Single crystals of calcium pyroniobate, Ca2Nb2O7, have been grown from the melt by the Czochralski method. Crystal growth along a 〈OVW〉 direction is easy, being characterized by the formation of large area mirror facets, which under certain conditions leads to the growth of thin ribbon crystals. Gro...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:physica status solidi (b) 1967, Vol.22 (2), p.499-504
1. Verfasser: Graves, P. W.
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page 504
container_issue 2
container_start_page 499
container_title physica status solidi (b)
container_volume 22
creator Graves, P. W.
description Single crystals of calcium pyroniobate, Ca2Nb2O7, have been grown from the melt by the Czochralski method. Crystal growth along a 〈OVW〉 direction is easy, being characterized by the formation of large area mirror facets, which under certain conditions leads to the growth of thin ribbon crystals. Growth along [100] is difficult and rates of less than 0.4 cm/h have to be used to obtain crack free crystals. Growth defects such as inclusions and cavities were found to be absent in the crystals, and no evidence was found for the presence of impurity striations. Einkristalle von Kalziumpyroniobat, Ca2Nb2O7, werden nach dem Czochralski‐Verfahren aus der Schmelze gezogen. Das Kristallwachstum in der 〈OVW〉‐Richtung ist leicht und ist durch die Bildung größflächiger Spiegelebenen gekennzeichnet. Dies führt unter gewissen Umständen zum Wachstum dünner Bandkristalle. Das Wachstum in der [100]‐Richtung ist schwierig und die Wachstumsgeschwindigkeit muß unter 0,4 cm/h liegen, um rißfreie Kristalle zu erhalten. Wachstumsfehler wie Einlagerungen und Hohlräume lassen sich nicht im Kristall nachweisen, und es liegen keine Beweise für die Anwesenheit von Verunreinigungsschichten vor.
doi_str_mv 10.1002/pssb.19670220222
format Article
fullrecord <record><control><sourceid>istex_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1002_pssb_19670220222</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>ark_67375_WNG_05SH5HQ0_5</sourcerecordid><originalsourceid>FETCH-LOGICAL-c3352-7a0b7198b37f7003a0a447d47eb731dacc2a459d38a3562ea7920490312ffbf03</originalsourceid><addsrcrecordid>eNqFz8FKw0AQgOFFFKzVu8c8gKmzO9lM9-BBg7ZC0UoUj8sm2dVo2pTdSM3b21IRPQkDc5lv4GfslMOIA4jzVQjFiKuUQIjNiD024FLwGJXk-2wASBBzReKQHYXwBgDEkQ_YWV4vXxobZb4PnWmiiW_X3WvUuigzTVl_LKJ579tl3Rams8fswJkm2JPvPWRPN9eP2TSe3U9us8tZXCJKEZOBgrgaF0iOANCASRKqErIFIa9MWQqTSFXh2KBMhTWkBCQKkAvnCgc4ZLD7W_o2BG-dXvl6YXyvOehtrd7W6l-1G3KxI-u6sf2_93qe51d_fbzzdejs5483_l2nhCT1891Eg8yncvoAWuIXcdNn4g</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Single Crystal Growth of Calcium Pyroniobate</title><source>Wiley Online Library Journals Frontfile Complete</source><creator>Graves, P. W.</creator><creatorcontrib>Graves, P. W.</creatorcontrib><description>Single crystals of calcium pyroniobate, Ca2Nb2O7, have been grown from the melt by the Czochralski method. Crystal growth along a 〈OVW〉 direction is easy, being characterized by the formation of large area mirror facets, which under certain conditions leads to the growth of thin ribbon crystals. Growth along [100] is difficult and rates of less than 0.4 cm/h have to be used to obtain crack free crystals. Growth defects such as inclusions and cavities were found to be absent in the crystals, and no evidence was found for the presence of impurity striations. Einkristalle von Kalziumpyroniobat, Ca2Nb2O7, werden nach dem Czochralski‐Verfahren aus der Schmelze gezogen. Das Kristallwachstum in der 〈OVW〉‐Richtung ist leicht und ist durch die Bildung größflächiger Spiegelebenen gekennzeichnet. Dies führt unter gewissen Umständen zum Wachstum dünner Bandkristalle. Das Wachstum in der [100]‐Richtung ist schwierig und die Wachstumsgeschwindigkeit muß unter 0,4 cm/h liegen, um rißfreie Kristalle zu erhalten. Wachstumsfehler wie Einlagerungen und Hohlräume lassen sich nicht im Kristall nachweisen, und es liegen keine Beweise für die Anwesenheit von Verunreinigungsschichten vor.</description><identifier>ISSN: 0370-1972</identifier><identifier>EISSN: 1521-3951</identifier><identifier>DOI: 10.1002/pssb.19670220222</identifier><language>eng</language><publisher>Berlin: WILEY-VCH Verlag</publisher><ispartof>physica status solidi (b), 1967, Vol.22 (2), p.499-504</ispartof><rights>Copyright © 1967 WILEY‐VCH Verlag GmbH &amp; Co. KGaA, Weinheim</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c3352-7a0b7198b37f7003a0a447d47eb731dacc2a459d38a3562ea7920490312ffbf03</citedby><cites>FETCH-LOGICAL-c3352-7a0b7198b37f7003a0a447d47eb731dacc2a459d38a3562ea7920490312ffbf03</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://onlinelibrary.wiley.com/doi/pdf/10.1002%2Fpssb.19670220222$$EPDF$$P50$$Gwiley$$H</linktopdf><linktohtml>$$Uhttps://onlinelibrary.wiley.com/doi/full/10.1002%2Fpssb.19670220222$$EHTML$$P50$$Gwiley$$H</linktohtml><link.rule.ids>314,776,780,1411,4010,27900,27901,27902,45550,45551</link.rule.ids></links><search><creatorcontrib>Graves, P. W.</creatorcontrib><title>Single Crystal Growth of Calcium Pyroniobate</title><title>physica status solidi (b)</title><addtitle>phys. stat. sol. (b)</addtitle><description>Single crystals of calcium pyroniobate, Ca2Nb2O7, have been grown from the melt by the Czochralski method. Crystal growth along a 〈OVW〉 direction is easy, being characterized by the formation of large area mirror facets, which under certain conditions leads to the growth of thin ribbon crystals. Growth along [100] is difficult and rates of less than 0.4 cm/h have to be used to obtain crack free crystals. Growth defects such as inclusions and cavities were found to be absent in the crystals, and no evidence was found for the presence of impurity striations. Einkristalle von Kalziumpyroniobat, Ca2Nb2O7, werden nach dem Czochralski‐Verfahren aus der Schmelze gezogen. Das Kristallwachstum in der 〈OVW〉‐Richtung ist leicht und ist durch die Bildung größflächiger Spiegelebenen gekennzeichnet. Dies führt unter gewissen Umständen zum Wachstum dünner Bandkristalle. Das Wachstum in der [100]‐Richtung ist schwierig und die Wachstumsgeschwindigkeit muß unter 0,4 cm/h liegen, um rißfreie Kristalle zu erhalten. Wachstumsfehler wie Einlagerungen und Hohlräume lassen sich nicht im Kristall nachweisen, und es liegen keine Beweise für die Anwesenheit von Verunreinigungsschichten vor.</description><issn>0370-1972</issn><issn>1521-3951</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1967</creationdate><recordtype>article</recordtype><recordid>eNqFz8FKw0AQgOFFFKzVu8c8gKmzO9lM9-BBg7ZC0UoUj8sm2dVo2pTdSM3b21IRPQkDc5lv4GfslMOIA4jzVQjFiKuUQIjNiD024FLwGJXk-2wASBBzReKQHYXwBgDEkQ_YWV4vXxobZb4PnWmiiW_X3WvUuigzTVl_LKJ579tl3Rams8fswJkm2JPvPWRPN9eP2TSe3U9us8tZXCJKEZOBgrgaF0iOANCASRKqErIFIa9MWQqTSFXh2KBMhTWkBCQKkAvnCgc4ZLD7W_o2BG-dXvl6YXyvOehtrd7W6l-1G3KxI-u6sf2_93qe51d_fbzzdejs5483_l2nhCT1891Eg8yncvoAWuIXcdNn4g</recordid><startdate>1967</startdate><enddate>1967</enddate><creator>Graves, P. W.</creator><general>WILEY-VCH Verlag</general><general>WILEY‐VCH Verlag</general><scope>BSCLL</scope><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>1967</creationdate><title>Single Crystal Growth of Calcium Pyroniobate</title><author>Graves, P. W.</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c3352-7a0b7198b37f7003a0a447d47eb731dacc2a459d38a3562ea7920490312ffbf03</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1967</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Graves, P. W.</creatorcontrib><collection>Istex</collection><collection>CrossRef</collection><jtitle>physica status solidi (b)</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Graves, P. W.</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Single Crystal Growth of Calcium Pyroniobate</atitle><jtitle>physica status solidi (b)</jtitle><addtitle>phys. stat. sol. (b)</addtitle><date>1967</date><risdate>1967</risdate><volume>22</volume><issue>2</issue><spage>499</spage><epage>504</epage><pages>499-504</pages><issn>0370-1972</issn><eissn>1521-3951</eissn><abstract>Single crystals of calcium pyroniobate, Ca2Nb2O7, have been grown from the melt by the Czochralski method. Crystal growth along a 〈OVW〉 direction is easy, being characterized by the formation of large area mirror facets, which under certain conditions leads to the growth of thin ribbon crystals. Growth along [100] is difficult and rates of less than 0.4 cm/h have to be used to obtain crack free crystals. Growth defects such as inclusions and cavities were found to be absent in the crystals, and no evidence was found for the presence of impurity striations. Einkristalle von Kalziumpyroniobat, Ca2Nb2O7, werden nach dem Czochralski‐Verfahren aus der Schmelze gezogen. Das Kristallwachstum in der 〈OVW〉‐Richtung ist leicht und ist durch die Bildung größflächiger Spiegelebenen gekennzeichnet. Dies führt unter gewissen Umständen zum Wachstum dünner Bandkristalle. Das Wachstum in der [100]‐Richtung ist schwierig und die Wachstumsgeschwindigkeit muß unter 0,4 cm/h liegen, um rißfreie Kristalle zu erhalten. Wachstumsfehler wie Einlagerungen und Hohlräume lassen sich nicht im Kristall nachweisen, und es liegen keine Beweise für die Anwesenheit von Verunreinigungsschichten vor.</abstract><cop>Berlin</cop><pub>WILEY-VCH Verlag</pub><doi>10.1002/pssb.19670220222</doi><tpages>6</tpages></addata></record>
fulltext fulltext
identifier ISSN: 0370-1972
ispartof physica status solidi (b), 1967, Vol.22 (2), p.499-504
issn 0370-1972
1521-3951
language eng
recordid cdi_crossref_primary_10_1002_pssb_19670220222
source Wiley Online Library Journals Frontfile Complete
title Single Crystal Growth of Calcium Pyroniobate
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T02%3A28%3A05IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-istex_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Single%20Crystal%20Growth%20of%20Calcium%20Pyroniobate&rft.jtitle=physica%20status%20solidi%20(b)&rft.au=Graves,%20P.%20W.&rft.date=1967&rft.volume=22&rft.issue=2&rft.spage=499&rft.epage=504&rft.pages=499-504&rft.issn=0370-1972&rft.eissn=1521-3951&rft_id=info:doi/10.1002/pssb.19670220222&rft_dat=%3Cistex_cross%3Eark_67375_WNG_05SH5HQ0_5%3C/istex_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true