Sol−Gel Replication of Microoptical Elements and Arrays

Facile replication of microoptical elements and arrays was performed in sol−gel matrixes prepared by the fast sol−gel method. These sol−gel resins, made from mixtures of alkylalkoxysilane monomers, undergo hydrolysis and polymerization within 10−20 min and curing within a few days. Single-step repro...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Chemistry of materials 1997-11, Vol.9 (11), p.2604-2615
Hauptverfasser: Haruvy, Y, Gilath, I, Maniewictz, M, Eisenberg, N
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 2615
container_issue 11
container_start_page 2604
container_title Chemistry of materials
container_volume 9
creator Haruvy, Y
Gilath, I
Maniewictz, M
Eisenberg, N
description Facile replication of microoptical elements and arrays was performed in sol−gel matrixes prepared by the fast sol−gel method. These sol−gel resins, made from mixtures of alkylalkoxysilane monomers, undergo hydrolysis and polymerization within 10−20 min and curing within a few days. Single-step reproducible fabrication of large crack-free elements of 1 cm thickness and up to 10 cm in diameter was demonstrated. High accuracy of replication was facilitated by maintaining a very small shrinkage of only a few percent during the curing stage. This was attained by removing most of the volatile products from the sol, without gelling, prior to casting it onto the template. Accurate replication depends on adequate control of two key parameters:  the replica-template adhesion-separation timing, by manipulating the template surface via oxidative etching, and the drying-cross-linking relative pace, by accurately tailoring the silanes mixture, the water-to-silane ratio, and their hydrolysis and polymerization.
doi_str_mv 10.1021/cm970229m
format Article
fullrecord <record><control><sourceid>acs_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1021_cm970229m</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>e95644079</sourcerecordid><originalsourceid>FETCH-LOGICAL-a295t-3ec698cdf91d4669c603262eb38adc53a1e05d47a0719dc05024c12a918595223</originalsourceid><addsrcrecordid>eNptz81KxDAUBeAgCtbRhW-QjQsX1ZukSZrlMM6MQgd_poK7ENMUOvZnSCo4b-DaR_RJrFRm5erC5eNwDkLnBK4IUHJtGyWBUtUcoIhwCjEHoIcoglTJOJFcHKOTEDYAZOBphNS6q78_v5auxk9uW1fW9FXX4q7Eq8r6rtv2w6vG89o1ru0DNm2Bp96bXThFR6Wpgzv7uxP0vJjns9s4u1_ezaZZbKjifcycFSq1RalIkQihrABGBXWvLDWF5cwQB7xIpAFJVGGBA00soUaRlCtOKZugyzF3qBOCd6Xe-qoxfqcJ6N_Ner95sPFoq9C7jz00_k0LySTX-cNarzKRPeY3mX4Z_MXojQ160737dljyT-4Pk7pkVA</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Sol−Gel Replication of Microoptical Elements and Arrays</title><source>ACS Publications</source><creator>Haruvy, Y ; Gilath, I ; Maniewictz, M ; Eisenberg, N</creator><creatorcontrib>Haruvy, Y ; Gilath, I ; Maniewictz, M ; Eisenberg, N</creatorcontrib><description>Facile replication of microoptical elements and arrays was performed in sol−gel matrixes prepared by the fast sol−gel method. These sol−gel resins, made from mixtures of alkylalkoxysilane monomers, undergo hydrolysis and polymerization within 10−20 min and curing within a few days. Single-step reproducible fabrication of large crack-free elements of 1 cm thickness and up to 10 cm in diameter was demonstrated. High accuracy of replication was facilitated by maintaining a very small shrinkage of only a few percent during the curing stage. This was attained by removing most of the volatile products from the sol, without gelling, prior to casting it onto the template. Accurate replication depends on adequate control of two key parameters:  the replica-template adhesion-separation timing, by manipulating the template surface via oxidative etching, and the drying-cross-linking relative pace, by accurately tailoring the silanes mixture, the water-to-silane ratio, and their hydrolysis and polymerization.</description><identifier>ISSN: 0897-4756</identifier><identifier>EISSN: 1520-5002</identifier><identifier>DOI: 10.1021/cm970229m</identifier><language>eng</language><publisher>American Chemical Society</publisher><ispartof>Chemistry of materials, 1997-11, Vol.9 (11), p.2604-2615</ispartof><rights>Copyright © 1997 American Chemical Society</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-a295t-3ec698cdf91d4669c603262eb38adc53a1e05d47a0719dc05024c12a918595223</citedby><cites>FETCH-LOGICAL-a295t-3ec698cdf91d4669c603262eb38adc53a1e05d47a0719dc05024c12a918595223</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://pubs.acs.org/doi/pdf/10.1021/cm970229m$$EPDF$$P50$$Gacs$$H</linktopdf><linktohtml>$$Uhttps://pubs.acs.org/doi/10.1021/cm970229m$$EHTML$$P50$$Gacs$$H</linktohtml><link.rule.ids>314,780,784,2765,27076,27924,27925,56738,56788</link.rule.ids></links><search><creatorcontrib>Haruvy, Y</creatorcontrib><creatorcontrib>Gilath, I</creatorcontrib><creatorcontrib>Maniewictz, M</creatorcontrib><creatorcontrib>Eisenberg, N</creatorcontrib><title>Sol−Gel Replication of Microoptical Elements and Arrays</title><title>Chemistry of materials</title><addtitle>Chem. Mater</addtitle><description>Facile replication of microoptical elements and arrays was performed in sol−gel matrixes prepared by the fast sol−gel method. These sol−gel resins, made from mixtures of alkylalkoxysilane monomers, undergo hydrolysis and polymerization within 10−20 min and curing within a few days. Single-step reproducible fabrication of large crack-free elements of 1 cm thickness and up to 10 cm in diameter was demonstrated. High accuracy of replication was facilitated by maintaining a very small shrinkage of only a few percent during the curing stage. This was attained by removing most of the volatile products from the sol, without gelling, prior to casting it onto the template. Accurate replication depends on adequate control of two key parameters:  the replica-template adhesion-separation timing, by manipulating the template surface via oxidative etching, and the drying-cross-linking relative pace, by accurately tailoring the silanes mixture, the water-to-silane ratio, and their hydrolysis and polymerization.</description><issn>0897-4756</issn><issn>1520-5002</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1997</creationdate><recordtype>article</recordtype><recordid>eNptz81KxDAUBeAgCtbRhW-QjQsX1ZukSZrlMM6MQgd_poK7ENMUOvZnSCo4b-DaR_RJrFRm5erC5eNwDkLnBK4IUHJtGyWBUtUcoIhwCjEHoIcoglTJOJFcHKOTEDYAZOBphNS6q78_v5auxk9uW1fW9FXX4q7Eq8r6rtv2w6vG89o1ru0DNm2Bp96bXThFR6Wpgzv7uxP0vJjns9s4u1_ezaZZbKjifcycFSq1RalIkQihrABGBXWvLDWF5cwQB7xIpAFJVGGBA00soUaRlCtOKZugyzF3qBOCd6Xe-qoxfqcJ6N_Ner95sPFoq9C7jz00_k0LySTX-cNarzKRPeY3mX4Z_MXojQ160737dljyT-4Pk7pkVA</recordid><startdate>19971118</startdate><enddate>19971118</enddate><creator>Haruvy, Y</creator><creator>Gilath, I</creator><creator>Maniewictz, M</creator><creator>Eisenberg, N</creator><general>American Chemical Society</general><scope>BSCLL</scope><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>19971118</creationdate><title>Sol−Gel Replication of Microoptical Elements and Arrays</title><author>Haruvy, Y ; Gilath, I ; Maniewictz, M ; Eisenberg, N</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-a295t-3ec698cdf91d4669c603262eb38adc53a1e05d47a0719dc05024c12a918595223</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1997</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Haruvy, Y</creatorcontrib><creatorcontrib>Gilath, I</creatorcontrib><creatorcontrib>Maniewictz, M</creatorcontrib><creatorcontrib>Eisenberg, N</creatorcontrib><collection>Istex</collection><collection>CrossRef</collection><jtitle>Chemistry of materials</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Haruvy, Y</au><au>Gilath, I</au><au>Maniewictz, M</au><au>Eisenberg, N</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Sol−Gel Replication of Microoptical Elements and Arrays</atitle><jtitle>Chemistry of materials</jtitle><addtitle>Chem. Mater</addtitle><date>1997-11-18</date><risdate>1997</risdate><volume>9</volume><issue>11</issue><spage>2604</spage><epage>2615</epage><pages>2604-2615</pages><issn>0897-4756</issn><eissn>1520-5002</eissn><abstract>Facile replication of microoptical elements and arrays was performed in sol−gel matrixes prepared by the fast sol−gel method. These sol−gel resins, made from mixtures of alkylalkoxysilane monomers, undergo hydrolysis and polymerization within 10−20 min and curing within a few days. Single-step reproducible fabrication of large crack-free elements of 1 cm thickness and up to 10 cm in diameter was demonstrated. High accuracy of replication was facilitated by maintaining a very small shrinkage of only a few percent during the curing stage. This was attained by removing most of the volatile products from the sol, without gelling, prior to casting it onto the template. Accurate replication depends on adequate control of two key parameters:  the replica-template adhesion-separation timing, by manipulating the template surface via oxidative etching, and the drying-cross-linking relative pace, by accurately tailoring the silanes mixture, the water-to-silane ratio, and their hydrolysis and polymerization.</abstract><pub>American Chemical Society</pub><doi>10.1021/cm970229m</doi><tpages>12</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0897-4756
ispartof Chemistry of materials, 1997-11, Vol.9 (11), p.2604-2615
issn 0897-4756
1520-5002
language eng
recordid cdi_crossref_primary_10_1021_cm970229m
source ACS Publications
title Sol−Gel Replication of Microoptical Elements and Arrays
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-06T22%3A17%3A18IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-acs_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Sol%E2%88%92Gel%20Replication%20of%20Microoptical%20Elements%20and%20Arrays&rft.jtitle=Chemistry%20of%20materials&rft.au=Haruvy,%20Y&rft.date=1997-11-18&rft.volume=9&rft.issue=11&rft.spage=2604&rft.epage=2615&rft.pages=2604-2615&rft.issn=0897-4756&rft.eissn=1520-5002&rft_id=info:doi/10.1021/cm970229m&rft_dat=%3Cacs_cross%3Ee95644079%3C/acs_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true