Memory of the magnetic field applied during cooling in the low-temperature phase of magnetite: Grain size dependence
Low‐temperature magnetic hysteresis properties of polycrystalline magnetite samples were studied as a function of the magnetic field (HFC) applied during cooling from 300 K to 10 K. The samples ranged in mean grain size from 0.04 to 100 μm, representing mostly single‐domain (SD), pseudosingle‐domain...