5_p5W7_km7fmtV5t8l4WOP-x6qrKaY3UdWWB_Q60cehIaS12BnpLKJTplRYSAbUsSIOypUZhOklWLtjDqdvHkFK0rp2iHykeWxDt_44W2vMO-Qsnx1HL</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Glass-forming ability and soft magnetic properties of FeCoSiAlGaPCB amorphous alloys</title><source>AIP Journals Complete</source><source>AIP Digital Archive</source><creator>Borrego, J. M. ; Conde, A. ; Roth, S. ; Eckert, J.</creator><creatorcontrib>Borrego, J. M. ; Conde, A. ; Roth, S. ; Eckert, J.</creatorcontrib><description>The glass-forming ability of (FexCoyBzCu)80Si3Al5Ga2P10 with x=5–70, y=0–63, z=5–12, and u=0–5 amorphous alloys has been analyzed in terms of the width of the supercooled liquid region, the reduced glass transition temperature, and the Vogel–Fulcher–Tammann parameters. Substitution of Fe by Co slightly decreases the glass-forming ability of the studied alloys. The value of the fragility parameter m is discussed in the frame of the general classification scheme of glass-forming liquids. The crystalline phases formed during the first crystallization step are identified. Magnetic moment at low and room temperature, Curie temperature, room temperature magnetostriction, and coercivity decrease with increasing Co content.</description><identifier>ISSN: 0021-8979</identifier><identifier>EISSN: 1089-7550</identifier><identifier>DOI: 10.1063/1.1494848</identifier><language>eng</language><ispartof>Journal of applied physics, 2002-08, Vol.92 (4), p.2073-2078</ispartof><lds50>peer_reviewed</lds50><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c328t-c37b77f668abb528cd169f8fa4660d91cea8049c4603818632a614e56809b3ae3</citedby><cites>FETCH-LOGICAL-c328t-c37b77f668abb528cd169f8fa4660d91cea8049c4603818632a614e56809b3ae3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,777,781,27905,27906</link.rule.ids></links><search><creatorcontrib>Borrego, J. M.</creatorcontrib><creatorcontrib>Conde, A.</creatorcontrib><creatorcontrib>Roth, S.</creatorcontrib><creatorcontrib>Eckert, J.</creatorcontrib><title>Glass-forming ability and soft magnetic properties of FeCoSiAlGaPCB amorphous alloys</title><title>Journal of applied physics</title><description>The glass-forming ability of (FexCoyBzCu)80Si3Al5Ga2P10 with x=5–70, y=0–63, z=5–12, and u=0–5 amorphous alloys has been analyzed in terms of the width of the supercooled liquid region, the reduced glass transition temperature, and the Vogel–Fulcher–Tammann parameters. Substitution of Fe by Co slightly decreases the glass-forming ability of the studied alloys. The value of the fragility parameter m is discussed in the frame of the general classification scheme of glass-forming liquids. The crystalline phases formed during the first crystallization step are identified. Magnetic moment at low and room temperature, Curie temperature, room temperature magnetostriction, and coercivity decrease with increasing Co content.</description><issn>0021-8979</issn><issn>1089-7550</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2002</creationdate><recordtype>article</recordtype><recordid>eNotkLFOwzAUAC0EEqEw8AdeGVL8Ysd5HktEA1IlkChz9JLaxSipIzsM_XtA7XK33XCM3YNYgtDyEZagjEKFFywDgSavylJcskyIAnI0lblmNyl9CwGA0mRs2wyUUu5CHP1hz6nzg5-PnA47noKb-Uj7g519z6cYJhtnbxMPjq9tHT78amjovX7iNIY4fYWfxGkYwjHdsitHQ7J3Zy_Y5_p5W7_km7fmtV5t8l4WOP-x6qrKaY3UdWWB_Q60cehIaS12BnpLKJTplRYSAbUsSIOypUZhOklWLtjDqdvHkFK0rp2iHykeWxDt_44W2vMO-Qsnx1HL</recordid><startdate>20020815</startdate><enddate>20020815</enddate><creator>Borrego, J. M.</creator><creator>Conde, A.</creator><creator>Roth, S.</creator><creator>Eckert, J.</creator><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20020815</creationdate><title>Glass-forming ability and soft magnetic properties of FeCoSiAlGaPCB amorphous alloys</title><author>Borrego, J. M. ; Conde, A. ; Roth, S. ; Eckert, J.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c328t-c37b77f668abb528cd169f8fa4660d91cea8049c4603818632a614e56809b3ae3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2002</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Borrego, J. M.</creatorcontrib><creatorcontrib>Conde, A.</creatorcontrib><creatorcontrib>Roth, S.</creatorcontrib><creatorcontrib>Eckert, J.</creatorcontrib><collection>CrossRef</collection><jtitle>Journal of applied physics</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Borrego, J. M.</au><au>Conde, A.</au><au>Roth, S.</au><au>Eckert, J.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Glass-forming ability and soft magnetic properties of FeCoSiAlGaPCB amorphous alloys</atitle><jtitle>Journal of applied physics</jtitle><date>2002-08-15</date><risdate>2002</risdate><volume>92</volume><issue>4</issue><spage>2073</spage><epage>2078</epage><pages>2073-2078</pages><issn>0021-8979</issn><eissn>1089-7550</eissn><abstract>The glass-forming ability of (FexCoyBzCu)80Si3Al5Ga2P10 with x=5–70, y=0–63, z=5–12, and u=0–5 amorphous alloys has been analyzed in terms of the width of the supercooled liquid region, the reduced glass transition temperature, and the Vogel–Fulcher–Tammann parameters. Substitution of Fe by Co slightly decreases the glass-forming ability of the studied alloys. The value of the fragility parameter m is discussed in the frame of the general classification scheme of glass-forming liquids. The crystalline phases formed during the first crystallization step are identified. Magnetic moment at low and room temperature, Curie temperature, room temperature magnetostriction, and coercivity decrease with increasing Co content.</abstract><doi>10.1063/1.1494848</doi><tpages>6</tpages><oa>free_for_read</oa></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0021-8979 |
ispartof | Journal of applied physics, 2002-08, Vol.92 (4), p.2073-2078 |
issn | 0021-8979 1089-7550 |
language | eng |
recordid | cdi_crossref_primary_10_1063_1_1494848 |
source | AIP Journals Complete; AIP Digital Archive |
title | Glass-forming ability and soft magnetic properties of FeCoSiAlGaPCB amorphous alloys |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T05%3A59%3A36IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-crossref&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Glass-forming%20ability%20and%20soft%20magnetic%20properties%20of%20FeCoSiAlGaPCB%20amorphous%20alloys&rft.jtitle=Journal%20of%20applied%20physics&rft.au=Borrego,%20J.%20M.&rft.date=2002-08-15&rft.volume=92&rft.issue=4&rft.spage=2073&rft.epage=2078&rft.pages=2073-2078&rft.issn=0021-8979&rft.eissn=1089-7550&rft_id=info:doi/10.1063/1.1494848&rft_dat=%3Ccrossref%3E10_1063_1_1494848%3C/crossref%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |