Wetting of substoichiometric YSZ2-x by molten Sn-based active alloys at 800–900 °C
Veröffentlicht in Ceramics international
VolltextArtikel -
3
Wetting of substoichiometric YSZ2- by molten Sn-based active alloys at 800–900 °C
Veröffentlicht in Ceramics international
VolltextArtikel -
4
Wetting of YSZ by molten Sn–8Zr, Sn–4Zr–4Ti, and Sn–8Ti alloys at 800–900 °C
Veröffentlicht in Ceramics international
VolltextArtikel -