Improved Ni based composite Ohmic contact to n -SiC for high temperature and high power device applications

Ni/WSi/Ti/Pt Ohmic contacts to n-SiC were investigated as a function of annealing temperatures up to 1000 °C. Annealing at temperatures between 950 and 1000 °C yielded excellent Ohmic behavior. At these temperatures the contact–SiC interface was smooth, defect free, and characterized by a narrow Ni2...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of applied physics 2000-09, Vol.88 (5), p.2652-2657
Hauptverfasser: Cole, M. W., Joshi, P. C., Hubbard, C. W., Wood, M. C., Ervin, M. H., Geil, B., Ren, F.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 2657
container_issue 5
container_start_page 2652
container_title Journal of applied physics
container_volume 88
creator Cole, M. W.
Joshi, P. C.
Hubbard, C. W.
Wood, M. C.
Ervin, M. H.
Geil, B.
Ren, F.
description Ni/WSi/Ti/Pt Ohmic contacts to n-SiC were investigated as a function of annealing temperatures up to 1000 °C. Annealing at temperatures between 950 and 1000 °C yielded excellent Ohmic behavior. At these temperatures the contact–SiC interface was smooth, defect free, and characterized by a narrow Ni2Si reaction region. The annealed contacts possessed atomically smooth surface morphologies and exhibited minimal contact expansion. The residual carbon, resultant from SiC decompositon and reaction with Ni to form Ni2Si, was constrained by reaction with the WSi and Ti layers forming carbide phases of W and Ti spatially distant from the metal semiconductor interface. Our results demonstrate that the Ni/WSi/Ti/Pt composite Ohmic contact maintains the desirable electrical properties associated with Ni contacts and possesses excellent interfacial, compositional, and surface properties which are required for reliable high power and high temperature device operation.
doi_str_mv 10.1063/1.1287776
format Article
fullrecord <record><control><sourceid>crossref</sourceid><recordid>TN_cdi_crossref_primary_10_1063_1_1287776</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>10_1063_1_1287776</sourcerecordid><originalsourceid>FETCH-LOGICAL-c293t-106b1e7d69b91967eecc2ee3250ab67187314a830fdd82923cc2b591e85fa8913</originalsourceid><addsrcrecordid>eNotULtOwzAUtRBIhMLAH3hlSPG1SWyPqOJRqaIDMEeOc0MMTWzZpoi_J6idzks60jmEXANbAqvFLSyBKyllfUIKYEqXsqrYKSkY41AqLfU5uUjpkzEAJXRBvtZjiH6PHX1xtDVpJtaPwSeXkW6H0dlZT9nYTLOnEy1f3Yr2PtLBfQw04xgwmvwdkZqpO5jB_2CkHe6dnd0Qds6a7PyULslZb3YJr464IO-PD2-r53KzfVqv7jel5Vrkct7RAsqu1q0GXUtEazmi4BUzbS1BSQF3RgnWd53imos5bisNqKreKA1iQW4OvTb6lCL2TYhuNPG3Adb8v9RAc3xJ_AHDq1oK</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Improved Ni based composite Ohmic contact to n -SiC for high temperature and high power device applications</title><source>AIP Journals Complete</source><source>AIP Digital Archive</source><creator>Cole, M. W. ; Joshi, P. C. ; Hubbard, C. W. ; Wood, M. C. ; Ervin, M. H. ; Geil, B. ; Ren, F.</creator><creatorcontrib>Cole, M. W. ; Joshi, P. C. ; Hubbard, C. W. ; Wood, M. C. ; Ervin, M. H. ; Geil, B. ; Ren, F.</creatorcontrib><description>Ni/WSi/Ti/Pt Ohmic contacts to n-SiC were investigated as a function of annealing temperatures up to 1000 °C. Annealing at temperatures between 950 and 1000 °C yielded excellent Ohmic behavior. At these temperatures the contact–SiC interface was smooth, defect free, and characterized by a narrow Ni2Si reaction region. The annealed contacts possessed atomically smooth surface morphologies and exhibited minimal contact expansion. The residual carbon, resultant from SiC decompositon and reaction with Ni to form Ni2Si, was constrained by reaction with the WSi and Ti layers forming carbide phases of W and Ti spatially distant from the metal semiconductor interface. Our results demonstrate that the Ni/WSi/Ti/Pt composite Ohmic contact maintains the desirable electrical properties associated with Ni contacts and possesses excellent interfacial, compositional, and surface properties which are required for reliable high power and high temperature device operation.</description><identifier>ISSN: 0021-8979</identifier><identifier>EISSN: 1089-7550</identifier><identifier>DOI: 10.1063/1.1287776</identifier><language>eng</language><ispartof>Journal of applied physics, 2000-09, Vol.88 (5), p.2652-2657</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c293t-106b1e7d69b91967eecc2ee3250ab67187314a830fdd82923cc2b591e85fa8913</citedby><cites>FETCH-LOGICAL-c293t-106b1e7d69b91967eecc2ee3250ab67187314a830fdd82923cc2b591e85fa8913</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,776,780,27901,27902</link.rule.ids></links><search><creatorcontrib>Cole, M. W.</creatorcontrib><creatorcontrib>Joshi, P. C.</creatorcontrib><creatorcontrib>Hubbard, C. W.</creatorcontrib><creatorcontrib>Wood, M. C.</creatorcontrib><creatorcontrib>Ervin, M. H.</creatorcontrib><creatorcontrib>Geil, B.</creatorcontrib><creatorcontrib>Ren, F.</creatorcontrib><title>Improved Ni based composite Ohmic contact to n -SiC for high temperature and high power device applications</title><title>Journal of applied physics</title><description>Ni/WSi/Ti/Pt Ohmic contacts to n-SiC were investigated as a function of annealing temperatures up to 1000 °C. Annealing at temperatures between 950 and 1000 °C yielded excellent Ohmic behavior. At these temperatures the contact–SiC interface was smooth, defect free, and characterized by a narrow Ni2Si reaction region. The annealed contacts possessed atomically smooth surface morphologies and exhibited minimal contact expansion. The residual carbon, resultant from SiC decompositon and reaction with Ni to form Ni2Si, was constrained by reaction with the WSi and Ti layers forming carbide phases of W and Ti spatially distant from the metal semiconductor interface. Our results demonstrate that the Ni/WSi/Ti/Pt composite Ohmic contact maintains the desirable electrical properties associated with Ni contacts and possesses excellent interfacial, compositional, and surface properties which are required for reliable high power and high temperature device operation.</description><issn>0021-8979</issn><issn>1089-7550</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2000</creationdate><recordtype>article</recordtype><recordid>eNotULtOwzAUtRBIhMLAH3hlSPG1SWyPqOJRqaIDMEeOc0MMTWzZpoi_J6idzks60jmEXANbAqvFLSyBKyllfUIKYEqXsqrYKSkY41AqLfU5uUjpkzEAJXRBvtZjiH6PHX1xtDVpJtaPwSeXkW6H0dlZT9nYTLOnEy1f3Yr2PtLBfQw04xgwmvwdkZqpO5jB_2CkHe6dnd0Qds6a7PyULslZb3YJr464IO-PD2-r53KzfVqv7jel5Vrkct7RAsqu1q0GXUtEazmi4BUzbS1BSQF3RgnWd53imos5bisNqKreKA1iQW4OvTb6lCL2TYhuNPG3Adb8v9RAc3xJ_AHDq1oK</recordid><startdate>20000901</startdate><enddate>20000901</enddate><creator>Cole, M. W.</creator><creator>Joshi, P. C.</creator><creator>Hubbard, C. W.</creator><creator>Wood, M. C.</creator><creator>Ervin, M. H.</creator><creator>Geil, B.</creator><creator>Ren, F.</creator><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>20000901</creationdate><title>Improved Ni based composite Ohmic contact to n -SiC for high temperature and high power device applications</title><author>Cole, M. W. ; Joshi, P. C. ; Hubbard, C. W. ; Wood, M. C. ; Ervin, M. H. ; Geil, B. ; Ren, F.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c293t-106b1e7d69b91967eecc2ee3250ab67187314a830fdd82923cc2b591e85fa8913</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2000</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Cole, M. W.</creatorcontrib><creatorcontrib>Joshi, P. C.</creatorcontrib><creatorcontrib>Hubbard, C. W.</creatorcontrib><creatorcontrib>Wood, M. C.</creatorcontrib><creatorcontrib>Ervin, M. H.</creatorcontrib><creatorcontrib>Geil, B.</creatorcontrib><creatorcontrib>Ren, F.</creatorcontrib><collection>CrossRef</collection><jtitle>Journal of applied physics</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Cole, M. W.</au><au>Joshi, P. C.</au><au>Hubbard, C. W.</au><au>Wood, M. C.</au><au>Ervin, M. H.</au><au>Geil, B.</au><au>Ren, F.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Improved Ni based composite Ohmic contact to n -SiC for high temperature and high power device applications</atitle><jtitle>Journal of applied physics</jtitle><date>2000-09-01</date><risdate>2000</risdate><volume>88</volume><issue>5</issue><spage>2652</spage><epage>2657</epage><pages>2652-2657</pages><issn>0021-8979</issn><eissn>1089-7550</eissn><abstract>Ni/WSi/Ti/Pt Ohmic contacts to n-SiC were investigated as a function of annealing temperatures up to 1000 °C. Annealing at temperatures between 950 and 1000 °C yielded excellent Ohmic behavior. At these temperatures the contact–SiC interface was smooth, defect free, and characterized by a narrow Ni2Si reaction region. The annealed contacts possessed atomically smooth surface morphologies and exhibited minimal contact expansion. The residual carbon, resultant from SiC decompositon and reaction with Ni to form Ni2Si, was constrained by reaction with the WSi and Ti layers forming carbide phases of W and Ti spatially distant from the metal semiconductor interface. Our results demonstrate that the Ni/WSi/Ti/Pt composite Ohmic contact maintains the desirable electrical properties associated with Ni contacts and possesses excellent interfacial, compositional, and surface properties which are required for reliable high power and high temperature device operation.</abstract><doi>10.1063/1.1287776</doi><tpages>6</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0021-8979
ispartof Journal of applied physics, 2000-09, Vol.88 (5), p.2652-2657
issn 0021-8979
1089-7550
language eng
recordid cdi_crossref_primary_10_1063_1_1287776
source AIP Journals Complete; AIP Digital Archive
title Improved Ni based composite Ohmic contact to n -SiC for high temperature and high power device applications
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T08%3A47%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-crossref&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Improved%20Ni%20based%20composite%20Ohmic%20contact%20to%20n%20-SiC%20for%20high%20temperature%20and%20high%20power%20device%20applications&rft.jtitle=Journal%20of%20applied%20physics&rft.au=Cole,%20M.%20W.&rft.date=2000-09-01&rft.volume=88&rft.issue=5&rft.spage=2652&rft.epage=2657&rft.pages=2652-2657&rft.issn=0021-8979&rft.eissn=1089-7550&rft_id=info:doi/10.1063/1.1287776&rft_dat=%3Ccrossref%3E10_1063_1_1287776%3C/crossref%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true