Effect of stereoregularity on the thermo-oxidative degradation of poly(propylene)s estimated by chemiluminescence
The effect of stereoregularity on the thermo‐oxidative degradation of poly(propylene)s, isotactic (IPP) and syndiotactic (SPP), was compared with that of high density polyethylene (HDPE) by means of chemiluminescence (CL). SPP is extremely stable to thermal oxidation and CL signals appeared much lat...
Gespeichert in:
Veröffentlicht in: | Macromolecular rapid communications. 1997-08, Vol.18 (8), p.667-671 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 671 |
---|---|
container_issue | 8 |
container_start_page | 667 |
container_title | Macromolecular rapid communications. |
container_volume | 18 |
creator | Osawa, Zenjiro Kato, Masahide Terano, Minoru |
description | The effect of stereoregularity on the thermo‐oxidative degradation of poly(propylene)s, isotactic (IPP) and syndiotactic (SPP), was compared with that of high density polyethylene (HDPE) by means of chemiluminescence (CL). SPP is extremely stable to thermal oxidation and CL signals appeared much later than in IPP and even later than in HDPE. For example, at 160°C the maximum intensity of CL was measured after only 13 min for IPP, 60 min for HDPE and 260 min for SPP. IR spectroscopic results support the conclusions drawn from CL results. |
doi_str_mv | 10.1002/marc.1997.030180807 |
format | Article |
fullrecord | <record><control><sourceid>wiley_cross</sourceid><recordid>TN_cdi_crossref_primary_10_1002_marc_1997_030180807</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>MARC030180807</sourcerecordid><originalsourceid>FETCH-LOGICAL-c3697-2711f16efeb8be3738c1baf7eab048cfcd6c78f5eee5a7d798a668af53b834de3</originalsourceid><addsrcrecordid>eNqNkEtLw0AUhYMoWKu_wE0WLnSROo8kM9kIUmsVqkKpFNwMk8mddjQvZ1Jt_r0JleLSxeWexTnnXj7PO8dohBEi14W0aoSThI0QRZgjjtiBN8ARwQFNCDvsNCIkwJTGx96Jc-8IIR4iMvA-J1qDavxK-64BC5WF1SaX1jStX5V-s4Z-bFEF1dZksjFf4GewsrLXnaHL1VXeXta2qtscSrhyPrjGFLKBzE9bX62hMPmmMCU4BaWCU-9Iy9zB2e8eeq_3k8X4IZi9TB_Ht7NA0ThhAWEYaxyDhpSnQBnlCqdSM5ApCrnSKosV4zoCgEiyjCVcxjGXOqIpp2EGdOjRXa-ylXMWtKht95ZtBUaipyZ6aqKnJvbUutTFLlVLp2SurSyVcfsoYWGSINLZbna2b5ND-59m8XQ7H_-9E-wKTId9uy-Q9kPEjLJILJ-nYhnxOb9bvIkp_QHJGZNZ</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype></control><display><type>article</type><title>Effect of stereoregularity on the thermo-oxidative degradation of poly(propylene)s estimated by chemiluminescence</title><source>Access via Wiley Online Library</source><creator>Osawa, Zenjiro ; Kato, Masahide ; Terano, Minoru</creator><creatorcontrib>Osawa, Zenjiro ; Kato, Masahide ; Terano, Minoru</creatorcontrib><description>The effect of stereoregularity on the thermo‐oxidative degradation of poly(propylene)s, isotactic (IPP) and syndiotactic (SPP), was compared with that of high density polyethylene (HDPE) by means of chemiluminescence (CL). SPP is extremely stable to thermal oxidation and CL signals appeared much later than in IPP and even later than in HDPE. For example, at 160°C the maximum intensity of CL was measured after only 13 min for IPP, 60 min for HDPE and 260 min for SPP. IR spectroscopic results support the conclusions drawn from CL results.</description><identifier>ISSN: 1022-1336</identifier><identifier>EISSN: 1521-3927</identifier><identifier>DOI: 10.1002/marc.1997.030180807</identifier><language>eng</language><publisher>Zug: Hüthig & Wepf Verlag</publisher><subject>Applied sciences ; Exact sciences and technology ; Organic polymers ; Physicochemistry of polymers ; Properties and characterization ; Thermal and thermodynamic properties</subject><ispartof>Macromolecular rapid communications., 1997-08, Vol.18 (8), p.667-671</ispartof><rights>1997 Hüthig & Wepf Verlag, Zug</rights><rights>1997 INIST-CNRS</rights><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed><citedby>FETCH-LOGICAL-c3697-2711f16efeb8be3738c1baf7eab048cfcd6c78f5eee5a7d798a668af53b834de3</citedby><cites>FETCH-LOGICAL-c3697-2711f16efeb8be3738c1baf7eab048cfcd6c78f5eee5a7d798a668af53b834de3</cites></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktopdf>$$Uhttps://onlinelibrary.wiley.com/doi/pdf/10.1002%2Fmarc.1997.030180807$$EPDF$$P50$$Gwiley$$H</linktopdf><linktohtml>$$Uhttps://onlinelibrary.wiley.com/doi/full/10.1002%2Fmarc.1997.030180807$$EHTML$$P50$$Gwiley$$H</linktohtml><link.rule.ids>315,781,785,1418,27928,27929,45578,45579</link.rule.ids><backlink>$$Uhttp://pascal-francis.inist.fr/vibad/index.php?action=getRecordDetail&idt=2749902$$DView record in Pascal Francis$$Hfree_for_read</backlink></links><search><creatorcontrib>Osawa, Zenjiro</creatorcontrib><creatorcontrib>Kato, Masahide</creatorcontrib><creatorcontrib>Terano, Minoru</creatorcontrib><title>Effect of stereoregularity on the thermo-oxidative degradation of poly(propylene)s estimated by chemiluminescence</title><title>Macromolecular rapid communications.</title><addtitle>Macromol. Rapid Commun</addtitle><description>The effect of stereoregularity on the thermo‐oxidative degradation of poly(propylene)s, isotactic (IPP) and syndiotactic (SPP), was compared with that of high density polyethylene (HDPE) by means of chemiluminescence (CL). SPP is extremely stable to thermal oxidation and CL signals appeared much later than in IPP and even later than in HDPE. For example, at 160°C the maximum intensity of CL was measured after only 13 min for IPP, 60 min for HDPE and 260 min for SPP. IR spectroscopic results support the conclusions drawn from CL results.</description><subject>Applied sciences</subject><subject>Exact sciences and technology</subject><subject>Organic polymers</subject><subject>Physicochemistry of polymers</subject><subject>Properties and characterization</subject><subject>Thermal and thermodynamic properties</subject><issn>1022-1336</issn><issn>1521-3927</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>1997</creationdate><recordtype>article</recordtype><recordid>eNqNkEtLw0AUhYMoWKu_wE0WLnSROo8kM9kIUmsVqkKpFNwMk8mddjQvZ1Jt_r0JleLSxeWexTnnXj7PO8dohBEi14W0aoSThI0QRZgjjtiBN8ARwQFNCDvsNCIkwJTGx96Jc-8IIR4iMvA-J1qDavxK-64BC5WF1SaX1jStX5V-s4Z-bFEF1dZksjFf4GewsrLXnaHL1VXeXta2qtscSrhyPrjGFLKBzE9bX62hMPmmMCU4BaWCU-9Iy9zB2e8eeq_3k8X4IZi9TB_Ht7NA0ThhAWEYaxyDhpSnQBnlCqdSM5ApCrnSKosV4zoCgEiyjCVcxjGXOqIpp2EGdOjRXa-ylXMWtKht95ZtBUaipyZ6aqKnJvbUutTFLlVLp2SurSyVcfsoYWGSINLZbna2b5ND-59m8XQ7H_-9E-wKTId9uy-Q9kPEjLJILJ-nYhnxOb9bvIkp_QHJGZNZ</recordid><startdate>199708</startdate><enddate>199708</enddate><creator>Osawa, Zenjiro</creator><creator>Kato, Masahide</creator><creator>Terano, Minoru</creator><general>Hüthig & Wepf Verlag</general><general>Wiley</general><scope>BSCLL</scope><scope>IQODW</scope><scope>AAYXX</scope><scope>CITATION</scope></search><sort><creationdate>199708</creationdate><title>Effect of stereoregularity on the thermo-oxidative degradation of poly(propylene)s estimated by chemiluminescence</title><author>Osawa, Zenjiro ; Kato, Masahide ; Terano, Minoru</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-LOGICAL-c3697-2711f16efeb8be3738c1baf7eab048cfcd6c78f5eee5a7d798a668af53b834de3</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>1997</creationdate><topic>Applied sciences</topic><topic>Exact sciences and technology</topic><topic>Organic polymers</topic><topic>Physicochemistry of polymers</topic><topic>Properties and characterization</topic><topic>Thermal and thermodynamic properties</topic><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Osawa, Zenjiro</creatorcontrib><creatorcontrib>Kato, Masahide</creatorcontrib><creatorcontrib>Terano, Minoru</creatorcontrib><collection>Istex</collection><collection>Pascal-Francis</collection><collection>CrossRef</collection><jtitle>Macromolecular rapid communications.</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Osawa, Zenjiro</au><au>Kato, Masahide</au><au>Terano, Minoru</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Effect of stereoregularity on the thermo-oxidative degradation of poly(propylene)s estimated by chemiluminescence</atitle><jtitle>Macromolecular rapid communications.</jtitle><addtitle>Macromol. Rapid Commun</addtitle><date>1997-08</date><risdate>1997</risdate><volume>18</volume><issue>8</issue><spage>667</spage><epage>671</epage><pages>667-671</pages><issn>1022-1336</issn><eissn>1521-3927</eissn><abstract>The effect of stereoregularity on the thermo‐oxidative degradation of poly(propylene)s, isotactic (IPP) and syndiotactic (SPP), was compared with that of high density polyethylene (HDPE) by means of chemiluminescence (CL). SPP is extremely stable to thermal oxidation and CL signals appeared much later than in IPP and even later than in HDPE. For example, at 160°C the maximum intensity of CL was measured after only 13 min for IPP, 60 min for HDPE and 260 min for SPP. IR spectroscopic results support the conclusions drawn from CL results.</abstract><cop>Zug</cop><pub>Hüthig & Wepf Verlag</pub><doi>10.1002/marc.1997.030180807</doi><tpages>5</tpages></addata></record> |
fulltext | fulltext |
identifier | ISSN: 1022-1336 |
ispartof | Macromolecular rapid communications., 1997-08, Vol.18 (8), p.667-671 |
issn | 1022-1336 1521-3927 |
language | eng |
recordid | cdi_crossref_primary_10_1002_marc_1997_030180807 |
source | Access via Wiley Online Library |
subjects | Applied sciences Exact sciences and technology Organic polymers Physicochemistry of polymers Properties and characterization Thermal and thermodynamic properties |
title | Effect of stereoregularity on the thermo-oxidative degradation of poly(propylene)s estimated by chemiluminescence |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-16T17%3A21%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-wiley_cross&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Effect%20of%20stereoregularity%20on%20the%20thermo-oxidative%20degradation%20of%20poly(propylene)s%20estimated%20by%20chemiluminescence&rft.jtitle=Macromolecular%20rapid%20communications.&rft.au=Osawa,%20Zenjiro&rft.date=1997-08&rft.volume=18&rft.issue=8&rft.spage=667&rft.epage=671&rft.pages=667-671&rft.issn=1022-1336&rft.eissn=1521-3927&rft_id=info:doi/10.1002/marc.1997.030180807&rft_dat=%3Cwiley_cross%3EMARC030180807%3C/wiley_cross%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |