Mechanically Robust Anion Exchange Membranes via Long Hydrophilic Cross-Linkers

Mechanically tough, cross-linked anion exchange membranes (AEM) based on poly­(2,6-dimethyl­phenylene oxide) (PPO) were achieved by introducing a hydrophilic and flexible Jeffamine (O,O′-bis­(2-amino­propyl)­polypropylene glycol-block-poly­(ethylene glycol)-block-polypropylene glycol 500) cross-link...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Macromolecules 2017-03, Vol.50 (6), p.2329-2337
Hauptverfasser: Zhu, Liang, Zimudzi, Tawanda J, Wang, Ying, Yu, Xuedi, Pan, Jing, Han, Juanjuan, Kushner, Douglas I, Zhuang, Lin, Hickner, Michael A
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Mechanically tough, cross-linked anion exchange membranes (AEM) based on poly­(2,6-dimethyl­phenylene oxide) (PPO) were achieved by introducing a hydrophilic and flexible Jeffamine (O,O′-bis­(2-amino­propyl)­polypropylene glycol-block-poly­(ethylene glycol)-block-polypropylene glycol 500) cross-linker into the cationic macromolecular network. The Jeffamine cross-linked AEMs demonstrated outstanding strength and flexibility and were mechanically tougher than AEM samples based on benzyl­trimethyl­ammonium (BTMA) functionalized PPO alone. The hydrated BTMA40 membrane showed 52% elongation at break, while the Jeffamine-based J10PPO sample had a 167% elongation at break. In addition, the hydroxide (OH–) conductivity of the J10PPO sample was 52 mS/cm at 80 °C with a swelling ratio of 61%, while BTMA60 suffered severe swelling above 60 °C. The alkaline stabilities of the AEMs with different degrees of Jeffamine cross-linking were evaluated in 1 M NaOH at 80 °C for 500 h. During the 500 h degradation test, J10PPO exhibited the greatest cation stability. The OH– conductivity of this membrane decreased by 30% over 500 h. In contrast, the OH– conductivity of BTMA40 decreased to 9.6 mS/cm at 20 °C, which is 60% lower than the value measured for the sample before the stability test. Based on the high-performance Jeffamine cross-linked AEM, a Pt-catalyzed fuel cell with a peak power density of 314 mW/cm2 was demonstrated at 60 °C under 100% related humidity.