Single-Ion-Conducting Polyether Electrolytes via Orthogonal Postpolymerization Modification

Solid polymer electrolytes are considered promising alternatives for overcoming the safety issues of conventional liquid electrolytes. In particular, poly­(ethylene oxide)-based polymer electrolytes are widely studied because of their high flexibility and ion-solvating capability but suffer from low...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Macromolecules 2023-09, Vol.56 (18), p.7520-7531
Hauptverfasser: Lee, Jiyoung, Kim, Seonho, Kwon, Hyeoksu, Jo, Seungyun, Ryu, Du Yeol, Choi, U Hyeok, Kim, Byeong-Su
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 7531
container_issue 18
container_start_page 7520
container_title Macromolecules
container_volume 56
creator Lee, Jiyoung
Kim, Seonho
Kwon, Hyeoksu
Jo, Seungyun
Ryu, Du Yeol
Choi, U Hyeok
Kim, Byeong-Su
description Solid polymer electrolytes are considered promising alternatives for overcoming the safety issues of conventional liquid electrolytes. In particular, poly­(ethylene oxide)-based polymer electrolytes are widely studied because of their high flexibility and ion-solvating capability but suffer from low ionic conductivity at room temperature due to high crystallinity of poly­(ethylene oxide) restricting segmental motion. To address this challenge, we present a new type of polyether-based single-ion-conducting solid polymer electrolyte whose constituent functional groups can be tailored in an orthogonal manner. The electrolyte structure was designed to possess weakly binding anionic and flexible lithium-cation-solvating pendants along the polyether backbone. Specifically, bulk polymerization between allylamine and diepoxide was employed to synthesize the polyether backbone with functional allyl and hydroxyl groups. The resulting polymer was subsequently further functionalized with lithium bis­(trifluoromethanesulfonyl)­imide and tri­(ethylene glycol) groups to create a single-ion conductor. Tri­(ethylene glycol) promoted segmental α and ion-rearranging α2 relaxations (arising from a lowered glass transition temperature and increased ion mobility, μ) as well as increased the dielectric constant (leading to a large number density of conducting ions, p), resulting in a significant increase in the ionic conductivity (σ ∼ μp), e.g., a 250-fold increase at 60 °C. Furthermore, addition of succinonitrile (a plasticizer) increased the ionic conductivity of the single-ion-conducting solid polymer electrolyte to 1.8 × 10–5 S cm–1 at 60 °C because of a weakened ion–ion correlation as revealed by wide-angle X-ray scattering analyses. These results demonstrate the potential of tailoring properties of solid polymer electrolytes by introducing various functional moieties.
doi_str_mv 10.1021/acs.macromol.3c00985
format Article
fullrecord <record><control><sourceid>acs_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1021_acs_macromol_3c00985</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>b902932452</sourcerecordid><originalsourceid>FETCH-LOGICAL-a241t-3d8bb695e9834d0e14f2f2433ff269ae9e331e2b2029dcb899503dba3c27b5e33</originalsourceid><addsrcrecordid>eNp9kM1OAjEUhRujiYi-gYt5geLtH0yXhqCSYDBRVy4mnU4LJTNT0hYTfHqK4NbVzbnnnpucD6F7AiMClDwoHUed0sF3vh0xDSBLcYEGRFDAomTiEg0AKMeSysk1uolxA0CI4GyAvt5dv2oNnvseT33f7HTKi-LNt3uT1iYUs9boFLJMJhbfThXLkNZ-5XvV5quYttnqTHA_KjnfF6--cdbpX3GLrqxqo7k7zyH6fJp9TF_wYvk8nz4usKKcJMyasq7HUhhZMt6AIdxSSzlj1tKxVEYaxoihNQUqG12XUgpgTa2YppNaZHOI-OlvJhBjMLbaBtepsK8IVEdAVQZU_QGqzoByDE6xo7vxu5Arxf8jBzYmcCo</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Single-Ion-Conducting Polyether Electrolytes via Orthogonal Postpolymerization Modification</title><source>ACS Publications</source><creator>Lee, Jiyoung ; Kim, Seonho ; Kwon, Hyeoksu ; Jo, Seungyun ; Ryu, Du Yeol ; Choi, U Hyeok ; Kim, Byeong-Su</creator><creatorcontrib>Lee, Jiyoung ; Kim, Seonho ; Kwon, Hyeoksu ; Jo, Seungyun ; Ryu, Du Yeol ; Choi, U Hyeok ; Kim, Byeong-Su</creatorcontrib><description>Solid polymer electrolytes are considered promising alternatives for overcoming the safety issues of conventional liquid electrolytes. In particular, poly­(ethylene oxide)-based polymer electrolytes are widely studied because of their high flexibility and ion-solvating capability but suffer from low ionic conductivity at room temperature due to high crystallinity of poly­(ethylene oxide) restricting segmental motion. To address this challenge, we present a new type of polyether-based single-ion-conducting solid polymer electrolyte whose constituent functional groups can be tailored in an orthogonal manner. The electrolyte structure was designed to possess weakly binding anionic and flexible lithium-cation-solvating pendants along the polyether backbone. Specifically, bulk polymerization between allylamine and diepoxide was employed to synthesize the polyether backbone with functional allyl and hydroxyl groups. The resulting polymer was subsequently further functionalized with lithium bis­(trifluoromethanesulfonyl)­imide and tri­(ethylene glycol) groups to create a single-ion conductor. Tri­(ethylene glycol) promoted segmental α and ion-rearranging α2 relaxations (arising from a lowered glass transition temperature and increased ion mobility, μ) as well as increased the dielectric constant (leading to a large number density of conducting ions, p), resulting in a significant increase in the ionic conductivity (σ ∼ μp), e.g., a 250-fold increase at 60 °C. Furthermore, addition of succinonitrile (a plasticizer) increased the ionic conductivity of the single-ion-conducting solid polymer electrolyte to 1.8 × 10–5 S cm–1 at 60 °C because of a weakened ion–ion correlation as revealed by wide-angle X-ray scattering analyses. These results demonstrate the potential of tailoring properties of solid polymer electrolytes by introducing various functional moieties.</description><identifier>ISSN: 0024-9297</identifier><identifier>EISSN: 1520-5835</identifier><identifier>DOI: 10.1021/acs.macromol.3c00985</identifier><language>eng</language><publisher>American Chemical Society</publisher><ispartof>Macromolecules, 2023-09, Vol.56 (18), p.7520-7531</ispartof><rights>2023 American Chemical Society</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><cites>FETCH-LOGICAL-a241t-3d8bb695e9834d0e14f2f2433ff269ae9e331e2b2029dcb899503dba3c27b5e33</cites><orcidid>0000-0003-2466-5771 ; 0000-0002-6419-3054 ; 0000-0002-0048-9550 ; 0000-0002-0929-7934</orcidid></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://pubs.acs.org/doi/pdf/10.1021/acs.macromol.3c00985$$EPDF$$P50$$Gacs$$H</linktopdf><linktohtml>$$Uhttps://pubs.acs.org/doi/10.1021/acs.macromol.3c00985$$EHTML$$P50$$Gacs$$H</linktohtml><link.rule.ids>314,780,784,2765,27076,27924,27925,56738,56788</link.rule.ids></links><search><creatorcontrib>Lee, Jiyoung</creatorcontrib><creatorcontrib>Kim, Seonho</creatorcontrib><creatorcontrib>Kwon, Hyeoksu</creatorcontrib><creatorcontrib>Jo, Seungyun</creatorcontrib><creatorcontrib>Ryu, Du Yeol</creatorcontrib><creatorcontrib>Choi, U Hyeok</creatorcontrib><creatorcontrib>Kim, Byeong-Su</creatorcontrib><title>Single-Ion-Conducting Polyether Electrolytes via Orthogonal Postpolymerization Modification</title><title>Macromolecules</title><addtitle>Macromolecules</addtitle><description>Solid polymer electrolytes are considered promising alternatives for overcoming the safety issues of conventional liquid electrolytes. In particular, poly­(ethylene oxide)-based polymer electrolytes are widely studied because of their high flexibility and ion-solvating capability but suffer from low ionic conductivity at room temperature due to high crystallinity of poly­(ethylene oxide) restricting segmental motion. To address this challenge, we present a new type of polyether-based single-ion-conducting solid polymer electrolyte whose constituent functional groups can be tailored in an orthogonal manner. The electrolyte structure was designed to possess weakly binding anionic and flexible lithium-cation-solvating pendants along the polyether backbone. Specifically, bulk polymerization between allylamine and diepoxide was employed to synthesize the polyether backbone with functional allyl and hydroxyl groups. The resulting polymer was subsequently further functionalized with lithium bis­(trifluoromethanesulfonyl)­imide and tri­(ethylene glycol) groups to create a single-ion conductor. Tri­(ethylene glycol) promoted segmental α and ion-rearranging α2 relaxations (arising from a lowered glass transition temperature and increased ion mobility, μ) as well as increased the dielectric constant (leading to a large number density of conducting ions, p), resulting in a significant increase in the ionic conductivity (σ ∼ μp), e.g., a 250-fold increase at 60 °C. Furthermore, addition of succinonitrile (a plasticizer) increased the ionic conductivity of the single-ion-conducting solid polymer electrolyte to 1.8 × 10–5 S cm–1 at 60 °C because of a weakened ion–ion correlation as revealed by wide-angle X-ray scattering analyses. These results demonstrate the potential of tailoring properties of solid polymer electrolytes by introducing various functional moieties.</description><issn>0024-9297</issn><issn>1520-5835</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2023</creationdate><recordtype>article</recordtype><recordid>eNp9kM1OAjEUhRujiYi-gYt5geLtH0yXhqCSYDBRVy4mnU4LJTNT0hYTfHqK4NbVzbnnnpucD6F7AiMClDwoHUed0sF3vh0xDSBLcYEGRFDAomTiEg0AKMeSysk1uolxA0CI4GyAvt5dv2oNnvseT33f7HTKi-LNt3uT1iYUs9boFLJMJhbfThXLkNZ-5XvV5quYttnqTHA_KjnfF6--cdbpX3GLrqxqo7k7zyH6fJp9TF_wYvk8nz4usKKcJMyasq7HUhhZMt6AIdxSSzlj1tKxVEYaxoihNQUqG12XUgpgTa2YppNaZHOI-OlvJhBjMLbaBtepsK8IVEdAVQZU_QGqzoByDE6xo7vxu5Arxf8jBzYmcCo</recordid><startdate>20230926</startdate><enddate>20230926</enddate><creator>Lee, Jiyoung</creator><creator>Kim, Seonho</creator><creator>Kwon, Hyeoksu</creator><creator>Jo, Seungyun</creator><creator>Ryu, Du Yeol</creator><creator>Choi, U Hyeok</creator><creator>Kim, Byeong-Su</creator><general>American Chemical Society</general><scope>AAYXX</scope><scope>CITATION</scope><orcidid>https://orcid.org/0000-0003-2466-5771</orcidid><orcidid>https://orcid.org/0000-0002-6419-3054</orcidid><orcidid>https://orcid.org/0000-0002-0048-9550</orcidid><orcidid>https://orcid.org/0000-0002-0929-7934</orcidid></search><sort><creationdate>20230926</creationdate><title>Single-Ion-Conducting Polyether Electrolytes via Orthogonal Postpolymerization Modification</title><author>Lee, Jiyoung ; Kim, Seonho ; Kwon, Hyeoksu ; Jo, Seungyun ; Ryu, Du Yeol ; Choi, U Hyeok ; Kim, Byeong-Su</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-a241t-3d8bb695e9834d0e14f2f2433ff269ae9e331e2b2029dcb899503dba3c27b5e33</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2023</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Lee, Jiyoung</creatorcontrib><creatorcontrib>Kim, Seonho</creatorcontrib><creatorcontrib>Kwon, Hyeoksu</creatorcontrib><creatorcontrib>Jo, Seungyun</creatorcontrib><creatorcontrib>Ryu, Du Yeol</creatorcontrib><creatorcontrib>Choi, U Hyeok</creatorcontrib><creatorcontrib>Kim, Byeong-Su</creatorcontrib><collection>CrossRef</collection><jtitle>Macromolecules</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Lee, Jiyoung</au><au>Kim, Seonho</au><au>Kwon, Hyeoksu</au><au>Jo, Seungyun</au><au>Ryu, Du Yeol</au><au>Choi, U Hyeok</au><au>Kim, Byeong-Su</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Single-Ion-Conducting Polyether Electrolytes via Orthogonal Postpolymerization Modification</atitle><jtitle>Macromolecules</jtitle><addtitle>Macromolecules</addtitle><date>2023-09-26</date><risdate>2023</risdate><volume>56</volume><issue>18</issue><spage>7520</spage><epage>7531</epage><pages>7520-7531</pages><issn>0024-9297</issn><eissn>1520-5835</eissn><abstract>Solid polymer electrolytes are considered promising alternatives for overcoming the safety issues of conventional liquid electrolytes. In particular, poly­(ethylene oxide)-based polymer electrolytes are widely studied because of their high flexibility and ion-solvating capability but suffer from low ionic conductivity at room temperature due to high crystallinity of poly­(ethylene oxide) restricting segmental motion. To address this challenge, we present a new type of polyether-based single-ion-conducting solid polymer electrolyte whose constituent functional groups can be tailored in an orthogonal manner. The electrolyte structure was designed to possess weakly binding anionic and flexible lithium-cation-solvating pendants along the polyether backbone. Specifically, bulk polymerization between allylamine and diepoxide was employed to synthesize the polyether backbone with functional allyl and hydroxyl groups. The resulting polymer was subsequently further functionalized with lithium bis­(trifluoromethanesulfonyl)­imide and tri­(ethylene glycol) groups to create a single-ion conductor. Tri­(ethylene glycol) promoted segmental α and ion-rearranging α2 relaxations (arising from a lowered glass transition temperature and increased ion mobility, μ) as well as increased the dielectric constant (leading to a large number density of conducting ions, p), resulting in a significant increase in the ionic conductivity (σ ∼ μp), e.g., a 250-fold increase at 60 °C. Furthermore, addition of succinonitrile (a plasticizer) increased the ionic conductivity of the single-ion-conducting solid polymer electrolyte to 1.8 × 10–5 S cm–1 at 60 °C because of a weakened ion–ion correlation as revealed by wide-angle X-ray scattering analyses. These results demonstrate the potential of tailoring properties of solid polymer electrolytes by introducing various functional moieties.</abstract><pub>American Chemical Society</pub><doi>10.1021/acs.macromol.3c00985</doi><tpages>12</tpages><orcidid>https://orcid.org/0000-0003-2466-5771</orcidid><orcidid>https://orcid.org/0000-0002-6419-3054</orcidid><orcidid>https://orcid.org/0000-0002-0048-9550</orcidid><orcidid>https://orcid.org/0000-0002-0929-7934</orcidid></addata></record>
fulltext fulltext
identifier ISSN: 0024-9297
ispartof Macromolecules, 2023-09, Vol.56 (18), p.7520-7531
issn 0024-9297
1520-5835
language eng
recordid cdi_crossref_primary_10_1021_acs_macromol_3c00985
source ACS Publications
title Single-Ion-Conducting Polyether Electrolytes via Orthogonal Postpolymerization Modification
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T11%3A05%3A09IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-acs_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Single-Ion-Conducting%20Polyether%20Electrolytes%20via%20Orthogonal%20Postpolymerization%20Modification&rft.jtitle=Macromolecules&rft.au=Lee,%20Jiyoung&rft.date=2023-09-26&rft.volume=56&rft.issue=18&rft.spage=7520&rft.epage=7531&rft.pages=7520-7531&rft.issn=0024-9297&rft.eissn=1520-5835&rft_id=info:doi/10.1021/acs.macromol.3c00985&rft_dat=%3Cacs_cross%3Eb902932452%3C/acs_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true