High-Temperature Formation of Titanate Nanotubes and the Transformation Mechanism of Nanotubes into Nanowires
Large-scale pure titanate nanotubes were synthesized through the hydrothermal reaction between TiO2 powders and concentrated NaOH under an unexpected high temperature of 240 °C, while it was generally claimed that it is impossible to form nanotubes at temperatures higher than 180 °C. The titanate na...